Effect of ECAP on sliding wear behaviour of Mg-Zn-Gd-Zr alloy

被引:14
|
作者
Patil, Aneesh [1 ]
Bontha, Srikanth [1 ]
Ramesh, M. R. [1 ]
机构
[1] Natl Inst Technol Karnataka, Dept Mech Engn, Mangalore 575025, India
关键词
ECAP; Wear; Mg-Zn-Gd-Zr Alloy; COF; As-cast; MECHANICAL-PROPERTIES; MAGNESIUM ALLOY; MICROSTRUCTURE;
D O I
10.1016/j.matpr.2019.10.045
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Magnesium is a lightweight, recyclable, and biocompatible material. However, the extensive commercial use of Magnesium and its alloys is hindered by their poor wear behaviour and mechanical properties. Equal Channel Angular Pressing (ECAP) is a severe plastic deformation technique which improves the material properties through grain refinement. In the present study, wear behaviour of ECAP processed Mg-Zn-Gd-Zr alloy was investigated. ECAP process was carried out up to 3 passes at a temperature of 380 degrees C. Wear testing of as-cast and ECAP processed alloy were carried out using dry sliding wear method on a pin on disk tribometer by varying loads. The wear mechanism was analysed using Scanning Electron Microscope (SEM) and Energy Dispersive X-ray Spectroscopy (EDS). Average Coefficient of Friction (COF) increased after each pass of ECAP. Wear rate increased with the applied load. Despite severe plastic deformation, wear resistance of ECAP processed samples was found to be lower than that of as-cast samples at higher loads. Abrasive and oxidation wear mechanisms were found in both as-cast and ECAP processed samples. (C) 2019 Elsevier Ltd. All rights reserved.
引用
收藏
页码:97 / 102
页数:6
相关论文
共 50 条
  • [31] Effect of Zn/(Gd plus Y) ratio on the microstructure evolution and mechanical properties of Mg-Gd-Y-Zn-Zr alloy
    Wei, Xiaoxiao
    Jin, Li
    Dong, Shuai
    Wang, Fenghua
    Dong, Jie
    MATERIALS CHARACTERIZATION, 2020, 169 (169)
  • [32] Improving the Corrosion and Wear Behaviour of ECAP-Processed Biodegradable Mg-Zn-Ca Alloy for Bone Repair Applications
    El-Garaihy, W. H.
    Alateyah, A., I
    Alrumayh, A.
    BaQais, Amal
    Alawad, Majed O.
    El-Asfoury, Mohamed S.
    TMS 2024 153RD ANNUAL MEETING & EXHIBITION: SUPPLEMENTAL PROCEEDINGS, 2024, : 717 - 730
  • [33] Influence of Pre-Solution Treatment on Microstructure and Mechanical Properties of Mg-Gd-Nd-Zn-Zr Alloy Processed by ECAP
    Liu, Yong
    Kang, Zhi Xin
    Zhang, Jun Yi
    Wang, Fen
    Li, Yuan Yuan
    ADVANCED ENGINEERING MATERIALS, 2016, 18 (05) : 833 - 838
  • [34] Formation of profuse long period stacking ordered microcells in Mg-Gd-Zn-Zr alloy during multipass ECAP process
    20141317517428
    Ma, A.B. (aibin-ma@hhu.edu.cn), 1600, Elsevier Ltd (601):
  • [35] Formation of profuse long period stacking ordered microcells in Mg-Gd-Zn-Zr alloy during multipass ECAP process
    Lu, F. M.
    Ma, A. B.
    Jiang, J. H.
    Yang, D. H.
    Yuan, Y. C.
    Zhang, L. Y.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 601 : 140 - 145
  • [36] Microstructure and creep behaviour of Mg-12Gd-3Y-1Zn-0.4Zr alloy
    Zhu Xiurong
    Wang Jun
    Xu Yongdong
    Wang Rong
    Nie Jingjiang
    Zhu Liping
    JOURNAL OF RARE EARTHS, 2013, 31 (02) : 186 - 191
  • [37] Microstructure and creep behaviour of Mg-12Gd-3Y-1Zn-0.4Zr alloy
    朱秀荣
    王军
    徐永东
    王荣
    聂景江
    朱利萍
    Journal of Rare Earths, 2013, 31 (02) : 186 - 191
  • [38] Achieving enhanced thermal conductivity and mechanical properties in Mg-Zn-Gd-Zr alloys via regulation microstructure characteristics
    Zhang, Yong
    Wang, Yu
    Liu, Tao
    Wang, Xiaogang
    Xin, Yong
    Liu, Yong
    Wu, Chengxing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 903
  • [39] Dry sliding wear behavior of cast Mg-11Y-5Gd-2Zn magnesium alloy
    Hu Mao-liang
    Wang Qu-dong
    Li Cheng
    Ding Wen-jiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (08) : 1918 - 1923
  • [40] Gd对心血管支架用Mg-Zn-Gd-Zr合金的腐蚀性能的影响
    赵兵
    韩少兵
    贾长健
    许春香
    张金山
    中国铸造装备与技术, 2017, (04) : 7 - 10