摘要
A detailed study of the kinetics of discontinuous precipitation (DP) and type I discontinuous coarsening (DCI) in Zn-4 at % Ag alloy is reported here for the first time. DCI succeeds DP during prolonged isothermal ageing. Both DP and DCI are characterized by a predominantly lamellar morphology of the precipitate phase, statistically constant interlamellar spacing and steady state reaction front (RF) velocity at a given temperature. The interlamellar spacing increases with temperature. The RF velocity shows a C-curve behavior for DP, but increases monotonically for DCI, as a function of temperature. DCI is distinguished from DP by a 3-5 times larger interlamellar spacing and 1-2 orders of magnitude lower RF velocity than those of DP under comparable conditions. DCI may be initiated from an interface between two DP colonies, a former DP-RF, or the free surface intersecting a DP colony. Kinetic analysis of DP using the models of Turnbull, Cahn, Hillert, and Petermann and Hornbogen, and of DCI using the modified Petermann and Hornbogen model (by Fournelle) have yielded grain boundary diffusivity data in the temperature range 353-573 K. Subsequent Arrhenius analysis shows that the activation energy of the DP and DCI processes lies between 50-66 kJ mol(-1). The latter is comparable with the activation energy of grain-boundary self-diffusion of Zn and is nearly half that of tracer impurity diffusion (volume/bulk) of Ag in Zn. Hence, it is concluded that DP and DCI are grain-boundary diffusion-controlled processes in the present alloy. (C) 1999 Kluwer Academic Publishers.
引用
收藏
页码:773 / 781
页数:9
相关论文
共 50 条
  • [21] DISCONTINUOUS COARSENING AND DISSOLUTION IN AN FE-13.5 AT-PERCENT ZN ALLOY
    CHUANG, TH
    GUST, W
    PREDEL, B
    FOURNELLE, RA
    JOURNAL OF METALS, 1987, 39 (10): : A81 - A81
  • [22] DISCONTINUOUS COARSENING OF DISCONTINUOUS PRECIPITATE IN A NI-7.5 AT-PERCENT IN ALLOY
    CHUANG, TH
    FOURNELLE, RA
    GUST, W
    PREDEL, B
    ACTA METALLURGICA, 1988, 36 (03): : 775 - 785
  • [23] Discontinuous coarsening of discontinuous precipitates in a Co-6 at.% Mo alloy
    Lee, SL
    Lee, KC
    Chuang, TH
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 251 (1-2): : 135 - 141
  • [24] KINETICS OF CELLULAR PRECIPITATION AND DISCONTINUOUS COARSENING OF THE CELLULAR PRECIPITATE IN CU-SB ALLOYS
    BALASUBRAHMANYAM, VV
    GUPTA, SP
    ACTA METALLURGICA, 1989, 37 (01): : 291 - 301
  • [25] On the initiation, growth, and coarsening of discontinuous precipitation in Cu-10 at.%Co alloy
    N. M. Suguihiro
    I. G. Solórzano
    Journal of Materials Science, 2016, 51 : 71 - 81
  • [26] On the initiation, growth, and coarsening of discontinuous precipitation in Cu-10 at.%Co alloy
    Suguihiro, N. M.
    Solrzano, I. G.
    JOURNAL OF MATERIALS SCIENCE, 2016, 51 (01) : 71 - 81
  • [27] Dilatometric and DSC Study of the Kinetics of Discontinuous Precipitation of Ag2Al Intermetallic in Al – 10% Ag Alloy
    H. Belhouchet
    M. Fatmi
    F. Sahnoune
    M. Heraiz
    N. Saheb
    Metal Science and Heat Treatment, 2018, 60 : 185 - 189
  • [28] Effect of heat treatments on discontinuous precipitation kinetics in Al-30 wt.% Zn alloy
    Boumerzoug, Z.
    Fatmi, M.
    MATERIALS CHARACTERIZATION, 2009, 60 (08) : 768 - 774
  • [29] Discontinuous precipitation of spinodal Al-Zn alloy with symmetrical composition
    Wang, Da-Peng
    Hao, Shi-Ming
    Dong, Dan-Yang
    Zhao, Gang
    Dongbei Daxue Xuebao/Journal of Northeastern University, 2003, 24 (05): : 467 - 470
  • [30] Effect of an applied stress on discontinuous precipitation in a Cu-Ag alloy
    Monzen, R.
    Terazawa, T.
    Watanabe, C.
    15TH INTERNATIONAL CONFERENCE ON THE STRENGTH OF MATERIALS (ICSMA-15), 2010, 240