On the extent of fracture toughness transfer from 1D/2D nanomodified epoxy matrices to glass fibre composites

被引:26
|
作者
Domun, Nadiim [1 ]
Paton, Keith R. [2 ]
Blackman, Bamber R. K. [3 ]
Kaboglu, Cihan [3 ]
Vahid, Samireh [1 ]
Zhang, Tao [1 ]
Dear, John P. [3 ]
Kinloch, Anthony J. [3 ]
Hadavinia, Homayoun [1 ]
机构
[1] Kingston Univ London, Dept Mech Engn, London, England
[2] Natl Phys Lab, Hampton Rd, Teddington, Middx, England
[3] Imperial Coll London, Dept Mech Engn, London, England
关键词
MECHANICAL-PROPERTIES; MODE-I; TOUGHENING MECHANISMS; BEHAVIOR; DCB; PERFORMANCE; STRENGTH; FAILURE; ELS;
D O I
10.1007/s10853-019-04340-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the effects of adding nanofillers to an epoxy resin (EP) used as a matrix in glass fibre-reinforced plastic (GFRP) composites have been investigated. Both 1D and 2D nanofillers were used, specifically (1) carbon nanotubes (CNTs), (2) few-layer graphene nanoplatelets (GNPs), as well as hybrid combinations of (3) CNTs and boron nitride nanosheets, and (4) GNPs and boron nitride nanotubes (BNNTs). Tensile tests have shown improvements in the transverse stiffness normal to the fibre direction of up to about 25% for the GFRPs using the `EP ? CNT' and the `EP ? BNNT ? GNP' matrices, compared to the composites with the unmodified epoxy (`EP'). Mode I and mode II fracture toughness tests were conducted using double cantilever beam (DCB) and end-notched flexure (ENF) tests, respectively. In the quasi-static mode I tests, the values of the initiation interlaminar fracture toughness, GCIC, of the GFRP composites showed that the transfer of matrix toughness to the corresponding GFRP composite is greatest for the GFRP composite with the GNPs in the matrix. Here, a coefficient of toughness transfer (CTT), defined as the ratio of mode I initiation interlaminar toughness for the composite to the bulk polymer matrix toughness, of 0.68 was recorded. The highest absolute values of the mode I interlaminar fracture toughness at crack initiation were achieved for the GFRP composites with the epoxy matrix modified with the hybrid combinations of nanofillers. The highest value of the CTT during steady-state crack propagation was * 2 for all the different types of GFRPs. Fractographic analysis of the composite surfaces from the DCB and ENF specimens showed that failure was by a combination of cohesive (through the matrix) and interfacial (along the fibre/matrix interface) modes, depending on the type of nanofillers used.
引用
收藏
页码:4717 / 4733
页数:17
相关论文
共 50 条
  • [21] Classification of 1D and 2D Orbifolds
    Nilse, Lars
    SUSY06: The 14th International Conference on Supersymmetry and the Unification of Fundamental Interactions, 2007, 903 : 411 - 414
  • [22] Nonlinear Transient Heat Transfer and Optimisation of Multidirectional (1D/2D/3D) Functionally Graded Porous Composites
    Kumar, Samarjeet
    Kar, Vishesh Ranjan
    INTERNATIONAL JOURNAL OF COMPUTATIONAL METHODS, 2025,
  • [23] From 1D to 2D: Controllable Preparation of 2D Ni-MOFs for Supercapacitors
    Zhang, Xu
    Liu, Zhiqing
    Jin, Xingchen
    Liu, Fengrui
    Ma, Xinlei
    Qu, Ning
    Lu, Wang
    Tian, Yuhan
    Zhang, Qiang
    INORGANIC CHEMISTRY, 2023, 62 (19) : 7360 - 7365
  • [24] 1D, 2D, and 3D carbon nanostructures as additives in glassy and rubbery epoxy nanocomposites
    Xidas, Panagiotis I.
    Giliopoulos, Dimitrios J.
    Gournis, Dimitrios
    Bikiaris, Dimitrios N.
    Manias, Evangelos D.
    Triantafyllidis, Konstantinos S.
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2014, 248
  • [25] 1D "Spikelet" Projections from Heteronuclear 2D NMR Data-Permitting 1D Chemometrics While Preserving 2D Dispersion
    Anaraki, Maryam Tabatabaei
    Bermel, Wolfgang
    Majumdar, Rudraksha Dutta
    Soong, Ronald
    Simpson, Myrna
    Monnette, Martine
    Simpson, Andre J.
    METABOLITES, 2019, 9 (01):
  • [26] The transfer of matrix toughness to composite mode I interlaminar fracture toughness in glass-fibre/vinyl ester composites
    Compston, P
    Jar, PYB
    Burchill, PJ
    Takahashi, K
    APPLIED COMPOSITE MATERIALS, 2002, 9 (05) : 291 - 314
  • [27] The Transfer of Matrix Toughness to Composite Mode I Interlaminar Fracture Toughness in Glass-Fibre/vinyl Ester Composites
    P. Compston
    P.-Y. B. Jar
    P. J. Burchill
    K. Takahashi
    Applied Composite Materials, 2002, 9 : 291 - 314
  • [28] From 1D to 2D: dopamine constructed 2D NiCo-hydroxide nanosheets/graphene composites for high-performance supercapacitors†
    Zhang, Xu
    Yang, Shixuan
    Tian, Yuhan
    Liu, Anmin
    Lu, Wang
    Qu, Ning
    Guo, Minggang
    Mi, Panpan
    SUSTAINABLE ENERGY & FUELS, 2021, 5 (08): : 2373 - 2381
  • [29] 2D Microscale Observations of Interlaminar Transverse Tensile Fracture in Carbon/Epoxy Composites
    Smith, Austin J.
    Arndt, Caitlin M.
    Benson, Danielle
    Czabaj, Michael W.
    MECHANICS OF COMPOSITE, HYBRID AND MULTIFUNCTIONAL MATERIALS, VOL 5, 2019, : 181 - 183
  • [30] Cluster analysis of acoustic emission signals for 2D and 3D woven glass/epoxy composites
    Li, Li
    Lomov, Stepan V.
    Yan, Xiong
    Carvelli, Valter
    COMPOSITE STRUCTURES, 2014, 116 : 286 - 299