Effect of expanded organoclay by stearic acid to curing, mechanical and swelling properties of natural rubber nanocomposites

被引:1
|
作者
Ramadhan, A. [1 ]
Fathurrohman, M. Irfan [1 ]
Falaah, A. F. [1 ]
Setyawan, N. [2 ]
Soegijono, B. [3 ]
机构
[1] Indonesian Rubber Res Inst, Bogor, Indonesia
[2] Indonesian Ctr Agr Post Harvest Res & Dev, Bogor, Indonesia
[3] Univ Indonesia, Jakarta, Indonesia
关键词
SILICATE-NANOCOMPOSITES; LAYERED SILICATE; INTERCALATION;
D O I
10.1088/1757-899X/223/1/012030
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The interlayer basal spacing of organoclay (OC) could be increased with stearic acid (SA) added, thus OC changed into expanded organoclay by SA (OCSA). The effect of various loadings of OCSA on the curing, mechanical and swelling properties of natural rubber (NR) nanocomposites were studied. The natural rubber/expanded organoclay (NR/OCSA) nanocomposites were prepared by melt intercalation using a laboratory open mill. The curing characteristics of NR compounds were determined using a Moving Die Rheometer (MDR). The X-ray Diffraction (XRD), Attenuated Total Reflectance Infrared (ATR-IR) Spectroscopy and Field Emission Scanning Electron Microscopy (FESEM) were used to study the dispersion of OCSA in the NR matrix. The mechanical properties of NR/OCSA nanocomposites such as tensile strength, elongation at break and hardness were determined using ISO standard and swelling of NR/OCSA nanocomposites in toluene were determined using ISO 1817. The results showed that the SA intercalated into the gallery of OC and reacted with the hydroxyl groups in OC. It was indicated with the shifting of the negative peak 1,700 to 1,723 cm(-1) in the ATR-IR spectrum and increase the d-spacing of OC. The adding of various loadings of OCSA into NR could increase the torque and accelerate the curing of nanocomposites and it also could increase the mechanical and swelling properties of nanocomposites. The change in modulus at 100% elongation significantly increased with increasing the OCSA load until maximum loading at 10 phr. This trend was same with the hardness and modulus at 300% elongation. Meanwhile, the improvement of tensile strength and elongation at break was higher at 4 phr OCSA compared with the other loading. The increase of mechanical and swelling properties of NR/OCSA nanocomposites was due to intercalation/exfoliation of OCSA in NR matrix. It was revealed by appearing of the out-of-plane Si-O-(Al) stretch with peak value 1080 cm(-1) in the ATR-IR spectrum and the peaks of OCSA in the XRD pattern was disappeared until the loading of OCSA 8 phr and the thickness of morphology of OCSA below 100 nm.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Vulcanization kinetics of natural rubber-organoclay nanocomposites
    López-Manchado, MA
    Arroyo, M
    Herrero, B
    Biagiotti, J
    JOURNAL OF APPLIED POLYMER SCIENCE, 2003, 89 (01) : 1 - 15
  • [42] Effect of processing methods on the mechanical properties of natural rubber filled with stearic acid-modified soy protein particles
    Jong, Lei
    JOURNAL OF ELASTOMERS AND PLASTICS, 2014, 46 (05): : 413 - 426
  • [43] Curing Characteristics, Mechanical, Thermal, and Morphological Properties of Halloysite Nanotubes (HNTs)-Filled Natural Rubber Nanocomposites
    Ismail, Hanafi
    Salleh, Siti Zuliana
    Ahmad, Zulkifli
    POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2011, 50 (07) : 681 - 688
  • [44] Graphene-filled natural rubber nanocomposites: Influence of the composition on curing, morphological, mechanical, and electrical properties
    Siriwas, Thananya
    Pichaiyut, Skulrat
    Susoff, Markus
    Petersen, Svea
    Nakason, Charoen
    EXPRESS POLYMER LETTERS, 2023, 17 (08): : 819 - 836
  • [45] Curing characteristics and mechanical properties of natural rubber/chloroprene rubber and epoxidized natural rubber/chloroprene rubber blends
    Ismail, H
    Leong, HC
    POLYMER TESTING, 2001, 20 (05) : 509 - 516
  • [46] Effect of Mixing Parameters on Mechanical Properties of Organoclay Epoxy Nanocomposites
    Sharma, Bikramjit
    Chhibber, Rahul
    Mehta, Rajeev
    MATERIALS TODAY-PROCEEDINGS, 2018, 5 (01) : 276 - 286
  • [47] Effect of epoxidized natural rubber-organoclay nanocomposites on NR/high styrene rubber blends with fillers
    Pal, Kaushik
    Rajasekar, R.
    Kang, Dong Jin
    Zhang, Zhen Xiu
    Kim, Jin Kuk
    Das, C. K.
    MATERIALS & DESIGN, 2009, 30 (10) : 4035 - 4042
  • [48] Effect of Montmorillonite and Cellulose II Hybridization on Mechanical Properties of Natural Rubber Nanocomposites
    Mariano, Roberta M.
    Nunes, Regina C. R.
    Visconte, Leila L. Y.
    Altstaedt, Volker
    POLIMEROS-CIENCIA E TECNOLOGIA, 2013, 23 (01): : 123 - 127
  • [49] Effect of Electron Beam Irradiation on the Properties of Ethylene-(vinyl acetate) Copolymer/Natural Rubber/Organoclay Nanocomposites
    Munusamy, Y.
    Ismail, H.
    Mariatti, M.
    Ratnam, C. T.
    JOURNAL OF VINYL & ADDITIVE TECHNOLOGY, 2009, 15 (01): : 39 - 46
  • [50] Mechanical properties and curing characteristics of shape memory natural rubber
    Setyadewi, N. M.
    Indrajati, I. N.
    Darmawan, N.
    INTERNATIONAL SEMINAR ON METALLURGY AND MATERIALS, 2019, 541