A reinvestigation of the validity of the indentation fracture (IF) method as applied to ceramics

被引:22
|
作者
Miyazaki, Hiroyuki [1 ]
Yoshizawa, Y. [1 ]
机构
[1] AIST, Moriyama Ku, Anagahora 2266-98, Nagoya, Aichi 4638560, Japan
关键词
Indentation; Toughness; Indentation fracture resistance; SILICON-NITRIDE CERAMICS; ELASTIC-PLASTIC INDENTATION; POWERFUL OPTICAL MICROSCOPY; TOUGHNESS TEST; INDUCED DENSIFICATION; BRITTLE SOLIDS; ROUND-ROBIN; CRACK; RESISTANCE; MICROSTRUCTURES;
D O I
10.1016/j.jeurceramsoc.2017.07.027
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Poor correlation between indentation fracture resistance, K-IFR, and fracture toughness, K-IC, has long been considered a weak point of the indentation fracture (IF) method of materials analysis. The present work therefore assessed the reliability of the experimental data that has historically been used for comparisons of K-IFR and K-IC. A painstaking survey of primary literature reports concerning the IF method revealed that the comparisons of K-IC with K-IFR in most studies were imperfect because both K-IC and K-IFR were measured using unreliable techniques and because improper test materials such as silicate glass were employed. These findings indicate that the standard objections against the use of the IF model are not well supported, and also that the majority of the empirically-derived calibration constants used in various IF equations are suspect. Accordingly, it is evident that new experimental measurements using the latest and most reliable techniques will be required to allow well-informed discussions of the validity of this test method in future.
引用
收藏
页码:4437 / 4441
页数:5