Lithium Metal Penetration Induced by Electrodeposition through Solid Electrolytes: Example in Single-Crystal Li6La3ZrTaO12 Garnet

被引:184
|
作者
Swamy, Tushar [1 ]
Park, Richard [2 ]
Sheldon, Brian W. [3 ]
Rettenwander, Daniel [4 ]
Porz, Lukas [5 ]
Berendts, Stefan [6 ]
Uecker, Reinhard [7 ]
Carter, W. Craig [2 ]
Chiang, Yet-Ming [2 ]
机构
[1] MIT, Dept Mech Engn, Cambridge, MA 02139 USA
[2] MIT, Dept Mat Sci & Engn, Cambridge, MA 02139 USA
[3] Brown Univ, Sch Engn, Providence, RI 02912 USA
[4] Graz Univ Technol, Inst Chem & Technol Mat, A-8010 Graz, Austria
[5] Tech Univ Darmstadt, Inst Mat Sci, D-64287 Darmstadt, Germany
[6] Tech Univ Berlin, Dept Chem, Berlin, Germany
[7] Leibniz Inst Crystal Growth, D-12489 Berlin, Germany
基金
奥地利科学基金会;
关键词
INTERFACE STABILITY; FRACTURE-TOUGHNESS; BETA-ALUMINA; HIGH-ENERGY; LI; CHALLENGES; DEPOSITION; DEGRADATION; TEMPERATURE; PROPAGATION;
D O I
10.1149/2.1391814jes
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Solid electrolytes potentially enable rechargeable batteries with lithium metal anodes possessing higher energy densities than today's lithium ion batteries. To do so the solid electrolyte must suppress instabilities that lead to poor coulombic efficiency and short circuits. In this work, lithium electrodeposition was performed on single-crystal Li6La3ZrTaO12 garnets to investigate factors governing lithium penetration through brittle electrolytes. In single crystals, grain boundaries are excluded as paths for lithium metal propagation. Vickers microindentation was used to introduce surface flaws of known size. However, operando optical microscopy revealed that lithium metal penetration propagates preferentially from a different, second class of flaws. At the perimeter of surface current collectors smaller in size than the lithium source electrode, an enhanced electrodeposition current density causes lithium filled cracks to initiate and grow to penetration, even when large Vickers defects are in proximity. Modeling the electric field distribution in the experimental cell revealed that a 5-fold enhancement in field occurs within 10 micrometers of the electrode edge and generates high local electrochemomechanical stress. This may determine the initiation sites for lithium propagation, overriding the presence of larger defects elsewhere. (C) The Author(s) 2018. Published by ECS.
引用
收藏
页码:A3648 / A3655
页数:8
相关论文
共 50 条
  • [31] Garnet-type Solid-state Electrolyte Li7La3Zr2O12: Crystal Structure, Element Doping and Interface Strategies for Solid-state Lithium Batteries
    Guo, Sijie
    Sun, Yonggang
    Cao, Anmin
    CHEMICAL RESEARCH IN CHINESE UNIVERSITIES, 2020, 36 (03) : 329 - 342
  • [32] Garnet-type Solid-state Electrolyte Li7La3Zr2O12: Crystal Structure, Element Doping and Interface Strategies for Solid-state Lithium Batteries
    Sijie Guo
    Yonggang Sun
    Anmin Cao
    Chemical Research in Chinese Universities, 2020, 36 : 329 - 342
  • [33] Synthesis, Structure, Transport Properties, Electrochemical Stability Window, and Lithium Plating/Stripping of Mg and Nb Codoped Li7La3Zr2O12 Garnet-Type Solid Electrolytes
    Ma, Kai
    Chen, Bowen
    Li, Cheng-Xin
    Thangadurai, Venkataraman
    JOURNAL OF PHYSICAL CHEMISTRY C, 2022, 126 (18): : 7828 - 7840
  • [34] Effect of lithium ion concentration on the microstructure evolution and its association with the ionic conductivity of cubic garnet-type nominal Li7Al0.25La3Zr2O12 solid electrolytes
    Zhang, Yanhua
    Chen, Fei
    Tu, Rong
    Shen, Qiang
    Zhang, Xulong
    Zhang, Lianmeng
    SOLID STATE IONICS, 2016, 284 : 53 - 60
  • [35] Toward a Fundamental Understanding of the Lithium Metal Anode in Solid-State Batteries-An Electrochemo-Mechanical Study on the Garnet-Type Solid Electrolyte Li6.25Al0.25La3Zr3O12
    Krauskopf, Thorben
    Hartmann, Hannah
    Zeier, Wolfgang G.
    Janek, Juergen
    ACS APPLIED MATERIALS & INTERFACES, 2019, 11 (15) : 14463 - 14477
  • [36] Diffusion coefficient of lithium ions in garnet-type Li6.5La3Zr1.5Ta0.5O12 single crystal probed by 7Li pulsed field gradient-NMR spectroscopy
    Dorai, Arunkumar
    Kuwata, Naoaki
    Takekawa, Reiji
    Kawamura, Junichi
    Kataoka, Kunimitsu
    Akimoto, Junji
    SOLID STATE IONICS, 2018, 327 : 18 - 26
  • [37] Rapid sintering of Li6.5La3Zr1Nb0.5Ce0.25Ti0.25O12 for high density lithium garnet electrolytes with current induced in situ interfacial resistance reduction
    Stockham, M. P.
    Dong, B.
    James, M. S.
    Zhu, P.
    Kendrick, E.
    Slater, P. R.
    ENERGY ADVANCES, 2023, 2 (10): : 1660 - 1673
  • [38] Ultrathin Li6.75La3Zr1.75Ta0.25O12-Based Composite Solid Electrolytes Laminated on Anode and Cathode Surfaces for Anode-free Lithium Metal Batteries
    Zegeye, Tilahun Awoke
    Su, Wei-Nien
    Fenta, Fekadu Wubatu
    Zeleke, Tamene Simachew
    Jiang, Shi-Kai
    Hwang, Bing Joe
    ACS APPLIED ENERGY MATERIALS, 2020, 3 (12): : 11713 - 11723
  • [39] Li7La3Zr2O12 Protonation as a Means to Generate Porous/Dense/Porous-Structured Electrolytes for All-Solid-State Lithium-Metal Batteries
    Grissa, Rabeb
    Seidl, Lukas
    Dachraoui, Walid
    Sauter, Ulrich
    Battaglia, Corsin
    ACS APPLIED MATERIALS & INTERFACES, 2022, 14 (40) : 46001 - 46009
  • [40] Excellent Lithium Metal Anode Performance via In Situ Interfacial Layer Induced by Li6.75La3Zr1.75Ta0.25O12@Amorphous Li3OCl Composite Solid Electrolyte
    Tian, Yijun
    Ding, Fei
    Sang, Lin
    He, Yan-Bing
    Liu, Xingjiang
    Xu, Qiang
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (05): : 4781 - 4798