Teak wood is widely used for the housing interior and decoration because of its beautiful grains appearance; however, it often suffers from surface damage especially in the tiling application. The remedy is to apply a protective layer such as polyurethane (PU). In this work, the sol-gel inorganic reinforced hard coating formulation based on silicon dioxide (SiO2) nanoparticles (SNPs) and methyltrimethoxysilane (MTMS) was investigated as a protective layer for teak wood. The coating formulation was applied by brushing, followed by pre-cured at 65 degrees C for 1 hr and cured at 95 degrees C for 3 hrs, yielding a transparent nanocomposite film. The SiO2 nanocomposite coating showed an improvement in abrasion resistance property, tested with Taber abrasion at 5 N for 1000 cycles, as evidenced by a lower weight loss than an uncoated counterpart. The nanocomposite film also showed a higher wear through resistance than the commercial PU coating. Water can be easily absorbed by uncoated wood while the nanocomposite coated wood showed an improvement in water resistance as evidence by water contact angle. The cross-sectional image showed that the nanocomposite film and the wood surface were forming a physical interlocking.
引用
收藏
页码:1089 / 1092
页数:4
相关论文
共 50 条
  • [31] Characterization of nanopolyurethane/SiO2 coating
    Zhang Fan
    Han Xianghong
    Ge Jing
    Xin Zhongyin
    7TH ASIAN INTERNATIONAL CONFERENCE OF LEATHER SCIENCE AND TECHNOLOGY SECT 1 AND 2, 2006, : 614 - 622
  • [32] Synthesis and characterization of a nanocomposite NiO/SiO2 from a sustainable source of SiO2
    Rebelo, Querem H. F.
    Ferreira, Carlos S.
    Santos, Pamyla L.
    Bonacin, Juliano A.
    Passos, Raimundo R.
    Pocrifka, Leandro A.
    Paula, Marcos M. S.
    PARTICULATE SCIENCE AND TECHNOLOGY, 2019, 37 (08) : 907 - 911
  • [33] TA/siO2 Hydrophobic Coating and Its effect on Corrosion Resistance of Concrete
    Lai X.
    Wang Y.
    Wang Y.
    Sun X.
    Jianzhu Cailiao Xuebao/Journal of Building Materials, 2024, 27 (01): : 30 - 36
  • [34] Synthesizing and Evaluating the Photocatalytic and Antibacterial Ability of TiO2/SiO2 Nanocomposite for Silicate Coating
    Manh-Cuong Le
    Thu-Huong Le
    Thanh-Huyen Bui Thi
    Quang-Dat Nguyen
    Thanh-Ha Do Thi
    Minh-Nguyet Tran Thi
    FRONTIERS IN CHEMISTRY, 2021, 9
  • [35] Synergistic effect of SiO2, ZnO and nanoclay on mechanical and thermal properties of wood polymer nanocomposite
    Deka, Biplab K.
    Baishya, Prasanta
    Maji, Tarun K.
    JOURNAL OF THERMOPLASTIC COMPOSITE MATERIALS, 2014, 27 (04) : 464 - 480
  • [36] Acid and alkali resistance of Acrylic polyurethane/R-SiO2 nanocomposite coating
    Nguyen Thi Mai
    Bui Thi Mai Anh
    Nguyen Thien Vuong
    VIETNAM JOURNAL OF CHEMISTRY, 2020, 58 (01) : 67 - 73
  • [37] Synthesis and characterization of ATO/SiO2 nanocomposite coating obtained by sol-gel method
    Chen, XC
    MATERIALS LETTERS, 2005, 59 (10) : 1239 - 1242
  • [38] Electrophoretic Deposition of Ni/SiO2 Nanocomposite Coating: Fabrication Process and Tribological and Corrosion Properties
    Isfahani, Arash Ghalayani
    Ghorbani, Mohammad
    JOURNAL OF NANO RESEARCH, 2014, 26 : 45 - 51
  • [39] Improvement of mechanical robustness of the superhydrophobic wood surface by coating PVA/SiO2 composite polymer
    Liu, Feng
    Wang, Shuliang
    Zhang, Ming
    Ma, Miaolian
    Wang, Chengyu
    Li, Jian
    APPLIED SURFACE SCIENCE, 2013, 280 : 686 - 692
  • [40] Scratch resistance of SiO2 and SiO2-ZrO2 sol-gel coatings on glass-ceramic obtained by sintering
    Soares, V. O.
    Soares, Paulo
    Peitl, O.
    Zanotto, E. D.
    Duran, A.
    Castro, Y.
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2013, 52 (05): : 225 - 230