Growth of β-Sic interlayers on WC-Co substrates with varying hydrogen/tetramethylsilane flow ratio for adhesion enhancement of diamond coatings

被引:14
|
作者
Hei, Hongjun [1 ]
Yu, Shengwang [1 ]
Shen, Yanyan [1 ]
Li, Xiaojing [2 ]
Ma, Jing [1 ]
Tang, Bin [1 ]
Tang, Weizhong [3 ]
机构
[1] Taiyuan Univ Technol, Res Inst Surface Engn, Taiyuan 030024, Peoples R China
[2] Ordnance Sci Inst China, Ningbo Branch, Ningbo 315103, Zhejiang, Peoples R China
[3] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
beta-SiC films; H-2/TMS flow ratios; WC-Co substrates; Interlayers; Diamond coatings; CHEMICAL-VAPOR-DEPOSITION; TUNGSTEN CARBIDE; FILMS; STRENGTH; PRETREATMENT; TEMPERATURE; PERFORMANCE; RAMAN;
D O I
10.1016/j.surfcoat.2015.03.054
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cubic silicon carbide (beta-SiC) thin films were synthesized on cemented carbide (WC-Co) substrates as an interlayer for modifying the adhesion of diamond coatings. The influence of varying the hydrogen (H-2)/tetramethylsilane (TMS) flow ratios on the microstructure, phase composition and adhesion of the beta-SiC films was investigated. It was found that with the increase of the H-2/TMS flow ratios, the SiC crystallite size increases from 6.5 nm to 22.2 nm. When the flow ratio was 40:5, the film was formed of loose cauliflower-like agglomerates, containing SiC granular particles. With the flow ratio increased from 40:5 to 120:5, the films became more uniform and denser, resulting in adhesion enhancement. However, when the ratio increased from 160:5 to 200:5, clusters composed of faceted particles replaced the agglomerates, and the adhesion reduced. The beta-SiC film deposited with a H2/TMS flow ratio of 120:5 possessed a more uniform and denser structure, as well as better adhesion than the others. After subsequent diamond deposition, homogeneous nanocrystalline diamond coatings were realized on the beta-Sic interlayered substrates. Compared with the results on the well-known two-step chemically etched substrates, the diamond coatings deposited on the substrates with the beta-Sic interlayer possess excellent adhesion. It was also validated in this research that the beta-Sic interlayer deposited with a H2/TMS flow ratio of 120:5 was effective in enhancing the adhesion of diamond coatings prepared on WC-Co substrates. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:278 / 284
页数:7
相关论文
共 50 条
  • [41] Effect of deposition parameters on micro- and nano-crystalline diamond films growth on WC-Co substrates by HFCVD
    Zhang, Jian-guo
    Wang, Xin-chang
    Shen, Bin
    Sun, Fang-hong
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (10) : 3181 - 3188
  • [42] Diamond growth on WC-Co substrates by hot filament chemical vapor deposition: Effect of filament-substrate separation
    Wei, Qiuping
    Ashfold, Michael N. R.
    Mankelevich, Yu A.
    Yu, Z. M.
    Liu, P. Z.
    Ma, L.
    DIAMOND AND RELATED MATERIALS, 2011, 20 (5-6) : 641 - 650
  • [43] MURAKAMI AND H2SO4/H2O2 PRETREATMENT OF WC-CO HARD METAL SUBSTRATES TO INCREASE THE ADHESION OF CVD DIAMOND COATINGS
    HAUBNER, R
    KUBELKA, S
    LUX, B
    GRIESSER, M
    GRASSERBAUER, M
    JOURNAL DE PHYSIQUE IV, 1995, 5 (C5): : 753 - 760
  • [44] Murakami and H2SO4/H2O2 pretreatment of WC-Co hard metal substrates to increase the adhesion of CVD diamond coatings
    Haubner, R.
    Kubelka, S.
    Lux, B.
    Griesser, M.
    Grasserbauer, M.
    Journal De Physique, 1995, 5 (06) : 5 - 753
  • [45] ENHANCEMENT OF ADHESION STRENGTH AND TRIBOLOGICAL PERFORMANCE OF CVD DIAMOND FILMS ON TUNGSTEN CARBIDE SUBSTRATES WITH HIGH COBALT CONTENT VIA AMORPHOUS SiC INTERLAYERS
    He, Yuanping
    Cui, Yu-Xiao
    Sun, Fang-Hong
    SURFACE REVIEW AND LETTERS, 2019, 26 (09)
  • [46] Gradient-Modified HfC-SiC Mixed Bi-Interlayers Synthesized under Different TMS Flow Rate Increment for Depositing Diamond Coating onto WC-Co Substrate
    Zheng, Ke
    Gao, Jie
    Yu, Shengwang
    Wang, Yongsheng
    Hei, Hongjun
    Ma, Yong
    Zhou, Bing
    Tang, Bin
    Wu, Yucheng
    MATERIALS, 2020, 13 (07)
  • [47] Improvement to the adhesion of polycrystalline diamond films on WC-Co cemented carbides through ion etching of loosely bound growth centers
    Linnik, S. A.
    Gaydaychuk, A. V.
    Okhotnikov, V. V.
    SURFACE & COATINGS TECHNOLOGY, 2018, 334 : 227 - 232
  • [48] Effects of urea versus N2 addition on growth and mechanical properties of HFCVD diamond films on WC-Co substrates
    Wang, Xinchang
    Song, Xin
    Qiao, Yu
    Larsson, Karin
    Sun, Fanghong
    DIAMOND AND RELATED MATERIALS, 2022, 125
  • [49] Tribological Behavior of Ni-Based WC-Co Coatings Deposited via Spray and Fuse Technique Varying the Oxygen Flow
    Jimenez, H.
    Olaya, J. J.
    Alfonso, J. E.
    ADVANCES IN TRIBOLOGY, 2021, 2021
  • [50] Effects of carbon concentration and gas pressure with hydrogen-rich gas chemistry on synthesis and characterizations of HFCVD diamond films on WC-Co substrates
    Wang, Hua
    Wang, Chengchuan
    Wang, Xinchang
    Sun, Fanghong
    SURFACE & COATINGS TECHNOLOGY, 2021, 409