Fretting wear behaviour of surface mechanical attrition treated alloy 718

被引:64
|
作者
Kumar, S. Anand [1 ]
Raman, S. Ganesh Sundara [1 ]
Narayanan, T. S. N. Sankara [2 ]
Gnanamoorthy, R. [3 ]
机构
[1] IIT Madras, Dept Met & Mat Engn, Madras, Tamil Nadu, India
[2] Madras Ctr, Natl Met Lab, CSIR, Madras, Tamil Nadu, India
[3] Indian Inst Informat Technol Design & Mfg, Madras, Tamil Nadu, India
来源
SURFACE & COATINGS TECHNOLOGY | 2012年 / 206卷 / 21期
关键词
Surface mechanical attrition treatment; Nanocrystallization; Fretting wear resistance; Friction; Alloy; 718; STEAM-GENERATOR TUBE; GRAIN-REFINEMENT; FRICTION; CONTACT; NICKEL; LAYER; DEFORMATION; INCONEL-600; ROOM;
D O I
10.1016/j.surfcoat.2012.04.085
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Alloy 718 was subjected to surface mechanical attrition treatment (SMAT) using SAE 52100 steel balls of a 5 mm diameter for four different treatment durations (15, 30, 45 and 60 min). Fretting wear tests were conducted at different normal loads on untreated and treated samples for 25,000 cycles using alumina as a counterbody material. Microstructural features of the surface layer of samples treated by SMAT were characterized by cross-sectional optical microscopy and transmission electron microscopy. Hardness, surface roughness and residual stress were determined using a nano-indenter, surface roughness tester and X-ray residual stress analyzer respectively. SMAT resulted in the formation of nanocrystallites on the surface and near surface regions, increased hardness, increased surface roughness and compressive residual stress at the surface. Treated samples exhibited lower tangential force coefficient (TFC) compared to untreated samples. Samples treated for 60 min exhibited higher grain refinement, higher hardness, lower surface roughness and higher TFC compared to the samples treated for 30 min. The wear volume and wear rate of samples treated for 30 min were lower compared to those of the untreated samples, which may be attributed to an optimum combination of hardness and toughness and a low work hardening rate of the nanocrystalline structure at the surface of the treated samples. In contrast, the wear volume and wear rate of the samples treated for 60 min were higher than those of untreated samples, presumably due to the higher hardness and reduced toughness of the samples treated for 60 min. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:4425 / 4432
页数:8
相关论文
共 50 条
  • [21] Precipitation Behavior of IN718 After Surface Mechanical Attrition Treatment (SMAT) and Its Effect on Wear Properties
    Bisht, Anuj
    Gaddam, Supreeth
    Kumar, Lailesh
    Dileep, B. P.
    Suwas, Satyam
    JOM, 2018, 70 (11) : 2667 - 2676
  • [22] FINE GRAIN STRUCTURE AS PALLIATIVES FOR FRETTING WEAR OF INCONEL 718 ALLOY AT VARIOUS TEMPERATURES
    Amanov, Auezhan
    Pyun, Young-Sik
    Wang Qingyuan
    Khan, Muhammad Kashif
    8TH INTERNATIONAL SYMPOSIUM ON SUPERALLOY 718 AND DERIVATIVES, 2014, : 555 - 562
  • [23] Improvement in Fretting Wear Damage of Annealed Inconel 718 Alloy at a Temperature of 200 °C
    Amanov, Auezhan
    Kim, Jun-Hyong
    Pyun, Young-Sik
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2016, 16 (12) : 12742 - 12748
  • [24] Dual-motion fretting wear behaviour of 7075 aluminium alloy
    Zhu, MH
    Zhou, ZR
    WEAR, 2003, 255 : 269 - 275
  • [25] Fretting wear behaviour in 6061-T6 aluminium alloy
    Erturun, V.
    Odabas, D.
    AERONAUTICAL JOURNAL, 2023, 128 (1319): : 178 - 190
  • [26] Surface modification of aluminum alloy to improve fretting wear properties
    Nimura, Kenji
    Sugawara, Takashi
    Jibiki, Tatsuhiro
    Ito, Satoshi
    Shima, Masayuki
    TRIBOLOGY INTERNATIONAL, 2016, 93 : 702 - 708
  • [27] Structure and fretting wear behavior of surface alloying of Ti alloy
    Tang, Bin
    Fan, Ailan
    Qin, Lin
    Tian, Linhai
    He Jishu/Nuclear Techniques, 2007, 30 (12): : 979 - 982
  • [28] Machining Behaviour, surface integrity and tool wear analysis in environment friendly turning of Inconel 718 alloy
    Sivalingam, Vinothkumar
    Zhao, Yanzhe
    Thulasiram, Ramkumar
    Sun, Jie
    Kai, Guo
    Nagamalai, Thangapandian
    MEASUREMENT, 2021, 174
  • [29] Wear behaviour of Electron beam surface melted Inconel 718
    Sharma, Sumit K.
    Biswas, K.
    Majumdar, J. Dutta
    2ND INTERNATIONAL CONFERENCE ON SUSTAINABLE MATERIALS PROCESSING AND MANUFACTURING (SMPM 2019), 2019, 35 : 866 - 873
  • [30] Increase in Strength and Fretting Resistance of Alloy 718 Using the Surface Modification Process
    Amanov, Auezhan
    Umarov, Rakhmatjon
    Amanov, Tileubay
    MATERIALS, 2018, 11 (08)