Effect of coatings and tool geometry on the dry milling of wrought aluminium alloys

被引:6
|
作者
Lopez de Lacalle, L. N. [1 ]
Celaya, A. [1 ]
Lamikiz, A. [1 ]
Bravo, U. [1 ]
机构
[1] Univ Basque Country, Dept Mech Engn, ETSII UPV, Bilbao 48013, Spain
关键词
aluminium; chip removal; coolant; dry milling; high speed machining; milling;
D O I
10.1504/IJMPT.2008.018374
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The work presented here is focused on the elimination of coolants in the high speed milling of wrought aluminium alloys. This is a very interesting issue from the point of view of the high costs of the coolant life cycle and for environment preservation. The main factor to be considered is the estimation of temperature at the tool/chip interface, since it acts directly on the tool degradation mechanism: the previous diffusion and the later adhesion of aluminium on the rake and clearance faces, the well-known BUL (built up layer) effect. Two techniques are discussed to keep the temperature below the diffusion threshold, the tool geometry optimisation making use of the simulation of the removal process using the finite element method and the measurement of the tool edge temperature with an infrared L device. Five different types of hard metal tools have been tested under the same conditions.
引用
收藏
页码:41 / 55
页数:15
相关论文
共 50 条
  • [21] The effect of grain refinement and cooling rate on the hot tearing of wrought aluminium alloys
    Easton, Mark
    Grandfield, John
    StJohn, David
    Rinderer, Barbara
    ALUMINIUM ALLOYS 2006, PTS 1 AND 2: RESEARCH THROUGH INNOVATION AND TECHNOLOGY, 2006, 519-521 : 1675 - 1680
  • [22] Experimental analysis and optimisation of tool wear in dry machining of aluminium alloys
    Nouari, M
    List, G
    Girot, F
    Coupard, D
    WEAR, 2003, 255 (7-12) : 1359 - 1368
  • [23] Cutting conditions and tool optimization in the high-speed milling of aluminium alloys
    de Lacalle, LNL
    Lamikiz, A
    Sánchez, JA
    Cabanes, I
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2001, 215 (09) : 1257 - 1269
  • [24] Mechanical properties of friction stir welded butt joint of steel/aluminium alloys: effect of tool geometry
    Syafiq, W. M.
    Afendi, M.
    Daud, R.
    Mazlee, M. N.
    Majid, M. S. Abdul
    Lee, Y. S.
    INTERNATIONAL CONFERENCE ON APPLICATIONS AND DESIGN IN MECHANICAL ENGINEERING (ICADME 2017), 2017, 908
  • [25] Hybrid Ti-MoS2 Coatings for Dry Machining of Aluminium Alloys
    Brzezinka, Tomasz L.
    Rao, Jeff
    Chowdhury, Mohamad
    Kohlscheen, Joern
    Rabinovich, German S. Fox
    Veldhuis, Stephen C.
    Endrino, Jose L.
    COATINGS, 2017, 7 (09):
  • [26] Design of potent grain refiners for wrought aluminium alloys
    Birol, Y.
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2013, 26 (05) : 273 - 278
  • [27] Friction Stir Processing in Wrought and Cast Aluminium Alloys
    Cao, Ye
    Lados, Diana A.
    LIGHT METALS TECHNOLOGY 2013, 2013, 765 : 741 - 745
  • [28] Grain Morphology of As-Cast Wrought Aluminium Alloys
    Easton, Mark
    Davidson, Cameron
    StJohn, David
    MATERIALS TRANSACTIONS, 2011, 52 (05) : 842 - 847
  • [29] Primary and wrought products for semisolid forming of aluminium alloys
    Fiorini, P.
    Zanardi, L.
    Pellegrini, V.
    Metallurgia Italiana, 1994, 86 (02): : 91 - 98
  • [30] Modelling technological properties of commercial wrought aluminium alloys
    Zander, Johan
    Sandstrom, Rolf
    MATERIALS & DESIGN, 2009, 30 (09) : 3752 - 3759