Empirical Stress Intensity Factors for Surface Cracks under Rolling Contact Fatigue

被引:9
|
作者
Levesque, George [1 ]
Arakere, Nagaraj K. [1 ]
机构
[1] Univ Florida, Dept Mech & Aerosp Engn, Gainesville, FL 32611 USA
关键词
Ball Bearings; Ceramics; Semi-Elliptical Crack; Contact Mechanics; Fatigue Crack Propagation; Rolling Contact Fatigue; Stress Analysis; Finite Element Analysis; Stress Intensity Factor; Silicon Nitride Balls; SILICON-NITRIDE; BREAKING CRACKS; PART I; PROPAGATION; TECHNOLOGY; BEARINGS; FAILURE; BALLS;
D O I
10.1080/10402001003642759
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This article contains empirical equations for the K(I), K(II), and K(III) stress intensity factors (SIFs) for semi-elliptical surface cracks for brittle materials subjected to rolling contact fatigue (RCF) as a function of the contact patch diameter, angle of crack to the surface, max pressure, position along the crack front, and aspect ratio of the crack. The equations were developed from SIFs calculated by parametric three-dimensional (3D) finite element analysis (FEA) for a range of contact patch radii (1b, 2b, and 3b) and angles of the crack to the surface (0 degrees., 45 degrees, and 60 degrees). Calculating mixed-mode SIFs for surface cracks subject to RCF using 3D FEA is computationally complex because of extreme mesh refinement required at multiple levels to capture steep stress gradients. The comprehensive empirical curve fits presented are accurate to within 0.5% of FE simulations and are useful for component design where contact-initiated surface fatigue damage is important such as in gears, roller bearings, and railway wheels. The results are of particular relevance to hybrid silicon nitride ball bearings, which are susceptible to failure from fatigue spalls emanating from preexisting surface cracks, due to crack growth driven by RCF (G. Levesque and N. K. Arakere, An investigation of partial cone cracks in silicon nitride balls. International Journal of Solids and Structures, 2008, 45:6301-6315).
引用
收藏
页码:621 / 629
页数:9
相关论文
共 50 条
  • [31] Stress intensity factors for surface cracks in round bar under single and combined loadings
    Ismail, A. E.
    Ariffin, A. K.
    Abdullah, S.
    Ghazali, M. J.
    MECCANICA, 2012, 47 (05) : 1141 - 1156
  • [32] Stress intensity factors of longitudinal surface cracks in a pipe with cladding under thermal loading
    Grebner, H.
    International Journal of Materials and Product Technology, 1988, 3 (3-4) : 318 - 325
  • [33] An application of the weight function technique to inclined surface cracks under rolling contact fatigue, assessment and parametric analysis
    Beghini, M.
    Santus, C.
    ENGINEERING FRACTURE MECHANICS, 2013, 98 : 153 - 168
  • [34] Rough surface rolling contact fatigue crack stress intensity factor calculation for modern rail steels
    Fletcher, D. I.
    Corteen, J.
    Wilby, A.
    WEAR, 2024, 540
  • [35] Experimental analysis of surface cracks in rails under rolling contact loading
    Guagliano, M.
    Sangirardi, M.
    Vergani, L.
    WEAR, 2008, 265 (9-10) : 1380 - 1386
  • [36] LOCAL STRESS INTENSITY FACTORS FOR SURFACE CRACKS IN PLATES UNDER POWER-SHAPED STRESS DISTRIBUTIONS
    FETT, T
    MUNZ, D
    NEUMANN, J
    ENGINEERING FRACTURE MECHANICS, 1990, 36 (04) : 647 - 651
  • [37] Stress Intensity Factors for Fatigue Cracks at the Toe of a Transverse Weld.
    Skorupa, Malgorzata
    Archiwum Budowy Maszyn, 1984, 31 (3-4): : 247 - 266
  • [38] Analysis of surface crack growth under rolling contact fatigue
    Canadinc, D.
    Sehitoglu, H.
    Verzal, K.
    INTERNATIONAL JOURNAL OF FATIGUE, 2008, 30 (09) : 1678 - 1689
  • [39] THE EARLY DETECTION OF ROLLING SLIDING CONTACT FATIGUE CRACKS
    GARNHAM, JE
    BEYNON, JH
    WEAR, 1991, 144 (1-2) : 103 - 116
  • [40] Investigation of rolling contact fatigue cracks in ball bearings
    Song Deng
    Lin Hua
    Xinghui Han
    Song Huang
    International Journal of Fracture, 2014, 188 : 71 - 78