The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe

被引:192
|
作者
Xiong, XY
Ohkubo, T
Koyama, T
Ohashi, K
Tawara, Y
Hono, K
机构
[1] Natl Inst Mat Sci, Met Nanostruct Grp, Tsukuba, Ibaraki 3050047, Japan
[2] Shin Etsu Chem Co Ltd, Fukui 915, Japan
关键词
SmCo alloys; coercivity; permanent magnets; three-dimensional atom probe; microstructure;
D O I
10.1016/j.actamat.2003.10.015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure and the compositions of the constituent phases in a sintered SM(Co0.72Fe0.20Cu0.055Zr0.025)(7.5) permanent magnet with different cooling processes have been investigated by transmission electron microscopy and the three-dimensional atom probe (3DAP) technique. The Cu concentration in the SmCo5 phase increases during slow cooling from 820 to 520 degreesC, having a wider concentration profile than that of Sm at cell boundaries. Enrichment of Cu at the triple junction of cell boundaries was also found. These results explain the substantial increase in coercivity during the slow cooling process. High resolution transmission electron microscopy and nano-beam electron diffraction analysis have confirmed that the Z-phase is Zr(Co, Fe)(3), having the Be3Nb structure with a approximate to 0.5 nm, c approximate to 2.4 nm. In the Z-phase, Sm is almost completely replaced with Zr during slow cooling. (C) 2003 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:737 / 748
页数:12
相关论文
共 50 条
  • [31] Effect of heat treatment modes on the structure and magnetic properties of sintered permanent magnets based on Sm(Co, Fe, Cu, Zr) Z
    Arinicheva, O. A.
    Lileev, A. S.
    Reissner, M.
    Dormidontov, A. G.
    METAL SCIENCE AND HEAT TREATMENT, 2013, 55 (1-2) : 63 - 67
  • [32] Effects of Sintering Time on High-Temperature Magnetic Properties and Microstructure of Sintered Sm(Co0.79Fe0.09Cu0.09Zr0.03)7.68 Magnet
    Wang, Guangqing
    Liu, Zhuang
    Zhang, Chaoyue
    Yan, Guanghui
    Liu, Lei
    Chen, Renjie
    Hou, Xueling
    Yan, Aru
    IEEE TRANSACTIONS ON MAGNETICS, 2020, 56 (01)
  • [33] Effect of grain size on microstructure and magnetic properties of Sm2(Co,Cu,Fe,Zr)17 permanent magnets
    Palit, Mithun
    Rajkumar, D. M.
    Pandian, S.
    Kamat, S. V.
    MATERIALS CHEMISTRY AND PHYSICS, 2016, 179 : 214 - 222
  • [34] THE INFLUENCE OF THE SAMARIUM CONTENT ON THE COERCIVE FORCE AND ON THE STRUCTURE OF SINTERED PERMANENT-MAGNETS SM2(CO,FE,CU,ZR)17
    DIKO, P
    MISKUF, J
    HAJKO, V
    KOVAC, J
    KAREL, V
    ACTA PHYSICA SLOVACA, 1981, 31 (05) : 301 - 304
  • [35] Microstructure, electrical resistivity, and magnetic properties of Fe-rich Sm (Co0.66-xSixFe0.25Cu0.065Zr0.025)7.8 magnets
    Xia, Rui
    Zhang, Mingxiao
    Hou, Ruixia
    Zhu, Chaoqun
    Tan, Dongliang
    Li, Hangcheng
    Liu, Chengxiong
    Wu, Haichen
    Liu, Zhuang
    Chen, Renjie
    Yan, Aru
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2025, 616
  • [36] Microstructure and high temperature magnetic properties of Sm(Co,Cu,Fe,Zr)z (z = 6.7-9.1) permanent magnets
    Liu, JF
    Zhang, Y
    Dimitrov, D
    Hadjipanayis, GC
    JOURNAL OF APPLIED PHYSICS, 1999, 85 (05) : 2800 - 2804
  • [37] Peculiar Kinetics of Coercivity of Sintered Sm(Co0.78Fe0.10Cu0.10Zr0.02)7 Magnet Upon Slow Cooling
    Popov, A. G.
    Golovnia, O. A.
    Protasov, A. V.
    Gaviko, V. S.
    Gopalan, R.
    Jiang, C.
    Zhang, T.
    IEEE TRANSACTIONS ON MAGNETICS, 2018, 54 (06)
  • [38] 球磨时间对烧结Sm(Co0.72Fe0.15Cu0.1Zr0.03)7.5磁体性能和组织结构的影响
    胡盛青
    陈洪
    李彬
    稀土, 2016, 37 (04) : 23 - 28
  • [40] Identification of the cell boundary phase in the isothermally aged commercial Sm(Co0.725Fe0.1Cu0.12Zr0.04)7.4 sintered magnet
    Gopalan, R
    Ohkubo, T
    Hono, K
    SCRIPTA MATERIALIA, 2006, 54 (07) : 1345 - 1349