Effect of post-weld heat treatment on hydrogen-assisted cracking behavior of high-strength process pipe steel in a sour environment

被引:14
|
作者
Kim, Sung Jin [1 ]
Jung, Hwan Gyo [2 ]
Kim, Kyoo Young [1 ]
机构
[1] Pohang Univ Sci & Technol POSTECH, GIFT, Pohang 790784, South Korea
[2] POSCO Tech Res Labs, Pohang 790704, South Korea
关键词
Tempering; Transmission electron microscopy (TEM); High-strength low-alloy (HSLA) steels; Hydrogen embrittlement; Acicular ferrite; SULFIDE STRESS CRACKING; TRAPPING EFFICIENCY; MICROSTRUCTURE; PERMEATION; PERMEABILITY; SUSCEPTIBILITY; RESISTANCE; DIFFUSION;
D O I
10.1016/j.scriptamat.2012.08.021
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The influence of post-weld heat treatment on hydrogen-assisted cracking of process pipe steel is investigated in terms of change in hydrogen trapping site. This study reports that, contrary to other microstructures, in acicular ferrite, cementite bodies acting as reversible trapping sites for hydrogen atoms are newly precipitated along the grain boundary by the post-weld heat treatment conducted at 620 degrees C. This leads to an increase in diffusible hydrogen content in the steel that makes it more susceptible to hydrogen-induced cracking. (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:895 / 898
页数:4
相关论文
共 50 条
  • [41] Hydrogen-assisted cracking (HAC) of high-strength steels as a function of the hydrogen pre-charging time
    Brilz, Michael
    Hoche, Holger
    Oechsner, Matthias
    ENGINEERING FRACTURE MECHANICS, 2022, 261
  • [42] HYDROGEN-ASSISTED CRACKING IN HIGH-STRENGTH TI-6AL-4V ALLOY
    MEYN, DA
    REPORT OF NRL PROGRESS, 1971, (MAR): : 16 - &
  • [43] EFFECT OF WELDING AND POST-WELD HEAT TREATMENT ON QT35 STEEL
    SMITH, E
    APPS, RL
    METAL CONSTRUCTION AND BRITISH WELDING JOURNAL, 1971, 3 (08): : 303 - &
  • [44] Susceptibility to hydrogen-induced cracking of weld beads on high-strength structural steel
    Malina, J
    Samardzic, I
    Gliha, V
    MATERIALS SCIENCE, 2005, 41 (02) : 253 - 258
  • [45] Susceptibility to Hydrogen-Induced Cracking of Weld Beads on High-Strength Structural Steel
    J. Malina
    I. Samardzic
    V. Gliha
    Materials Science, 2005, 41 : 253 - 258
  • [46] A STUDY OF REHEAT CRACKING IN WELD HEAT-AFFECTED ZONE OF HIGH-STRENGTH STEEL
    WATANABE, T
    SAVAGE, WF
    TRANSACTIONS OF NATIONAL RESEARCH INSTITUTE FOR METALS, 1984, 26 (04): : 305 - 314
  • [47] Effect of tensile stress in elastic and plastic range on hydrogen permeation of high-strength steel in sour environment
    Kim, Sung Jin
    Jung, Hwan Gyo
    Kim, Kyoo Young
    ELECTROCHIMICA ACTA, 2012, 78 : 139 - 146
  • [48] Effect of Mn alloying on the hydrogen-assisted cracking behavior in multiphase/duplex stainless steel
    Liu, Menghao
    Du, Cuiwei
    Li, Xiaogang
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 207 : 126 - 141
  • [49] Effect of post-weld heat treatment on friction welded joint of carbon steel to stainless steel
    Ma, Hong
    Qin, Guoliang
    Geng, Peihao
    Li, Fei
    Meng, Xiangmeng
    Fu, Banglong
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2016, 227 : 24 - 33
  • [50] Microstructural and crystallographic study of hydrogen-assisted cracking in high strength PSB1080 steel
    Li, Xinfeng
    Zhang, Jin
    Akiyama, Eiji
    Wang, Yanfei
    Li, Qizhen
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2018, 43 (37) : 17898 - 17911