Age hardening behaviour of semi-solid squeeze cast A319 aluminium alloy

被引:1
|
作者
Wang, Q. F. [1 ,2 ]
Wang, L. D. [3 ,4 ,5 ]
Zhu, D. Y. [1 ]
Lin, Z. [3 ]
Chen, X. [3 ]
Sheng, B. [2 ]
机构
[1] Fuzhou Univ, Sch Mat Sci & Engn, 2 Xueyuan Rd, Fuzhou 350116, Fujian, Peoples R China
[2] Jimei Univ, Coll Mech & Energy Engn, 9 Shigu Rd, Xiamen 361021, Fujian, Peoples R China
[3] Fuzhou Univ, Sch Mech Engn & Auto, 2 Xueyuan Rd, Fuzhou 350116, Fujian, Peoples R China
[4] China Acad Machinery Sci & Technol, Inst Semisolid Met Technol, 22 Huancheng East Rd, Sanming 353300, Fujian, Peoples R China
[5] Fujian Kinrui Hitech Co Ltd, Econ Dev Area, Sanming 353399, Fujian, Peoples R China
关键词
A319; alloy; age hardening; semi-solid; squeeze casting; gravity die casting; HEAT-TREATMENT; AL; SI; DUCTILITY; STRENGTH; PHASE;
D O I
10.1002/mawe.201800037
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of age hardening treatment on the hardness and microstructure of semi-solid squeeze cast A319 alloy is investigated. At 175 degrees C, the age-hardening curve of the alloy shows two peaks between which there was an apparent valley. Analyses by transmission electron microscopy, selected area electron diffraction and energy-dispersive X-ray detection suggest that the first peak is caused by formation of G.P.2 zones while the second peak can be related to formation of the metastable theta '- and Q '-phases. Compared with gravity die cast A319 the semi-solid squeeze cast A319 shows a larger increase and a higher peak in hardness during the age hardening process. Additionally, the latter requires another 32 h to reach the first hardness peak while it reaches the second hardness peak about 24 h earlier than the former.
引用
收藏
页码:1503 / 1509
页数:7
相关论文
共 50 条
  • [31] Semi-solid squeeze casting process of a ZL109 alloy
    ZHAI Yanbo LIU Changming HAN Zhaotang WANG Kai College of Mechanical Engineering
    Rare Metals, 2008, (03) : 329 - 334
  • [32] Squeeze flow of semi-solid slurries
    Alexandrou, Andreas N.
    Florides, Georgios C.
    Georgiou, Georgios C.
    JOURNAL OF NON-NEWTONIAN FLUID MECHANICS, 2013, 193 : 103 - 115
  • [33] Squeeze Flow of Semi-Solid Slurries
    Alexandrou, Andreas N.
    Florides, Georgios C.
    Georgiou, Georgios C.
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES XII, 2013, 192-193 : 263 - +
  • [34] RHEOLOGICAL ANALYSIS OF SEMI-SOLID A380.0 ALUMINIUM ALLOY
    Solek, K.
    Szczepanik, S.
    ARCHIVES OF METALLURGY AND MATERIALS, 2015, 60 (04) : 2613 - 2617
  • [35] Rheological Characterization of Semi-Solid A356 Aluminium Alloy
    Das, Prosenjit
    Samanta, Sudip K.
    Chattopadhyay, Himadri
    Dutta, Pradip
    Barman, Nilkanta
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES XII, 2013, 192-193 : 329 - +
  • [36] Friction stir welding of dissimilar A319 and A356 aluminium cast alloys
    Hassan, A. S.
    Mahmoud, T. S.
    Mahmoud, F. H.
    Khalifa, T. A.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2010, 15 (05) : 414 - 422
  • [37] Effect of Zr addition on the aging behavior of A319 aluminum cast alloy
    Sepehrband, P
    Mahmudi, R
    Khomamizadch, F
    SCRIPTA MATERIALIA, 2005, 52 (04) : 253 - 257
  • [38] Effect of temperature on the tensile properties of an as-cast aluminum alloy A319
    Rincon, E.
    Lopez, H. F.
    Cisneros, M. M.
    Mancha, H.
    Cisneros, M. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 452 : 682 - 687
  • [39] Interaction of 308 stainless steel insert with A319 aluminium casting alloy
    Khoonsari, E. M.
    Jalilian, F.
    Paray, F.
    Emadi, D.
    Drew, R. A. L.
    MATERIALS SCIENCE AND TECHNOLOGY, 2010, 26 (07) : 833 - 841
  • [40] Electrodeposition of nanodiamond particles on aluminium alloy A319 for improved tribological properties
    Kalyanasundaram, D.
    Molian, P.
    MICRO & NANO LETTERS, 2008, 3 (04) : 110 - 116