Effects of temperature on the weathering of engineering thermoplastics

被引:47
|
作者
Pickett, J. E. [1 ]
Gibson, D. A. [1 ]
Rice, S. T. [1 ]
Gardner, M. M. [1 ]
机构
[1] GE Global Res, Niskayuna, NY 12309 USA
关键词
accelerated weathering; activation energy; thermoplastics; polycarbonate;
D O I
10.1016/j.polymdegradstab.2007.12.013
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
We have determined the activation energies (E-a) of yellowing and gloss loss for a large number of engineering thermoplastics and blends under accelerated weathering conditions. The E-a often depend on the property measured and exposure conditions, although they vary over a fairly small range. Under the CIRA/sodalime-filtered xenon arc conditions most likely to be representative of outdoor exposure, the E-a for gloss loss was <= 5 kcal/mol for all samples tested. The E-a for yellowing was also <= 5 kcal/mol except for SAN and ABS. Evidently the color bodies formed from photo-oxidation of SAN are more sensitive to temperature. A reaction with an E-a of 5 kcal/mol will increase its rate by about 33% for each 10 degrees C increase in temperature near room temperature. Temperature is an important, but not overwhelming, variable in the weathering of most engineering thermoplastics. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:684 / 691
页数:8
相关论文
共 50 条
  • [41] Engineering a change: What lies ahead for engineering thermoplastics?
    Robinson, S.
    European Plastics News, 1996, 23 (05):
  • [42] EFFECTS OF COMPOUNDING TECHNIQUES ON THE PROPERTIES OF MICA-REINFORCED ENGINEERING THERMOPLASTICS.
    Wright, A.N.
    Hawley, G.C.
    Advances in Polymer Technology, 1987, 7 (03) : 259 - 265
  • [43] VACUUM WEATHERING OF SULFUR - TEMPERATURE EFFECTS AND APPLICATIONS TO IO
    NASH, DB
    MOSES, JI
    GEOPHYSICAL RESEARCH LETTERS, 1988, 15 (07) : 697 - 700
  • [44] The Effect of Recycle on the Properties of Engineering Thermoplastics
    DeRudder, James
    Yang, Yuzhen
    He, Yuanqing
    Zhao, Wei
    Flores, Amanda
    PLASTICS ENGINEERING, 2012, 68 (08) : 26 - 29
  • [45] FIRE RESISTANCE IN ADVANCED ENGINEERING THERMOPLASTICS
    TESORO, GC
    ACS SYMPOSIUM SERIES, 1990, 425 : 241 - 252
  • [46] PES AND PEEK - TOUGH ENGINEERING THERMOPLASTICS
    BERGENN, WR
    RIGBY, RB
    CHEMICAL ENGINEERING PROGRESS, 1985, 81 (01) : 36 - 38
  • [47] Review of flame retardant engineering thermoplastics
    Hochberg, A
    TOMORROW'S TRENDS IN FIRE RETARDANT REGULATIONS, TESTING, APPLICATIONS AND CURRENT TECHNOLOGIES, 1996, : 159 - 169
  • [48] TWO NEW ENGINEERING THERMOPLASTICS.
    Anon
    PRT Polymer Age, 1973, 4 (06): : 204 - 205
  • [49] REACTIVE COUPLING OF FIBERS TO ENGINEERING THERMOPLASTICS
    DIBENEDETTO, AT
    HUANG, SJ
    BIRCH, D
    GOMEZ, J
    LEE, WC
    COMPOSITE STRUCTURES, 1994, 27 (1-2) : 73 - 82
  • [50] Blends of rigid and rubbery engineering thermoplastics
    Deanin, Rudolph D.
    Lee, S.Thomas