共 50 条
- [43] Influence of lateral critical current density distributions on AC transport losses for Ag-sheathed (Bi,Pb)-2223 multifilamentary tapes with different filament arrangements MATERIALS FOR HIGH-TEMPERATURE SUPERCONDUCTOR TECHNOLOGIES, 2002, 689 : 193 - 198
- [45] WORK INSTABILITY AND ITS INFLUENCE ON THE CRITICAL CURRENT-DENSITY OF SILVER SHEATHED BI2223 TAPES SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1992, 5 (01): : 1 - 6
- [46] Critical current density of Ag-sheathed (Bi,Pb)2223 tapes produced by various thermo-mechanical treatment patterns PHYSICA C, 1997, 281 (01): : 64 - 68
- [47] Effect of powder pre-annealing on microstructural development inside Bi2223/Ag-sheathed tapes Journal of Materials Science, 2005, 40 : 213 - 214
- [49] Spatial distribution of critical current and supercurrent density in individual filaments extracted from Ag-sheathed Bi-2223 tapes PHYSICA B, 2000, 284 : 2071 - 2072