The initial steps of atmospheric corrosion on magnesium alloy AZ91D

被引:54
|
作者
Jonsson, Martin [1 ]
Persson, Dan [1 ]
Gubner, Rolf [1 ]
机构
[1] KIMAB, Corros & Mat Res Inst, S-11428 Stockholm, Sweden
关键词
D O I
10.1149/1.2779957
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Magnesium, with its low density, is a very interesting metal in applications in which weight is important. In this work the initiation of corrosion attacks on magnesium alloy AZ91D has been investigated under atmospheric conditions, using confocal laser scanning microscopy and SKPFM. The corrosion attack starts in the alpha phase in larger grains and is under atmospheric conditions initiated at the boundary between the alpha phase and the eutectic alpha-/beta phase. The SKPFM measurement shows that a high Volta potential difference exists between the larger grains and the surrounding eutectic alpha-/beta phase and the beta phase. A microgalvanic element is formed in the thin adlayer on the surface, with anodic Mg dissolution in the alpha phase and the cathodic reaction primarily in the eutectic alpha-/beta phase. The initiation in the larger grains could be explained by the smaller aluminum content in the larger grains due to the solidification process. Even though intermetallic Al-Mn particles show a high Volta potential difference with the connecting alpha phase, they are not involved in the initiation of the corrosion. This is explained by the position within the microstructure of Al-Mn particles embedded in the beta phase and located away from the alpha phase.
引用
收藏
页码:C684 / C691
页数:8
相关论文
共 50 条
  • [31] Improved corrosion performance of AZ91D magnesium alloy coated with the KERONITE™ process
    Shrestha, S
    Sturgeon, A
    Shashkov, P
    Shatrov, A
    MAGNESIUM TECHNOLOGY 2002, 2002, : 283 - 287
  • [32] Effect of surface nanocrystallization on the microstructural and corrosion characteristics of AZ91D magnesium alloy
    Laleh, M.
    Kargar, Farzad
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (37) : 9150 - 9156
  • [33] Study of the corrosion inhibition effect of sodium silicate on AZ91D magnesium alloy
    Gao, H.
    Li, Q.
    Chen, F. N.
    Dai, Y.
    Luo, F.
    Li, L. Q.
    CORROSION SCIENCE, 2011, 53 (04) : 1401 - 1407
  • [35] Improving corrosion resistance of AZ91D magnesium alloy by nitrogen ion implantation
    Nakatsugawa, I
    Martin, R
    Knystautas, EJ
    CORROSION, 1996, 52 (12) : 921 - 926
  • [36] Improvement on the corrosion resistance of AZ91D magnesium alloy by aluminum diffusion coating
    Huo, Hongwei
    Li, Ying
    Wang, Fuhui
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2007, 23 (03) : 379 - 382
  • [37] Effect of Heat Treatment on Microstructure and Corrosion Behavior of Az91d Magnesium Alloy
    Lih, Chye T.
    Zamzuri, M. Z. M.
    Norbahiyah, S.
    Ismail, K. A.
    Derman, M. N. B.
    Illias, S.
    ADVANCED MATERIALS RESEARCH III, 2013, 685 : 102 - +
  • [38] Corrosion behavior of an AZ91D magnesium alloy under a heterogeneous electrolyte layer
    Wang, Yanhua
    Zhen, Cheng
    Zhang, Zhan
    Tao, Zhencheng
    PLOS ONE, 2020, 15 (06):
  • [39] Improving corrosion resistance of AZ91D magnesium alloy by nitrogen ion implantation
    Inst of Magnesium Technology, Rue Franquet, Canada
    Corrosion (Houston), 12 (921-926):
  • [40] Corrosion Behavior of thixoformed AZ91D magnesium alloy in NaCl aqueous solution
    Xu, Weijun
    Ma, Ying
    Chen, Tijun
    Hao, Yuan
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 2611 - 2614