Fatigue behavior of a Zr-based bulk metallic glass under uniaxial tension-tension and three-point bending loading mode

被引:32
|
作者
Yue, Y. [1 ]
Wang, R. [1 ,2 ]
Ma, D. Q. [1 ]
Tian, J. F. [1 ]
Zhang, X. Y. [1 ]
Jing, Q. [1 ]
Ma, M. Z. [1 ]
Liu, R. P. [1 ]
机构
[1] Yanshan Univ, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[2] Baosteel Roll Sci & Technol Co Ltd, Changzhou 213012, Peoples R China
关键词
Metallic glasses; Fatigue resistance and crack growth; Fracture; Electron microscopy; scanning; Mechanical testing; CRACK PROPAGATION BEHAVIOR; SUPERCOOLED LIQUID REGION; AMORPHOUS METAL; ENDURANCE LIMIT; NI; FRACTURE; ALLOY; MECHANISMS; GROWTH; DAMAGE;
D O I
10.1016/j.intermet.2015.02.005
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The fatigue behavior of as-cast Zr41.2Ti13.8Cu12.5Ni10Be22.5 bulk metallic glass was systematically investigated under uniaxial tension tension and three-point bending loading modes. To obtain the fatigue stress-life (S-N) diagram, stress-controlled experiments were conducted using a computer-controlled material test system electrohydraulic testing machine at 25 Hz with a 0.1 R ratio in air at room temperature. The fatigue endurance limit (630 MPa) in stress range terms under cyclic tensile load was almost three times higher than that under the three-point bending condition (225 MPa). Both fatigue resistances were similar at higher stress level. The fatigue fracture morphologies associated with the S-N curve indicated that the defects have little to no influence on the crack initiation and the fatigue life in low cycle fatigue range. However, at lower stress level, the most detrimental factor was the number of defects that resulted in fatigue endurance limit discrepancy. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:86 / 91
页数:6
相关论文
共 50 条
  • [41] Strain-hardening under uniaxial tension in a rejuvenated bulk metallic glass
    Zhou, W. H.
    Panagiotopoulos, N. T.
    Greer, A. L.
    Li, Y.
    SCRIPTA MATERIALIA, 2022, 212
  • [42] Effect of nanocrystalline dispersion on fatigue in a Zr-based bulk metallic glass
    Fujita, K
    Takayama, T
    Inoue, A
    Zhang, T
    Kimura, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (02) : 79 - 84
  • [43] Effect of loading rate on failure in Zr-based bulk metallic glass
    Xue, Y. F.
    Cai, H. N.
    Wang, L.
    Wang, F. C.
    Zhang, H. F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 473 (1-2): : 105 - 110
  • [44] Tensile and fatigue fracture mechanisms of a Zr-based bulk metallic glass
    Zhang, ZF
    Eckert, J
    Schultz, L
    JOURNAL OF MATERIALS RESEARCH, 2003, 18 (02) : 456 - 465
  • [45] Fatigue strength of notched components of Zr-Based bulk metallic glass
    Nakai Y.
    Fujihara K.
    Sei N.
    Ando K.
    Kim B.K.
    Zairyo/Journal of the Society of Materials Science, Japan, 2010, 59 (02) : 104 - 109
  • [46] Tensile and fatigue fracture mechanisms of a Zr-based bulk metallic glass
    Z. F. Zhang
    J. Eckert
    L. Schultz
    Journal of Materials Research, 2003, 18 : 456 - 465
  • [47] Fatigue coaxing experiments on a Zr-based bulk-metallic glass
    El-Shabasy, Adel B.
    Lewandowski, John J.
    SCRIPTA MATERIALIA, 2010, 62 (07) : 481 - 484
  • [48] Fatigue crack propagation in a nanocrystalline Zr-based bulk metallic glass
    Fujita, K
    Inoue, A
    Zhang, T
    MATERIALS TRANSACTIONS JIM, 2000, 41 (11): : 1448 - 1453
  • [49] Fatigue crack propagation in a nanocrystalline Zr-based bulk metallic glass
    Fujita, K
    Inoue, A
    Zhang, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (09) : 787 - 792
  • [50] A Highly Fatigue-Resistant Zr-Based Bulk Metallic Glass
    Steven E. Naleway
    Rawley B. Greene
    Bernd Gludovatz
    Neil K. N. Dave
    Robert O. Ritchie
    Jamie J. Kruzic
    Metallurgical and Materials Transactions A, 2013, 44 : 5688 - 5693