共 50 条
Strain effects on Co,N co-decorated graphyne catalysts for overall water splitting electrocatalysis
被引:38
|作者:
Gao, Xiaoping
[1
]
Zhou, Yanan
[2
]
Tan, Yujia
[1
]
Liu, Shiqiang
[1
]
Cheng, Zhiwen
[1
]
Shen, Zhemin
[1
,3
]
机构:
[1] Shanghai Jiao Tong Univ, Sch Environm Sci & Engn, Shanghai 200240, Peoples R China
[2] Sichuan Univ, Sch Chem Engn, Chengdu 610065, Sichuan, Peoples R China
[3] Shanghai Inst Pollut Control & Ecol Secur, Shanghai 200092, Peoples R China
关键词:
GENERALIZED GRADIENT APPROXIMATION;
HYDROGEN EVOLUTION REACTION;
OXYGEN EVOLUTION;
SINGLE ATOMS;
METAL;
CARBON;
NANOSHEETS;
MOLECULES;
EXCHANGE;
SURFACE;
D O I:
10.1039/c9cp05548g
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
Lattice strain, either tensile or compressive, can fine-tune the electronic structure of surfaces via altering the distances between surface atoms, thereby modifying the catalytic activity of catalysts. Numerous examples of strain engineering have been applied to various electrocatalysts for both hydrogen evolution reaction (HER) and oxygen evolution reaction (OER), but strain-optimized 2D carbon-based single-atom electrocatalysts for catalyzing the overall water splitting reaction have received little attention. Here, we applied the lattice strain of Co,N co-decorated graphyne (Co@N-1-GY) to directly optimize its catalytic activity for the overall water splitting reaction based on first-principles calculations. Our calculations suggest that compressive strain and tensile strain lead to less stability of Co@N-1-GY and the distances between C and Co atoms increase linearly with the strain changing from compressive to tensile, thus linearly upshifting the p-band center of C atoms and the d-band center of Co atoms. In addition, biaxial strain has more remarkable effects on these properties than uniaxial strain. From compressive to tensile strain, the chemisorption of electrochemically generated intermediates in both HER and OER becomes weaker and weaker. A tensile strain of 0.5% on Co@N-1-GY gives an ideal HER performance, while the OER reaches the minimum overpotential of 0.33 V under the biaxial tensile strain of 3%.