Corrosion of heating surfaces of power station boiler equipment made of steel 12X18H10T

被引:0
|
作者
Reformatskaya, II
Ryzhenkov, VA
Rodionova, IG
Ashcheulova, II
Yakushev, VV
Kiselev, VD
机构
[1] RF Karpov Inst Phys Chem, FGUP, GNTs, Moscow 103064, Russia
[2] Tech Univ, Moscow Power Inst, Moscow, Russia
[3] FGUP Bardin Cent Res Inst Ferrous Met, Moscow, Russia
来源
PROTECTION OF METALS | 2003年 / 39卷 / 06期
关键词
Stainless Steel; Inorganic Chemistry; Thermal Power; Heating Surface; Change Composition;
D O I
10.1023/B:PROM.0000007846.80803.b3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The long-term operation of thermal power equipment made of 12X18HIOT steel at a temperature of greater than or equal to 550degreesC and higher changes its performance due to the changed composition of inside surfaces and bodies of tubes. To avoid deterioration of service characteristics during the operation, the thermal equipment is recommended to make of low-carbon chrome-nickel stainless steels or niobium-stabilized steels. Preservation of the equipment by octadecylamine should be carried out only at a working temperature below its thermodestruction temperature.
引用
收藏
页码:537 / 542
页数:6
相关论文
共 50 条
  • [41] KINETICS OF GAS CORROSION OF AUSTENITIC STEEL 12Kh18N10T
    Priimak, E. Yu.
    Gryzunov, V. I.
    Gryzunova, T. I.
    METAL SCIENCE AND HEAT TREATMENT, 2009, 51 (9-10) : 429 - 432
  • [42] Kinetics of gas corrosion of austenitic steel 12Kh18N10T
    E. Yu. Priimak
    V. I. Gryzunov
    T. I. Gryzunova
    Metal Science and Heat Treatment, 2009, 51 : 429 - 432
  • [43] The susceptibility of low-sensitized 08X18H10T steel to corrosion cracking at indoor temperature
    Makarova, NL
    Nazarov, AA
    PROTECTION OF METALS, 1997, 33 (05): : 441 - 443
  • [44] Steel 08Kh18N10T-VO for Power Generation Equipment Components
    Khlyamkov, N. A.
    Petrov, S. N.
    Berezhko, B. I.
    Parkhomenko, S. N.
    Rudneva, E. L.
    METALLURGIST, 2017, 61 (7-8) : 585 - 590
  • [45] Steel 08Kh18N10T-VO for Power Generation Equipment Components
    N. A. Khlyamkov
    S. N. Petrov
    B. I. Berezhko
    S. N. Parkhomenko
    E. L. Rudneva
    Metallurgist, 2017, 61 : 585 - 590
  • [46] Structural Integrity of Welded Joint between Steel Grades X10CrMoVNb9-1 and 12X18H12T
    Krstevska, Aleksandra
    Zdraveski, Filip
    Petreski, Martin
    Gavriloski, Marjan
    Bogatinoski, Zoran
    TEHNICKI VJESNIK-TECHNICAL GAZETTE, 2025, 32 (02): : 512 - 516
  • [47] Rolling 08X18H10T steel rail profiles
    Peretyat'ko V.N.
    Pyataikin E.M.
    Dorofeev V.V.
    Karetnikov A.Y.
    Dobryanskii A.V.
    Steel in Translation, 2011, 41 (8) : 649 - 651
  • [48] A CASE OF PITTING CORROSION OF STEEL 12KH18N10T IN TAP WATER
    YAVOR, VA
    GITELMAN, MM
    KOVINSKAYA, SV
    PROTECTION OF METALS, 1980, 16 (02): : 124 - 125
  • [49] Effect of movement and temperature on steel 12Kh18N10T pitting corrosion
    V. S Pakhomov
    V. V. Makartsev
    Chemical and Petroleum Engineering, 2012, 47 (11-12) : 733 - 740
  • [50] The effect of heatings on corrosion resistance of 12Kh18N10T stainless steel
    VIAM, Moscow, Russia
    Zashch Met, 2 (133-138):