关键词
nanopowder; tungsten; tungsten carbide; WC-Co mixture; melt; nanosize; porosity; grain size; hardness; strength; fracture toughness; wear resistance; TUNGSTEN CARBIDE POWDERS; GRAIN-GROWTH; EARLY-STAGE; HARDMETALS;
D O I
10.1007/s11106-015-9670-2
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Production processes for fine powders of tungsten, tungsten carbide, and WC-Co and sintering methods for nanosized WC-Co hard metals are reviewed. The properties, structure, and applications of nanosized WC-Co hard metals described in the literature are analyzed. It is established that, regardless of the process, the mandatory requirements for the production of fine hard metals are: (i) purity of starting materials, (ii) precise compliance with the process procedure, and (iii) careful control at all production stages, which exclude unwanted phases and defects in the structure.
引用
收藏
页码:643 / 654
页数:12
相关论文
共 50 条
  • [31] The submicrostructure of WC-Co hard metals alloyed with transition metals by the technology of treatment with metallic melts
    Lisovskii, AF
    Tkachenko, NV
    POWDER METALLURGY AND METAL CERAMICS, 1997, 36 (11-12) : 633 - 638
  • [32] Sintering behavior of nanostructured WC-Co composite
    Kumar, Akshay
    Singh, K.
    Pandey, O. P.
    CERAMICS INTERNATIONAL, 2011, 37 (04) : 1415 - 1422
  • [33] Synthesis and processing of nanostructured WC-Co materials
    Ban, ZG
    Shaw, LL
    JOURNAL OF MATERIALS SCIENCE, 2002, 37 (16) : 3397 - 3403
  • [34] Deposition and characterization of nanostructured WC-Co coating
    Zhu, YC
    Ding, CX
    Yukimura, K
    Xiao, TD
    Strutt, PR
    CERAMICS INTERNATIONAL, 2001, 27 (06) : 669 - 674
  • [35] Metallographic analyses of laser cladded WC-Ni and WC-Co hard-facing metals
    Chikwanda, HK
    Chiremba, M
    Van Rooyen, C
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 and 2, PROCEEDINGS, 2004, : 996 - 999
  • [36] Metallographic Analyses of Laser Gladded WC-Ni and WC-Co Hard-facing Metals
    HK Chikwanda
    M Chiremba
    C Van Rooyen
    材料热处理学报, 2004, (05) : 996 - 999
  • [37] MICROSTRUCTURE OF NANOCRYSTALLINE WC POWDERS AND WC-Co HARD ALLOYS
    Kurlov, A. S.
    Leenaers, A.
    van den Berghe, S.
    Scibetta, M.
    Schroettner, H.
    Rempel, A. A.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2011, 27 (02) : 165 - 172
  • [38] OBSERVATION OF SPINEL PARTICLES IN SINTERED WC-CO HARD METAL BY TRANSMISSION ELECTRON-MICROSCOPY
    ROUX, HL
    JOURNAL OF PHYSICS F-METAL PHYSICS, 1978, 8 (10): : L213 - &
  • [39] Investigation of characteristics and properties of spark plasma sintered ultrafine WC-6.4Fe3.6Ni alloy as potential alternative WC-Co hard metals
    Silva, Erijanio Nonato da
    Santos, Alessandra Agna Araujo dos
    Nascimento, Rubens Maribondo do
    Alves, Salete Martins
    Guimaraes, Renan da Silva
    Filgueira, Marcello
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2021, 101
  • [40] THIN FOILS OF WC-CO HARD METAL
    PERSSON, G
    NATURE, 1968, 218 (5137) : 159 - &