Ballistic impact response of resistance-spot-welded (RSW) double-layered plates for Q&P980 steel

被引:5
|
作者
Ma, Bo-han [1 ]
Ma, Dong-fang [1 ,2 ]
Wang, Huan-ran [1 ]
Chen, Da-nian [1 ]
Zhou, Feng-hua [1 ]
机构
[1] Ningbo Univ, MOE Key Lab Impact & Safety Engn, Ningbo 315211, Peoples R China
[2] Ningbo Univ, Coll Sci & Technol, Ningbo 315211, Peoples R China
基金
中国国家自然科学基金;
关键词
RSW; Q& P980; steel; Ballistic impact; Deformation; Fracture; PROJECTILE NOSE SHAPE; DYNAMIC-BEHAVIOR; PERFORATION; STRENGTH; VELOCITY;
D O I
10.1016/j.dt.2021.04.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ballistic impact response of resistance-spot-welded (RSW) double-layered (2 x 1.6 mm) plates (190 mm x 150 mm) for Q&P980 steel impacted by a round-nosed steel bullet (12 mm diameter and 30 mm length) was investigated by using gas gun and high-speed camera system. The RSW specimens were spot welded using a 6 mm diameter electrode face producing a 7.2 mm diameter fusion zone of the spot weld. The ballistic curve and energy balance for the tests of the spot weld of the RSW specimens at different velocity were analyzed to characterize the ballistic behavior of the RSW specimens under bullet impact. The fracture mechanisms of the RSW specimens under bullet impact were presented. For the tests below the ballistic limit, the cracks initiated from the notch-tip and propagated along the faying surface or obliquely through the thickness depending on the impact velocity. For the tests above the ballistic limit, the plug fracture in the front plate of the RSW specimen could be caused by the thinning-induced necking in the BM near the HAZ, while the plug fracture in the rear plate of the RSW specimens may be consist of the circumferential cracking from the rear surface and the bending fracture of the hinged part of material. The effects of the electrode indentation and the weld interfaces on deformation and fracture of the RSW specimens under bullet impact were revealed. For the tests above the ballistic limit, the circumferential fracture from the rear surface of the RSW specimens was always initiated along the interior periphery of the electrode indentation and the crack paths were along the FZ/CGHAZ or CGHAZ/ FGHAZ interface. When the circumferential crack also formed outside the electrode indentation, the fracture on the BM/HAZ interface could be found. On the front plate of the RSW specimens, the shear/ bending induced cracking from the notch-tip were observed and the crack paths were along the FZ/ CGHAZ or CGHAZ/FGHAZ interface.(c) 2021 China Ordnance Society. Publishing services by Elsevier B.V. on behalf of KeAi Communications Co. Ltd. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/ licenses/by-nc-nd/4.0/).
引用
收藏
页码:1052 / 1064
页数:13
相关论文
共 38 条
  • [31] A study on improving the mechanical performance by controlling the halo ring in the Q&P 980 steel resistance spot welds
    Ramachandran, Dileep Chandran
    Figueredo, Bruna
    Sherepenko, Oleksii
    Jin, Woosung
    Park, Yeong-Do
    Biro, Elliot
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 75 : 320 - 330
  • [32] Effect of paint baking on the fusion boundary softening and fracture behavior of Q&P 980 steel resistance spot welds
    Ramachandran, Dileep Chandran
    Betiku, Olakunle Timothy
    Shojaee, Mohammad
    Salandari-Rabori, Adib
    Midawi, Abdelbaset R. H.
    Kim, Ji-Ung
    Bakhtiari, Reza
    Macwan, Andrew
    Biro, Elliot
    MATERIALS CHARACTERIZATION, 2023, 206
  • [33] Stress wave response analysis of nanoelectroplating steel plate resistance spot welding structure under ballistic impact loading
    Fan, Chunlei
    Wang, Huanran
    Ma, Dongfang
    Ma, Bohan
    MATERIALS EXPRESS, 2021, 11 (03) : 363 - 371
  • [34] Achieving excellent properties of resistance spot welded 2GPa-grade press hardened steel and galvanized DP980 steel via double-pulse
    Chen, Xuefei
    Li, Zhengxian
    Yang, Dapeng
    Wang, Yuqian
    Yi, Hongliang
    Xie, Guangming
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 28 : 4475 - 4487
  • [35] Experimental and numerical study on ballistic impact behavior of explosively-welded double-layered Weldox700E targets against ogival-nosed projectiles
    Ge, Yanxin
    Chen, Pengwan
    Wu, Xuan
    Zhou, Qiang
    Fan, Hang
    Wang, Chenguang
    Zhou, Changqing
    Liu, Mengce
    Deng, Lisha
    Zhou, Qiang.
    Jia, Bin
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2025, 195
  • [36] Effect of incorporating Lode angle parameter into a fracture criterion in predicting ballistic impact behavior of double-layered 2024-T351 aluminum alloy plates against blunt projectiles
    Xiao, Xinke
    Shi, Yahui
    Wang, Yaopei
    Chen, Xiaozhen
    Jia, Bin
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2022, 160
  • [37] Effect of incorporating Lode angle parameter into a fracture criterion in predicting ballistic impact behavior of double-layered 2024-T351 aluminum alloy plates against blunt projectiles
    Xiao, Xinke
    Shi, Yahui
    Wang, Yaopei
    Chen, Xiaozhen
    Jia, Bin
    International Journal of Impact Engineering, 2022, 160
  • [38] Effect of sheet thickness on liquid metal embrittlement cracking of Galva-annealed quench & partitioning (Q&P) 980 MPa steel during resistance spot welding
    Kwon, Hyuck Min
    Oh, Gyu Hwan
    Lee, Chang-Wook
    Jeong, Junyeong
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2025, 39 (01) : 339 - 345