Deformation induced degradation of hot-dip aluminized steel

被引:12
|
作者
Lemmens, B. [1 ,2 ]
Springer, H. [3 ]
Peeters, M. [1 ]
De Graeve, I. [1 ,2 ]
De Strycker, J. [4 ]
Raabe, D. [3 ]
Verbeken, K. [1 ]
机构
[1] Ghent Univ UGent, Dept Mat Text & Chem Engn, Technol Pk 903, B-9052 Zwijnaarde, Belgium
[2] Vrije Univ Brussel, Res Grp Electrochem & Surface Engn SURF, Pl Laan 2, B-1050 Brussels, Belgium
[3] Max Planck Inst Eisenforsch GmbH, D-40237 Dusseldorf, Germany
[4] ArcelorMittal Global R&D Gent, JF Kennedylaan 3, B-9060 Zelzate, Belgium
关键词
Hot-dip aluminizing; Intermetallics; Post-processing; Aluminium; Iron; Deformation; AL; COATINGS; SILICON; SCALE; LAYER;
D O I
10.1016/j.msea.2017.10.094
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work the fracture and corrosion behaviour of hot-dip aluminized steels is investigated in controlled dipping experiments which allowed to separately study the effects of Si in the Al bath (1-10 wt%) and the intermetallic phase thickness (5-30 mu m). The addition of Si had no direct influence on the performance of the coating system for similar thickness values of the IMP seam, which in turn showed to be the dominant factor independent from the amount of Si. Thin intermetallic phase seams ( < about 10 mu m) exhibited more (about 5-10 per 100 mu m interfacial length) but smaller cracks with a fishnet pattern on the outer Al-Si coating, which remained intact and interconnected until a tensile deformation of 15-20%. Thicker intermetallic phase seams resulted in less (about 2 per 100 mu m interfacial length) but broader cracks perpendicular to the tensile direction, giving rise to a lamellar pattern on the Al-Si coating, which cracks and uncovers the steel already at strains below 10%, and readily flakes off leaving the steel substrate to accelerated corrosion in chloride environments. Our results indicate that the reduction of the intermetallic phase seam thickness remains the main target to improve the performance of hot-dip aluminized coated steel by combining appropriate Si additions with minimized dipping temperatures and times.
引用
收藏
页码:385 / 391
页数:7
相关论文
共 50 条
  • [21] Effect of deformation on the electrochemical behavior of hot-dip galvanized steel sheets
    Vagge, S. T.
    Raja, V. S.
    Narayanan, R. Ganesh
    APPLIED SURFACE SCIENCE, 2007, 253 (20) : 8415 - 8421
  • [22] Research on Corrosion Inhibitors for Coatings on Hot-Dip Aluminized-Galvanized Steel in Marine Environment
    Zhenkai Xu
    Lian Chen
    Jingliang Han
    Chengfei Zhu
    Russian Journal of Physical Chemistry A, 2023, 97 (9) : 2044 - 2051
  • [23] Research on Corrosion Inhibitors for Coatings on Hot-Dip Aluminized-Galvanized Steel in Marine Environment
    Xu, Zhenkai
    Chen, Lian
    Han, Jingliang
    Zhu, Chengfei
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY A, 2023, 97 (09) : 2044 - 2051
  • [24] Heat Treatment Effect on Corrosion Resistance of Mg Coating Film on Hot-Dip Aluminized Steel
    Kim, Soon-Ho
    Lee, Seung-Hyo
    Lee, Myeong-Hoon
    SCIENCE OF ADVANCED MATERIALS, 2022, 14 (07) : 1220 - 1230
  • [25] Crystallographic features of Al4C3 phase in hot-dip aluminized steel
    School of Materials Science and Engineering, Henan University of Science and Technology, Luoyang 471003, China
    不详
    不详
    Cailiao Rechuli Xuebao, 2006, 2 (75-78):
  • [26] Micro-scale Observation of Corrosion of Hot-Dip Aluminized 11% Cr Stainless Steel
    Cho, Min-Seung
    Park, Choong-Nyeon
    Park, Chan-Jin
    CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2019, 18 (03): : 73 - 77
  • [27] The hot corrosion resistance of hot-dip aluminized low carbon steel with nickel interlayer under static load
    Liang, Huan-Chang
    Wang, Chaur-Jeng
    SURFACE & COATINGS TECHNOLOGY, 2018, 350 : 496 - 501
  • [28] Steel loss of hot-dip galvanizing
    Mei, Jianting
    Wu, Yongmin
    Cailiao Baohu/Materials Protection, 1997, 30 (07): : 12 - 13
  • [29] Continuous hot-dip aluminizing of steel
    Jinshu Rechuli/Heat Treatment of Metals, 2000, (05): : 15 - 17
  • [30] COATINGS FOR HOT-DIP GALVANIZED STEEL
    VANOETER.KA
    FETTE SEIFEN ANSTRICHMITTEL VERBUNDEN MIT DER ZEITSCHRIFT DIE ERNAHRUNGSINDUSTRIE, 1971, 73 (12): : 717 - &