A reinvestigation of the validity of the indentation fracture (IF) method as applied to ceramics

被引:22
|
作者
Miyazaki, Hiroyuki [1 ]
Yoshizawa, Y. [1 ]
机构
[1] AIST, Moriyama Ku, Anagahora 2266-98, Nagoya, Aichi 4638560, Japan
关键词
Indentation; Toughness; Indentation fracture resistance; SILICON-NITRIDE CERAMICS; ELASTIC-PLASTIC INDENTATION; POWERFUL OPTICAL MICROSCOPY; TOUGHNESS TEST; INDUCED DENSIFICATION; BRITTLE SOLIDS; ROUND-ROBIN; CRACK; RESISTANCE; MICROSTRUCTURES;
D O I
10.1016/j.jeurceramsoc.2017.07.027
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Poor correlation between indentation fracture resistance, K-IFR, and fracture toughness, K-IC, has long been considered a weak point of the indentation fracture (IF) method of materials analysis. The present work therefore assessed the reliability of the experimental data that has historically been used for comparisons of K-IFR and K-IC. A painstaking survey of primary literature reports concerning the IF method revealed that the comparisons of K-IC with K-IFR in most studies were imperfect because both K-IC and K-IFR were measured using unreliable techniques and because improper test materials such as silicate glass were employed. These findings indicate that the standard objections against the use of the IF model are not well supported, and also that the majority of the empirically-derived calibration constants used in various IF equations are suspect. Accordingly, it is evident that new experimental measurements using the latest and most reliable techniques will be required to allow well-informed discussions of the validity of this test method in future.
引用
收藏
页码:4437 / 4441
页数:5
相关论文
共 50 条
  • [1] Monitoring of indentation fracture in CuO ceramics utilizing an electrical method
    Nakamichi, A
    Kishimoto, A
    Nakamura, Y
    Yanagida, H
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (03) : 249 - 251
  • [2] Fracture toughness of dental ceramics: comparison of bending and indentation method
    Fischer, H
    Marx, R
    DENTAL MATERIALS, 2002, 18 (01) : 12 - 19
  • [3] ELASTIC/PLASTIC INDENTATION IN CERAMICS: A FRACTURE TOUGHNESS DETERMINATION METHOD.
    Miranzo, P.
    Moya, J.S.
    Ceramics International, 1984, 10 (04) : 147 - 152
  • [4] INDENTATION FRACTURE EXAMINATIONS OF ENGINEERING CERAMICS
    DIETZ, M
    BUHLING, L
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 1995, 26 (11-12) : 615 - 622
  • [5] ACOUSTIC MICROSCOPY OF CERAMICS INDENTATION FRACTURE
    YAMANAKA, K
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1985, 24 : 184 - 186
  • [6] Indentation fracture of polycrystalline cubic ceramics
    Cook, Robert F.
    Liniger, Eric G.
    Pascucci, Marina R.
    Journal of hard materials, 1994, 5 (04): : 191 - 212
  • [7] Test method for fracture toughness of monolithic ceramics by indentation fracture (IF) method: Improvement of reliability and international standardization activity
    Miyazaki H.
    Yasuda K.
    Yoshizawa Y.-I.
    Synthesiology, 2021, 13 (01): : 29 - 44
  • [8] Fracture-toughness measurement of dental ceramics using the indentation fracture method with different formulas
    Maehara, S
    Fujishima, A
    Hotta, Y
    Miyazaki, T
    DENTAL MATERIALS JOURNAL, 2005, 24 (03) : 328 - 334
  • [9] FRACTURE TOUGHNESS OF CERAMICS BY THE VICKERS INDENTATION CRACK LENGTH METHOD: A CRITICAL REVIEW
    Quinn, George D.
    MECHANICAL PROPERTIES AND PERFORMANCE OF ENGINEERING CERAMICS AND COMPOSITES II, 2007, 27 (02): : 45 - 62
  • [10] Statistical analysis of fracture toughness of SiC ceramics determined by Vickers indentation method
    Curkovic L.
    Rede V.
    Lalic M.
    International Journal of Microstructure and Materials Properties, 2011, 6 (05) : 359 - 365