Features of Austenite Formation in Low-Carbon Steel upon Heating in the Intercritical Temperature Range

被引:5
|
作者
Panov, D. O. [1 ]
Smirnov, A. I. [2 ]
机构
[1] Perm Natl Res Polytech Univ, Perm 614990, Russia
[2] Novosibirsk State Tech Univ, Novosibirsk 630073, Russia
来源
PHYSICS OF METALS AND METALLOGRAPHY | 2017年 / 118卷 / 11期
关键词
low-carbon steel; austenite; intercritical temperature range; dilatometry; recrystallization; phase transformations; RECRYSTALLIZATION; MARTENSITE; KINETICS; ALLOY;
D O I
10.1134/S0031918X17110102
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The features of austenite formation upon continuous heating of low-carbon steel at the rates of 90-0.15 K/s in the intercritical temperature range (ICTR) have been studied. It has been found that, in the initially high-tempered, initially quenched, and initially cold-deformed steel, the alpha -> gamma transition in the ICTR consists of three stages. The thermokinetic diagrams of the austenite formation with the indication of the positions of the critical points Ac-1 and Ac-3 and also of the temperature ranges of the development of each identified stage of the alpha -> gamma transformation have been constructed. A complex of structural studies has been carried out, and a scheme of the austenite formation upon continuous heating at a rate of 90 K/s in the ICTR for the initially high-tempered steel, initially quenched steel, and initially cold-deformed low-carbon steel has been suggested, which reflects all stages of this process.