In this study, integration of an hydrogen barrier into a FeRAM process flow is investigated. It is reported in the literature that ferroelectric properties can be maintained after hydrogen annealing by using IrOx as a top electrode [16][17][18]. Advantage of materials like IrOx is less catalytic activity compared to Pt. However, we found that IrOx is not a promising candidate for top electrode barrier. (Pt)/IrOx/SBT/Pt capacitors are prone to shorting or exhibit high leakage. IrOx films are very easily reduced by reducing ambient which will result in peeling off. Also, IrOx films tend to oxidize Ti or TiN layers immediately. Therefore, other barrier materials or layer sequences like Ir/IrOx have to be considered. For protection of the entire capacitor an Encapsulation Barrier Layer (EBL) is required. In this study, LPCVD SiN is used. LPCVD SiN is a standard material in CMOS technology. Production tools are available and it is well known as hydrogen barrier. By modifying the deposition process and using a novel process sequence, no visual damage of the capacitors after SiN-deposition and FGA is seen. Also, no degradation of electrical properties after capacitor formation as well as after SiN-deposition and FGA is observed. However, after metal 1 and metal 2 processing, 2P(r) values at 1.8V are reduced from 12 muC/cm(2) to 2 muC/cm(2). Polarization at 5.0V is not affected.
引用
收藏
页码:273 / 284
页数:12
相关论文
共 50 条
  • [41] Quantitative XPS determination of Pt coverage on SrBi2Ta2O9 thin films for ferroelectric memories
    Asami, K
    Koiwa, I
    Yamanobe, T
    SURFACE AND INTERFACE ANALYSIS, 2001, 31 (04) : 265 - 270
  • [42] Electrical and ferroelectric studies of the 2-layered SrBi2Ta2O9 based ceramics
    Swain, Sridevi
    Kumar, Pawan
    Choudhary, Ram Bilash
    PHYSICA B-CONDENSED MATTER, 2015, 477 : 56 - 63
  • [43] The effect of annealing temperature on the formation of SrBi2Ta2O9 (SBT) thin films
    Ravichandran, D
    Yamakawa, K
    Roy, R
    Bhalla, AS
    TrolierMcKinstry, S
    Guo, R
    Cross, LE
    ISAF '96 - PROCEEDINGS OF THE TENTH IEEE INTERNATIONAL SYMPOSIUM ON APPLICATIONS OF FERROELECTRICS, VOLS 1 AND 2, 1996, : 601 - 603
  • [44] 溶胶-凝胶法制备SrBi2Ta2O9(SBT)的研究
    王文
    贾德昌
    周玉
    叶枫
    功能材料, 2002, (02) : 195 - 197
  • [45] Ferroelectric and piezoelectric properties of tungsten substituted SrBi2Ta2O9 ferroelectric ceramics
    Coondoo, Indrani
    Agarwal, S. K.
    Jha, A. K.
    MATERIALS RESEARCH BULLETIN, 2009, 44 (06) : 1288 - 1292
  • [46] Orientation dependent ferroelectric properties of SrBi2Ta2O9 ferroelectric thin films
    Moon, SE
    Back, SB
    Kwun, SI
    Song, TK
    Yoon, JG
    PROCEEDINGS OF THE 2001 12TH IEEE INTERNATIONAL SYMPOSIUM ON APPLICATIONS OF FERROELECTRICS, VOLS I AND II, 2001, : 933 - 936
  • [47] Effects of crystallization annealing sequence for SrBi2Ta2O9 (SBT) film on Pt/SBT interface morphology and electrical properties of ferroelectric capacitor
    Yang, Woo Seok
    Yeom, Seung Jin
    Kim, Nam Kyeong
    Kweon, Soon Yong
    Roh, Jae Sung
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 2000, 39 (9 B): : 5465 - 5468
  • [48] Effects of crystallization annealing sequence for SrBi2Ta2O9 (SBT) film on Pt/SBT interface morphology and electrical properties of ferroelectric capacitor
    Yang, WS
    Yeom, SJ
    Kim, NK
    Kweon, SY
    Roh, JS
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2000, 39 (9B): : 5465 - 5468
  • [49] Non-volatile memories using SrBi2Ta2O9 ferroelectrics
    Jones Jr., R.E.
    Chu, P.Y.
    Jiang, B.
    Melnick, B.M.
    Taylor, D.J.
    White Jr., B.E.
    Zafar, S.
    Price, D.
    Zurcher, P.
    Gillespie, S.J.
    Otsuki, T.
    Sumi, T.
    Judai, Y.
    Uemoto, Y.
    Fujii, E.
    Integrated Ferroelectrics, 1997, 17 (1 -4 pt 1) : 21 - 30
  • [50] Non-volatile memories using SrBi2Ta2O9 ferroelectrics
    Jones, RE
    Chu, PY
    Jiang, B
    Melnick, BM
    Taylor, DJ
    White, BE
    Zafar, S
    Price, D
    Zurcher, P
    Gillespie, SJ
    Otsuki, T
    Sumi, T
    Judai, Y
    Uemoto, Y
    Fujii, E
    Hayashi, S
    Moriwaki, N
    Azuma, M
    Shimada, Y
    Arita, K
    Hirano, H
    Nakane, J
    Nakakum, T
    Kano, G
    INTEGRATED FERROELECTRICS, 1997, 17 (1-4) : 21 - 30