Dissolution behaviour of MgO based refractories in CaO-Al2O3-SiO2 slag

被引:28
|
作者
Huang, F. [1 ]
Liu, C. [1 ]
Maruoka, N. [2 ]
Kitamura, S. -Y. [2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Tohoku Univ, Inst Multidisciplinary Res Adv Mat, Aoba Ku, Sendai, Miyagi 9808577, Japan
基金
中国国家自然科学基金;
关键词
Dissolution; Refractory; MgO-C; MgO-Cr2O3; Slag; STAINLESS-STEEL SLAGS; DEGRADATION MECHANISMS; CORROSION; PARTICLES; OXIDE;
D O I
10.1179/1743281215Y.0000000003
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Magnesium oxide (MgO) based refractories are widely used in secondary refining processes, and their dissolution into refining slag is the primary cause of their shortened lifespan. The dissolution rate was investigated for sintered MgO and commercial MgO-C and MgO-Cr2O3 refractories in a synthesised 50CaO-45Al(2)O(3)-5SiO(2) liquid (mass-%) slag. The change in slag composition was measured after a refractory sample was placed into the molten slag that was stirred by flowing argon gas at 1773 K. The dissolution rate of the sintered MgO was above those of the MgO-C and MgO-Cr2O3 refractories under the same gas flowrate, although the dissolution rate of all samples increased as the gas flowrate was increased from 25 to 75 mL.min(-1). The slag containing 5 mass-% FeO considerably promoted the dissolution of the MgO-C refractory because of the oxidation of carbon by FeO. The dissolution of all the refractories was greatly affected by penetration of the liquid slag, with the mass transfer of MgO in the penetrating slag at lower gas flowrates likely being the rate controlling step. At high gas flowrates, Ar bubbles covered the surface and blocked the contact between the liquid slag and the solid phase, reducing the dissolution rate.
引用
收藏
页码:553 / 560
页数:8
相关论文
共 50 条
  • [21] Kinetic Model of Silica Dissolution in CaO-SiO2-MgO-Al2O3 Slag System
    An, Haifei
    Li, Jie
    Yang, Aimin
    Liu, Weixing
    Tian, Can
    TMS 2019 148TH ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2019, : 1045 - 1053
  • [22] Incorporation of chlorine in a secondary steelmaking slag based on the CaO-Al2O3-SiO2 system
    Patsiogiannis, F
    Pal, UB
    Chou, KC
    ISIJ INTERNATIONAL, 1996, 36 (09) : 1119 - 1126
  • [23] Kinetics of dissolution of sapphire in melts in the CaO-Al2O3-SiO2 system
    Shaw, Cliff S. J.
    Klausen, Kim B.
    Mao, Huahai
    GEOCHIMICA ET COSMOCHIMICA ACTA, 2018, 229 : 129 - 146
  • [24] Dissolution of CaO in SiO2-CaO-Al2O3 Slag in Si Production
    Folstad, Marit Buhaug
    Einarsrud, Kristian Etienne
    Tangstad, Merete
    METALS, 2024, 14 (02)
  • [25] Kinetics studies on the dissolution of nitrogen in the CaO-Al2O3-SiO2 and CaO-Al2O3-TiOx melts
    Koichi Iuchi
    Kazuki Morita
    Nobuo Sano
    Metallurgical and Materials Transactions B, 1998, 29 : 1235 - 1240
  • [26] Viscosity and desulphurisation behaviour of CaO-SiO2-MgO-Al2O3-BaO-MnO slag
    Yu, Yuanhao
    Liu, Wenguo
    Zuo, Haibin
    IRONMAKING & STEELMAKING, 2023, 50 (10) : 1420 - 1426
  • [27] THE MULLITE-CORUNDUM BOUNDARY IN THE SYSTEMS MGO-AL2O3-SIO2 AND CAO-AL2O3-SIO2
    ARAMAKI, S
    ROY, R
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1959, 42 (12) : 644 - 645
  • [28] In Situ Observation of the Dissolution of Al2O3 Particles in CaO-Al2O3-SiO2 Slags
    Changyu Ren
    Lifeng Zhang
    Ji Zhang
    Songjie Wu
    Pei Zhu
    Ying Ren
    Metallurgical and Materials Transactions B, 2021, 52 : 3288 - 3301
  • [29] Dissolution Kinetics of Synthetic FeCr2O4 in CaO-MgO-Al2O3-SiO2 Slag
    Wei, Kangji
    Wang, Lijun
    Liu, Shiyuan
    He, Xiaobo
    Xiao, Yiyu
    Chou, Kuochih
    ISIJ INTERNATIONAL, 2022, 62 (04) : 617 - 625
  • [30] Effect of Na2O on Dissolution Rate of Alumina in CaO-Al2O3-MgO-SiO2 Slag
    Shu, Qifeng
    Wang, Yanfei
    Li, Jiangling
    Liu, Yang
    Li, Pengfei
    Chou, Kuochih
    ISIJ INTERNATIONAL, 2015, 55 (11) : 2297 - 2303