Sulfidation of three two-phase Cu-Cr alloys in H2-H2S mixtures at 400-600°C

被引:12
|
作者
Niu, Y
Gesmundo, F
Fu, GY
Douglass, DL
机构
[1] Inst Corros & Protect Met, State Key Lab Corros & Protect, Shenyang 110015, Peoples R China
[2] Univ Genoa, Ist Chim, I-16129 Genoa, Italy
[3] Univ Arizona, Arizona Mat Lab, Tucson, AZ 85712 USA
来源
OXIDATION OF METALS | 1998年 / 50卷 / 5-6期
关键词
sulfidation; copper; chromium; two-phase alloys;
D O I
10.1023/A:1018896523030
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The sulfidation of three Cu-Cr alloys with nominal Cr contents of 25, 50, and 75 wt.% and of the two pure metals has been studied at 400-600 degrees C in H-2-H2S mixtures under sulfur pressures of 10(-12) atm at 400 and 500 degrees C and 10(-10) arm at 500 and 600 degrees C, slightly above the Cu-Cu2S equilibrium All the alloys were two-phase, containing a mixture of the solid solution of chromium in copper with nearly pure chromium. The corrosion rates of the three materials under the same conditions were similar and intermediate between those of the two pule metals and increased with temperature and sulfur pressure. The scales had a complex composition, often containing an external Cu2S layer, which became discontinuous or even disappeared, in some cases, followed by an intermediate layer of the double Cu-Cr sulfide CuCrS2 and an innermost complex layer, which generally consisted of a mixture of the double Cu-Cr sulfide CuCr2S4 with the chromium sulfide CrS and also commonly contained unsulfidized chromium metal particles. No chromium depletion was developed in the alloys beneath the corrosion-affected region. Moreover; no internal sulfidation of chromium was observed in the alloy richest in copper and no exclusive external sulfidation of chromium in those richest in chromium, in spite of the large difference in the thermodynamic stabilities of the sulfides of the two pure metals. These peculiar scale features are interpreted by taking into account the special two-phase nature of these alloys.
引用
收藏
页码:327 / 354
页数:28
相关论文
共 50 条
  • [21] HIGH-TEMPERATURE SULFIDATION OF FE-MN ALLOYS AND MN IN H2-H2S
    PAPAIACOVOU, P
    SCHMIDT, HP
    ERHART, H
    GRABKE, HJ
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1987, 38 (09): : 498 - 506
  • [22] The air oxidation of two-phase Cu-Cr alloys at 700–900°C
    Y. Niu
    F. Gesmundo
    F. Viani
    D. L. Douglass
    Oxidation of Metals, 1997, 48 : 357 - 380
  • [23] Sulfidation properties of Ti, Mn or Nb-bearing Fe-25Cr alloys in H2-H2S mixed environments at 800°C
    Qi, Huibin
    He, Yedong
    Huang, Zhenzhong
    Zhu, Rizhang
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 1998, 8 (01): : 33 - 37
  • [24] THE CORROSION OF THE 9CR-1MO COMMERCIAL STEEL IN H2-H2S AND IN H2-H2S-CO2 MIXTURES AT 400-DEGREES-C-700-DEGREES-C
    GESMUNDO, F
    GODLEWSKI, K
    VIANI, F
    BREGAN, F
    BULLETIN OF THE POLISH ACADEMY OF SCIENCES-CHEMISTRY, 1992, 40 (01): : 1 - 10
  • [25] The sulfidation of a Co-15 wt.% Ce alloy in H2-H2S mixture at 600-800°C
    Castello, P
    Fu, GY
    Niu, Y
    Gesmundo, F
    Viani, F
    OXIDATION OF METALS, 1998, 49 (1-2): : 71 - 89
  • [26] Sulfidation behavior of Fe-40Al sheet in H2-H2S mixtures at high temperatures
    Lang, FQ
    Yu, ZM
    Gedevanishvili, S
    Deevi, SC
    Hayashi, S
    Narita, T
    INTERMETALLICS, 2004, 12 (05) : 469 - 475
  • [27] THE OXIDATION SULFIDATION OF NI-NB ALLOYS AT 600-800-DEGREES-C IN H-2-H2S-CO2 MIXTURES
    NIU, Y
    GESMUNDO, F
    VIANI, F
    CORROSION SCIENCE, 1995, 37 (01) : 169 - &
  • [28] The air oxidation of two-phase Cu-Cr alloys at 700-900°C
    Niu, Y
    Gesmundo, F
    Viani, F
    Douglass, DL
    OXIDATION OF METALS, 1997, 48 (5-6): : 357 - 380
  • [30] THE SULFIDATION PROPERTIES OF TITANIUM-BEARING MANGANESE-BEARING AND NIOBIUM-BEARING FE-25CR ALLOYS IN H2-H2S MIXTURES AT 800-DEGREES-C
    QI, HB
    ZHU, RZ
    HE, YD
    CORROSION SCIENCE, 1993, 35 (5-8) : 1099 - 1105