Ferrite nucleation potency of non-metallic inclusions in medium carbon steels

被引:300
|
作者
Shim, JH
Oh, YJ
Suh, JY
Cho, YW [1 ]
Shim, JD
Byun, JS
Lee, DN
机构
[1] Korea Inst Sci & Technol, Div Mat Sci & Technol, Seoul 136791, South Korea
[2] Seoul Natl Univ, Sch Mat Sci & Engn, Seoul 151742, South Korea
关键词
steels; non-metallic inclusion; nucleation;
D O I
10.1016/S1359-6454(01)00134-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In recent years, there has been renewed interest in the role of non-metallic inclusions in controlling the microstructure of steels. The: potency of various inclusions and precipitates such as SiO2. MnO . SiO2, MnS, Al2O3, Ti2O3 and VN for the nucleation of intragranular ferrite has been examined in the present study. Among them, single SiO2, MnOSiO2, Al2O3. TiN and MnS particles seem to be inert to the nucleation of intragranular ferrite under the present experimental condition. Ti2O3 particles in a Mn-containing steel are very effective for the nucleation of intragranular ferrite. being (Ti,Mn)(2)O-3 particles by absorbing Mn atoms from a steel matrix. On the other hand, Ti2O3 particles in a Mn-free steel are not effective. MnS and Al2O3 particles in high nitrogen steels containing vanadium also appear to be potent for the nucleation of intragranular ferrite. The decrease in transformation temperature causes a change in the morphology of intragranular ferrite from idiomorphic ferrite to acicular ferrite. (C) 2001 Published by Elsevier Science Ltd on behalf of Acta Materialia Inc.
引用
收藏
页码:2115 / 2122
页数:8
相关论文
共 50 条
  • [31] Visualization of 3 Dimensional Distributions of Non-Metallic Inclusions in Steels
    Wakoh, Masamitsu
    Inoue, Shun
    Tsuji, Naofumi
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2017, 103 (08): : 451 - 457
  • [32] Ferrite Formation Behavior from Non-metallic Compounds in Steels
    Lee, Changjoon
    Nambu, Shoichi
    Inoue, Junya
    Koseki, Toshihiko
    TRENDS IN WELDING RESEARCH: PROCEEDINGS OF THE 9TH INTERNATIONAL CONFERENCE, 2013, : 43 - 47
  • [33] An investigation into the role of non-metallic inclusions in cleavage fracture of medium carbon pearlitic steels for high-speed railway wheel
    Zhou, Shi-tong
    Li, Zhao-dong
    Jiang, Lu
    Wang, Xin
    Xu, Pian
    Ma, Yu-xi
    Yan, Yu-ping
    Yang, Cai-fu
    Yong, Qi-long
    ENGINEERING FAILURE ANALYSIS, 2022, 131
  • [34] CONTRIBUTION TO KNOWLEDGE OF CHARACTERISTIC NON-METALLIC INCLUSIONS IN FERROCHROMIUMS WITH MEDIUM CARBON AND SILICON CONCENTRATIONS
    ZOJA, R
    REVUE DE METALLURGIE, 1967, 64 (7-8): : 675 - &
  • [35] High/very high cycle fatigue behaviors of medium carbon pearlitic wheel steels and the effects of microstructure and non-metallic inclusions
    Li, Zhao-dong
    Zhou, Shi-tong
    Yang, Cai-fu
    Yong, Qi-long
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 764
  • [36] Non-metallic inclusions in the ingot and final products of a medium-carbon tool steel
    Tripathi, N
    Sichen, D
    SCANDINAVIAN JOURNAL OF METALLURGY, 2004, 33 (06) : 362 - 369
  • [37] Influence of non-metallic inclusions on the austenite-to-ferrite phase transformation
    Gamsjäger, E
    Fischer, FD
    Svoboda, J
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 365 (1-2): : 291 - 297
  • [38] Behaviour of non-metallic inclusions in front of the solid-liquid interface in low carbon steels
    Kimura, S
    Nabeshima, Y
    Nakajima, K
    Mizoguchi, S
    BELTON MEMORIAL SYMPOSIUM PROCEEDINGS, 2000, : 275 - 287
  • [39] Micromechanical Modeling of Fatigue Crack Nucleation around Non-Metallic Inclusions in Martensitic High-Strength Steels
    Schaefer, Benjamin Josef
    Sonnweber-Ribic, Petra
    ul Hassan, Hamad
    Hartmaier, Alexander
    METALS, 2019, 9 (12)
  • [40] MICROSCOPIE EXAMINATION OF SPECIALTY STEELS FOR NON-METALLIC INCLUSIONS WITH INCLUSION CHARTS
    BARTELD, K
    STANZ, A
    ARCHIV FUR DAS EISENHUTTENWESEN, 1971, 42 (08): : 581 - &