Correlation of dynamic impact properties with adiabatic shear banding behaviour in Ti-15Mo-5Zr-3Al alloy

被引:23
|
作者
Lee, Woei-Shyan [1 ]
Lin, Chi-Feng [2 ]
Chen, Tao-Hsing [1 ]
Hwang, Hsin-Hwa [1 ]
机构
[1] Natl Cheng Kung Univ, Dept Mech Engn, Tainan 701, Taiwan
[2] Natl Ctr High Performance Comp, Hsin 744, Tainan Cty, Taiwan
关键词
Ti-15Mo-5Zr-3Al alloy; impact properties; adiabatic shear band; beta transus temperature; Splats and knobbles;
D O I
10.1016/j.msea.2007.05.027
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A compressive split-Hopkinson pressure bar is used to investigate the impact properties of Ti-15Mo-5Zr-3A1 alloy under strain rates ranging from 800 to 8000s(-1) at temperatures between 25 and 900 degrees C. The morphologies of the deformed microstructures and the fracture features of the adiabatic shear bands on the fracture surfaces are examined using optical and scanning electron microscopes. Based on the macroscopic and microscopic observations, the dynamic impact properties of the alloy are correlated with its adiabatic shear banding behaviour. The experimental results indicate that the strain rate and testing temperature both have a significant effect on the mechanical properties of Ti-15Mo-5Zr-3Al alloy. At a constant temperature, the flow stress increases with increasing strain rate. However, at a given strain rate, the flow stress reduces as the temperature increases. Furthermore, the fracture strain decreases with increasing temperature prior to phase transformation at 785 degrees C, but increases thereafter as the temperature is further increased. The temperature-dependent variation of the fracture strain is thought to be related to the amount of a phase in the deformed microstructure, which increases with increasing temperature prior to phase transformation, but dissolves entirely at higher temperatures and is replaced by a pure P phase. Fractographic analysis reveals that the specimens fracture as a consequence of adiabatic shear band formation. Specimens impacted at higher strain rates and lower temperatures are more likely to form adiabatic shear bands. The width of the shear band decreases with increasing temperature prior to phase transformation, but increases with increasing temperature thereafter. The microhardness within the adiabatic shear band is found to increase slightly in the specimens tested at higher strain rates and temperatures. The fracture surfaces of the impacted specimens exhibit both dimple-like and cleavage-like features. Finally, the splats and knobble-like features observed on the fracture surfaces of specimens deformed at the highest strain rate of 8 x 10(3) s(-1) and temperatures of 300 degrees C or higher, indicate that significant melting takes place during deformation under high strain rate and high temperature loading conditions prior to specimen fracture. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:172 / 184
页数:13
相关论文
共 50 条
  • [31] Effect of luting system with acidic primers on the durability of bonds with Ti-15Mo-5Zr-3Al titanium alloy and its component metals
    Wada, Takeshi
    Koizumi, Hiroyasu
    Hiraba, Haruto
    Hanawa, Takao
    Matsumura, Hideo
    Yoneyama, Takayuki
    DENTAL MATERIALS JOURNAL, 2023, 42 (03) : 418 - 425
  • [32] Bone integration capability of alkali- and heat-treated nanobimorphic Ti-15Mo-5Zr-3Al
    Tsukimura, Naoki
    Ueno, Takeshi
    Iwasa, Fuminori
    Minamikawa, Hajime
    Sugita, Yoshihiko
    Ishizaki, Ken
    Ikeda, Takayuki
    Nakagawa, Kaori
    Yamada, Masahiro
    Ogawa, Takahiro
    ACTA BIOMATERIALIA, 2011, 7 (12) : 4267 - 4277
  • [33] Dissimilar Brazing of Ti-15Mo-5Zr-3Al and Commercially Pure Titanium Using Ti-Cu-Ni Foil
    Yue, Gui-Lin
    Chen, Tai-Cheng
    Shiue, Ren-Kae
    Tsay, Leu-Wen
    MATERIALS, 2021, 14 (20)
  • [34] Biocompatible low Young's modulus achieved by strong crystallographic elastic anisotropy in Ti-15Mo-5Zr-3Al alloy single crystal
    Lee, S. -H.
    Todai, M.
    Tane, M.
    Hagihara, K.
    Nakajima, H.
    Nakano, T.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2012, 14 : 48 - 54
  • [35] MEASUREMENT OF INTERFACIAL SHEAR STRENGTHS IN SIC (CVD) FIBER-REINFORCED TI-15MO-5ZR-3AL COMPOSITE BY PUSH-OUT TECHNIQUE
    KAGAWA, Y
    OKURA, A
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (03) : 278 - 284
  • [36] Development of Single Crystalline Bone Plate with Low Young's Modulus Using Beta-type Ti-15Mo-5Zr-3Al Alloy
    Todai, Mitsuharu
    Hagihara, Koji
    Ishimoto, Takuya
    Yamamoto, Kengo
    Nakano, Takayoshi
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2015, 101 (09): : 501 - 505
  • [37] Microstructure Evolution in Adiabatic Shear Band in Ti-5Mo-5V-2Cr-3Al Alloy
    You Zhenping
    Mi Xujun
    Hui Songxiao
    Ye Wenjun
    Yu Yang
    Wang Bo
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (07) : 1184 - 1187
  • [38] Microstructure Evolution of Adiabatic Shear Band in Ti-15Mo-3Al-2.7Nb-0.2Si Alloy
    Cheng Xingwang
    Sun Kun
    Wang Fuchi
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (10) : 1756 - 1759
  • [39] Microstructure evolution of adiabatic shear band in Ti-15Mo-3Al-2.7Nb-0.2Si alloy
    Cheng, Xingwang
    Sun, Kun
    Wang, Fuchi
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2008, 37 (10): : 1756 - 1759
  • [40] FATIGUE-CRACK PROPAGATION IN BETA-TI-15MO-5ZR-3AL ALLOY
    TOKAJI, K
    BIAN, JC
    SHIOTA, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1995, 81 (09): : 930 - 935