Influence of early mineral deposits of silicate- and aluminate-based cements on push-out bond strength to root dentine

被引:21
|
作者
do Carmo, S. S. [1 ]
Nespoli, F. F. P. [1 ]
Bachmann, L. [2 ]
Miranda, C. E. S. [1 ]
Castro-Raucci, L. M. S. [1 ]
Oliveira, I. R. [3 ]
Raucci-Neto, W. [1 ]
机构
[1] Univ Ribeirao Preto, Dept Dent, Ribeirao Preto, SP, Brazil
[2] Univ Sao Paulo, Dept Phys, Ribeirao Preto, SP, Brazil
[3] Univ Vale Paraiba, Inst Res & Dev, Sao Jose Dos Campos, SP, Brazil
关键词
calcium silicate; hydroxyapatite; root-end cavities; TRIOXIDE AGGREGATE; ENDODONTIC CEMENT; EX-VIVO; CALCIUM; TEETH; MTA; BIODENTINE; BIOACTIVITY; PHOSPHATE; REPAIR;
D O I
10.1111/iej.12791
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
AimTo evaluate mineral trioxide aggregate (MTA), Biodentine and several formulations of calcium aluminate cements (CACb) in terms of their ability to release calcium ions (Ca2+) and form apatite-like precipitates after short-term immersion in phosphate-buffered saline (PBS) and its influence on the bond strength to the root-end cavity. MethodologyTen samples of MTA, Biodentine, CACb and calcium-enriched aluminate cement (CACb+) were placed in contact with PBS or deionized water for 14days. The cement surfaces were analysed using SEM, EDS-X and FTIR. Eighty standardized root-end cavities filled with the cements (ten samples of each cement) were immersed in PBS or deionized water for 14days, and the bond strengths were measured. Data from the push-out test were analysed using two-way ANOVA and Tukey's tests (=0.05). ResultsA gradual decrease was observed in Ca2+ concentrations and pH of all solutions. FTIR bands of different phases of hydroxyapatite were identified. Crystalline formation was observed on the surface of all cements after immersion in PBS. No significant difference was observed in the bond strength of the test materials (P>0.05); however, all cements without contact with the solution revealed significantly lower bond strength values than those in contact with the solution (P<0.05). ConclusionMTA, Biodentine, CACb e CACb+ were associated with precipitation of crystals after being in contact with PBS for 14days, indicated by different phases of hydroxyapatite crystalline formation, which also increased dislodgment resistance of the material from root-end cavities. The CACb+ had similar bond strengths and precipitation of crystals to existing materials.
引用
收藏
页码:92 / 101
页数:10
相关论文
共 50 条
  • [31] Effect of ultrasonic and sonic activation of root canal sealers on the push-out bond strength and interfacial adaptation to root canal dentine
    Wiesse, P. E. B.
    Silva-Sousa, Y. T.
    Pereira, R. D.
    Estrela, C.
    Domingues, L. M.
    Pecora, J. D.
    Sousa-Neto, M. D.
    INTERNATIONAL ENDODONTIC JOURNAL, 2018, 51 (01) : 102 - 111
  • [32] Influence of Irrigating Solutions on Push-Out Bond Strenght of Intraradicular Posts to Dentine
    Kaif, Mohammad
    Bissu, Raj
    ODOVTOS INTERNATIONAL JOURNAL OF DENTAL SCIENCES, 2016, 18 (01) : 73 - 81
  • [33] Push-out Bond Strength of Injectable Pozzolan-based Root Canal Sealer
    Nogueira Leal Silva, Emmanuel Joao
    Carvalho, Nancy Kudsi
    Prado, Marina C.
    Zanon, Mayara
    Senna, Plinio Mendes
    Souza, Erick M.
    De-Deus, Gustavo
    JOURNAL OF ENDODONTICS, 2016, 42 (11) : 1656 - 1659
  • [34] The push-out test to evaluate dentine-amalgam shear bond strength.
    Eid, N
    Degrange, M
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 679 - 679
  • [35] Effect of the timing of radiation therapy on the push-out strength of resin cement to root dentine
    Cancelier, Patricia da Agostim
    Machado, Renata Gondo
    Savaris, Julia Menezes
    Bortoluzzi, Eduardo Antunes
    Teixeira, Cleonice da Silveira
    Minamisako, Mariana Comparotto
    Rodrigues, Paulo Marcelo
    Netto, Vicente Ribeiro
    Dutra-Horstmann, Kamile Leonardi
    Roberti Garcia, Lucas da Fonseca
    AUSTRALIAN ENDODONTIC JOURNAL, 2023, 49 : 122 - 131
  • [36] The effect of XP-endo Finisher and ultrasonic irrigation on the push-out bond strength of a resin sealer to the root dentine
    Nogueira Leal da Silva, Emmanuel Joao
    Herrera, Daniel Rodrigo
    de Lima, Carolina Oliveira
    Fidel, Sandra Rivera
    Sassone, Luciana Moura
    ENDO-ENDODONTIC PRACTICE TODAY, 2019, 13 (01): : 41 - 47
  • [37] The Influence of Time and Cement Type on Push-Out Bond Strength of Fiber Posts to Root Dentin
    Leme, A. A.
    Coutinho, M.
    Insaurralde, A. F.
    Scaffa, P. M. C.
    da Silva, L. M.
    OPERATIVE DENTISTRY, 2011, 36 (06) : 643 - 648
  • [38] Influence of root dentin treatment on the push-out bond strength of fibre-reinforced posts
    de Moura, Altair Soares
    Pereira, Rodrigo Dantas
    Abi Rached-Junior, Fuad Jacob
    Crozeta, Bruno Monguilhott
    Mazzi-Chaves, Jardel Francisco
    Souza-Flamini, Luis Eduardo
    Cruz-Filho, Antonio Miranda
    BRAZILIAN ORAL RESEARCH, 2017, 31 : 1 - 11
  • [39] The Effect of Obturation Technique on the Push-out Bond Strength of Calcium Silicate Sealers
    DeLong, Christopher
    He, Jianing
    Woodmansey, Karl E.
    JOURNAL OF ENDODONTICS, 2015, 41 (03) : 385 - 388
  • [40] The effect of calcium silicate-based sealer on the push-out bond strength of fibre posts
    Ozcan, E.
    Capar, I. D.
    Cetin, A. R.
    Tuncdemir, A. R.
    Aydinbelge, H. A.
    AUSTRALIAN DENTAL JOURNAL, 2012, 57 (02) : 166 - 170