Lining of cast iron cylinder with copper alloy utilising high temperature oxidation

被引:0
|
作者
Yamazaki, T. [1 ]
Kikuta, T. [1 ]
Murata, Y. [2 ]
机构
[1] Toyama Univ, Grad Sch Sci & Engn, Toyama 9308555, Japan
[2] Nagoya Univ, Grad Sch Engn, Chikusa Ku, Nagoya, Aichi 4648603, Japan
关键词
Cast iron; Copper alloy; Decarburisation; High temperature oxidation; Bonding; INTERFACE; BEHAVIOR; STEEL;
D O I
10.1179/1743133610Y.0000000003
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Lining the inner surface of a cast iron hydraulic cylinder with copper alloy would generally not be possible. In this study, the surface of a cast iron cylinder was decarburised by high temperature oxidation. The cylinder, after decarburisation, was filled with borax anhydride and heated at a temperature of 1203 K. Molten copper alloy was then injected into the cylinder, displacing the molten borax anhydride. After cooling, the embedded copper alloy was drilled along its centre axis so that a prescribed thickness of the copper alloy remained. Thus, the cast iron cylinder could be successfully lined with copper alloy.
引用
收藏
页码:124 / 126
页数:3
相关论文
共 50 条