Surface-hardened polydimethylsiloxane (PDMS) with random cracks is studied by means of double replication. The PDMS samples are prepared under different curing conditions, resulting in a different Young's modulus of the bulk. To modify the surface, an excimer lamp at 172 nm is used. The samples are stretched uniaxially until the first cracks appear. As an evaluation under strain is hard or rather impossible, the idea is to replicate the cracked sample in a curable material and to characterize the cracks by inspection of the replica. To protect the sample from mechanical loading, this replication is done by molding in OrmoStamp on glass; these replicas are used for optical inspection to determine the crack spacing. As a characterization of the depth and width of the cracks is highly facilitated when cleaving is enabled, a second replication is performed into a thin layer of SU-8 on Si; these second replica are analyzed by secondary electron microscopy of cross sections. They provide a realistic picture of the crack shape. It is found that the curing conditions affect the crack shape; a U-shape occurs with a low bulk modulus, whereas a V-shape occurs with a high bulk modulus. The parameters width, depth, and spacing are largely unaffected by the curing conditions. This work provides a background to understand the behavior of random cracks, which is, e.g., useful to design a system with controlled cracks that remain stable. An important finding is that as soon as cracking occurs at a certain strain, already a number of cracks develop, yet without any further stretching. The cracks behave independently from neighboring cracks. Upon further stretching, new cracks develop, and the crack width and depth remain similar. Therefore, these random cracks are stable, and sample failure does not occur up to a strain of at least 40%.
引用
收藏
页数:7
相关论文
共 50 条
  • [21] POTENTIOMETRIC NON-DESTRUCTIVE TESTING OF SURFACE-HARDENED MATERIALS
    OMINI, M
    IAZZI, F
    RASTALDO, A
    TURCO, C
    REVIEW OF SCIENTIFIC INSTRUMENTS, 1981, 52 (07): : 1054 - 1060
  • [22] Predicting the Fatigue Limit of Surface-Hardened Parts with Stress Concentrators
    Pavlov V.F.
    Bukatyi A.S.
    Semenova O.Y.
    Russian Engineering Research, 2019, 39 (04) : 283 - 287
  • [23] Characterization of thermochemically surface-hardened titanium by light optical microscopy
    Gammeltoft-Hansen N.
    Munch S.S.
    Jellesen M.S.
    Somers M.A.J.
    Christiansen T.L.
    Christiansen, Thomas L. (tch@mek.dtu.dk), 1600, ASTM International (06): : 298 - 310
  • [24] Increasing the Accuracy of Measuring the Hardness of Surface-Hardened Steel Products
    Valko A.L.
    Rudenko S.P.
    Sandomirskii S.G.
    Steel in Translation, 2022, 52 (06) : 633 - 637
  • [25] FACTORS AFFECTING THE POSITION OF THE FATIGUE FRACTURE IN A SURFACE-HARDENED MATERIAL
    BOITSOV, BV
    SOVIET ENGINEERING RESEARCH, 1985, 5 (06): : 2 - 4
  • [26] METASTABLE PHASE IN CARBON-STEELS SURFACE-HARDENED WITH SILICON
    VENGRENOVICH, RD
    UDOVITSKIY, VI
    GORICHOK, BO
    RUSSIAN METALLURGY, 1980, (03): : 152 - 153
  • [27] SURFACE FAILURE OF SOFT AND SURFACE-HARDENED STEEL ROLLERS IN ROLLING-CONTACT
    FUJITA, K
    YOSHIDA, A
    WEAR, 1979, 55 (01) : 27 - 39
  • [28] WEAR TESTS ON SURFACE-HARDENED CP TITANIUM COMBINED WITH UHMWPE
    ALBREKTSSON, B
    ALBREKTSSON, T
    ANDERSSON, S
    ROSTLUND, T
    ACTA ORTHOPAEDICA SCANDINAVICA, 1987, 58 (02): : 176 - 177
  • [29] Layer Approach to Model Fatigue Strength of Surface-Hardened Components
    Dobberke, Denes
    Leitner, Martin
    Wiebesiek, Jens
    Froeschl, Juergen
    METALS, 2024, 14 (07)
  • [30] Optimization of the parameters of the surface-hardened layer in laser quenching of components
    Kondrat'ev, S. Yu
    Gorynin, V.I.
    Popov, V.O.
    Welding International, 2012, 26 (08) : 629 - 632