Torsional Shear Strength Tests for Glass-Ceramic Joined Silicon Carbide

被引:15
|
作者
Ferraris, Monica [1 ]
Ventrella, Andrea [1 ]
Salvo, Milena [1 ]
Katoh, Yutai [2 ]
Gross, Dietmar [3 ]
机构
[1] Politecn Torino, Dept Appl Sci & Technol, I-10129 Turin, Italy
[2] Oak Ridge Natl Lab, Mat Sci & Technol Div, Oak Ridge, TN 37831 USA
[3] Tech Univ Darmstadt, Div Solid Mech, D-64289 Darmstadt, Germany
关键词
A-RINGS - Mixed mode fracture - Torsional shear;
D O I
10.1111/ijac.12248
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A torsion test on hour-glass-shaped samples with a full joined or a ring-shaped joined area was chosen to measure shear strength of glass-ceramic joined silicon carbide. Shear strength of about 100 MPa was measured for full joined SiC with fracture completely inside their joined area. Attempts to obtain this shear strength with a ring-shaped joined area failed due to mixed mode fractures. On the contrary, full joined and ring-shaped steel hour-glasses joined by a glass-ceramic gave the same shear strength, thus suggesting that this test measures shear strength of joined components only when their fracture is completely inside their joined area.
引用
收藏
页码:693 / 699
页数:7
相关论文
共 50 条
  • [21] FATIGUE BEHAVIOR OF BOROSILICATE GLASS-CERAMIC MATRIX, NICALON (SILICON-CARBIDE) FIBER COMPOSITES
    RAMAKRISHNAN, V
    JAYARAMAN, N
    JOURNAL OF MATERIALS SCIENCE, 1993, 28 (20) : 5580 - 5591
  • [22] Mechanical behavior of silicon carbide fiber-reinforced strontium aluminosilicate glass-ceramic composites
    Bansal, NP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 231 (1-2): : 117 - 127
  • [23] FLEXURAL STRENGTH OF AN INFUSED CERAMIC, GLASS-CERAMIC, AND FELDSPATHIC PORCELAIN
    GIORDANO, RA
    PELLETIER, L
    CAMPBELL, S
    POBER, R
    JOURNAL OF PROSTHETIC DENTISTRY, 1995, 73 (05): : 411 - 418
  • [24] Torsional Shear Strength of Adhesive-Joined Steel in Saline Environments
    Benelli, Alessandro
    De La Pierre, Stefano
    Ferraris, Monica
    ADVANCED ENGINEERING MATERIALS, 2024, 26 (18)
  • [25] ENVIRONMENTAL AGING EFFECTS IN A SILICON-CARBIDE FIBER-REINFORCED GLASS-CERAMIC MATRIX COMPOSITE
    PLUCKNETT, KP
    SUTHERLAND, S
    DANIEL, AM
    CAIN, RL
    WEST, G
    TAPLIN, DMR
    LEWIS, MH
    JOURNAL OF MICROSCOPY-OXFORD, 1995, 177 : 251 - 263
  • [26] MICROSTRUCTURE AND HIGH-STRENGTH GLASS-CERAMIC COATINGS
    Gajek, Marcin
    Partyka, Janusz
    Lis, Jerzy
    DEVELOPMENTS IN STRATEGIC MATERIALS AND COMPUTATIONAL DESIGN V, 2015, : 169 - 174
  • [27] PROCESSES INVOLVED IN PRODUCTION OF CORDIERITE GLASS-CERAMIC FROM AMORPHOUS CHARGE IN PRESENCE OF SILICON-CARBIDE
    RUDENKO, NP
    SHVEDENKOV, GY
    KUZYUTIN, VP
    STREKHLETOV, AN
    INORGANIC MATERIALS, 1992, 28 (07) : 1234 - 1238
  • [28] STRENGTH AND DURABILITY OF A GLASS-CERAMIC CONTAINING SPODUMENE CRYSTALS
    KAY, JF
    DOREMUS, RH
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1974, 57 (11) : 480 - 482
  • [29] Bond Strength of Basalt Based Glass-Ceramic Coatings
    Bayrak, G.
    Ercenk, E.
    Sen, U.
    Yilmaz, S.
    ACTA PHYSICA POLONICA A, 2014, 125 (02) : 620 - 622
  • [30] STRENGTH OF A DENTAL GLASS-CERAMIC AFTER SURFACE COATING
    ROSENSTIEL, SF
    GUPTA, PK
    VANDERSLUYS, RA
    ZIMMERMAN, MH
    DENTAL MATERIALS, 1993, 9 (04) : 274 - 279