Evaluation of Microshear Bond Strength of Four Different CAD-CAM Polymer-Infiltrated Ceramic Materials after Thermocycling

被引:8
|
作者
Beyabanaki, Elaheh [1 ]
Ashtiani, Reza Eftekhar [1 ]
Feyzi, Marjan
Zandinejad, Amirali [2 ]
机构
[1] Shahid Beheshti Univ Med Sci, Dept Prosthodont, Sch Dent, Daneshjoo Bvld, Tehran, Iran
[2] Texas A&M Univ, Coll Dent, Comprehens Dent Dept, Dallas, TX USA
关键词
Hybrid ceramic; microshear bond strength; polymer-infiltrated ceramic network; resin cement; resin nanoceramic; zirconia-reinforced lithium silicate; MECHANICAL-PROPERTIES; COMPOSITE RESIN; FRACTURE-RESISTANCE; SELF-ADHESIVE; CEMENTS;
D O I
10.1111/jopr.13469
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose To evaluate the bond strength of three monolithic hybrid ceramics/resin nanoceramics and a zirconia-reinforced lithium silicate to resin cement after thermocycling. Materials and Methods Using four materials, including Vita Enamic (VITA Zahnfabrik), Lava Ultimate (3M ESPE), Crystal Ultra (Digital Dental), and Vita Suprinity (VITA Zahnfabrik), 64 specimens were prepared with dimensions of 4 mm x 3 mm x 1.5 mm. Vita Suprinity samples were sintered at 840 degrees C for 8 min. After polishing and cleaning all the samples in each group (n = 16), they were subjected to their recommended surface treatment: 10% hydrofluoric acid for Vita Enamic (60s) and Vita Suprinity (20s); air abrasion of Lava Ultimate and Crystal Ultra with 50 u Al2O3 particles. Then, tygon tubes were filled with dual cure resin cement (Panavia F2.0), cured and then subjected to thermal cycling (2000 cycles; 5-55 degrees C). The microshear bond strength was measured using microtensile testing machine. The data were analyzed using Welch and Games-Howell tests (alpha = 0.05). The mode of failure was also evaluated using a stereomicroscope. Results The highest and the lowest mean microshear bond strength belonged to the Crystal Ultra (7.71 +/- 1.54 MPa) and Vita Suprinity (4.73 +/- 1.87 MPa) groups, respectively. The differences between groups were significant and Crystal Ultra had higher bond strength in comparison to all three materials (p < 0.05). Conclusion Hybrid ceramics showed higher bond strength to resin cements in comparison to resin nanoceramics and zirconia-reinforced lithium silicate materials.
引用
收藏
页码:623 / 628
页数:6
相关论文
共 50 条
  • [41] Repair bond strength of different CAD-CAM ceramics after various surface treatments combined with laser irradiation
    Seda Üstün Aladağ
    Elif Aydoğan Ayaz
    Lasers in Medical Science, 38
  • [42] Comparison of optical properties and bond strength of new CAD/CAM ceramic materials
    Demir, Necla
    Bozkurt, Mehtap
    Temizci, Tugba
    MATERIALS RESEARCH EXPRESS, 2024, 11 (09)
  • [43] Effect of various surface treatments on relining bond strength of CAD-CAM denture base materials
    Karaokutan, Isil
    Ayvaz, Ilayda
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2024,
  • [44] Mechanical properties of resin-ceramic CAD-CAM materials after accelerated aging
    Blackburn, Caleb
    Rask, Hailee
    Awada, Abdallah
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (06): : 954 - 958
  • [45] Effect of thermocycling on the surface properties of resin-matrix CAD-CAM ceramics after different surface treatments
    Cakmak, Gulce
    Subasi, Meryem Gulce
    Yilmaz, Burak
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2021, 117
  • [46] Influence of different surface treatment on bonding of metal and ceramic Orthodontic Brackets to CAD-CAM all ceramic materials
    Haralur, Satheesh B.
    Alqahtani, Abdulrahman Mushabbab
    Shiban, Abdullah Saeed
    Alattaf, Zyad Muhammed
    Chaturvedi, Saurabh
    AlQahtani, Saeed M.
    Alqahtani, Nasser M.
    BMC ORAL HEALTH, 2023, 23 (01)
  • [47] Influence of different surface treatment on bonding of metal and ceramic Orthodontic Brackets to CAD-CAM all ceramic materials
    Satheesh B. Haralur
    Abdulrahman Mushabbab Alqahtani
    Abdullah Saeed Shiban
    Zyad Muhammed Alattaf
    Saurabh Chaturvedi
    Saeed M AlQahtani
    Nasser M Alqahtani
    BMC Oral Health, 23
  • [48] Impact of artificial aging by thermocycling on edge chipping resistance and Martens hardness of different dental CAD-CAM restorative materials
    Hampe, Rudiger
    Theelke, Bjorn
    Luemkemann, Nina
    Stawarczyk, Bogna
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 125 (02): : 326 - 333
  • [49] RESEARCH AND EDUCATION Different surface treatment strategies on etchable CAD-CAM materials: Part II-Effect on the bond strength
    Porto, Thiago Soares
    da Silva, Italo Guimaraes Medeiros
    Vallerini, Bruna de Freitas
    de Goes, Mario Fernando
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (05): : 770 - 779
  • [50] Influence of the foundation substrate on the fatigue behavior of bonded glass, zirconia polycrystals, and polymer infiltrated ceramic simplified CAD-CAM restorations
    Machry, Renan Vaz
    Borges, Alexandre Luiz Souto
    Pereira, Gabriel Kalil Rocha
    Kleverlaan, Cornelis Johannes
    Venturini, Andressa Borin
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2021, 117