Effects of Zn Additions on the Room Temperature Formability and Strength in Mg-1.2Al-0.5Ca-0.4Mn Alloy Sheets

被引:2
|
作者
Li, Z. H. [1 ,2 ]
Sasaki, T. T. [2 ]
Bian, M. Z. [2 ]
Nakata, T. [3 ]
Yoshida, Y. [4 ]
Kawabe, N. [4 ]
Kamado, S. [3 ]
Hono, K. [1 ,2 ]
机构
[1] Univ Tsukuba, Grad Sch Pure & Appl Sci, Tsukuba, Ibaraki 3058577, Japan
[2] Natl Inst Mat Sci, 1-2-1 Sengen, Tsukuba, Ibaraki 3050047, Japan
[3] Nagaoka Univ Technol, 1603-1 Kamitomioka, Nagaoka, Niigata 9402188, Japan
[4] Sumitomo Elect Ind Ltd, 1-1-1 Koyakita, Itami, Hyogo 6640016, Japan
来源
关键词
Magnesium alloy; Formability; Bake hardening; Texture weakening; Recrystallization; TEXTURE EVOLUTION; STATIC RECRYSTALLIZATION; ELEMENTS;
D O I
10.1007/978-3-030-36647-6_18
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
We investigated the effects of Zn additions on the mechanical properties and microstructure of Mg-1.2Al-0.5Ca-0.4Mn and Mg-1.2Al-0.5Ca-0.4Mn-1.6Zn (wt %) alloy sheets fabricated by twin-roll casting and conventional hot rolling. The room temperature stretch formability of the solution-treated alloy sheet is improved by the addition of Zn. The Mg-1.2Al-0.5Ca-0.4Mn-1.6Zn alloy shows an excellent stretch formability with the larger Index Erichsen value of 8.2 mm due to a weak transverse direction split texture. The development of the weak texture is attributed to the uniform grain growth by the solute segregation to the recrystallized grain boundaries. Subsequent bake-hardening treatment, 2% pre-strain at 170 degrees C for 20 min leads to substantial increase in strength without the loss of ductility. The bake-hardened Mg-1.2Al-0.5Ca-0.4Mn-1.6Zn alloy exhibits a high tensile yield strength of 235 MPa with an elongation to failure of 27.1%.
引用
收藏
页码:105 / 111
页数:7
相关论文
共 50 条
  • [31] Effects of manganese addition on microstructure and press formability of hot-rolled Mg-Al-Zn alloy sheets
    Huang, Xinsheng
    Suzuki, Kazutaka
    Watazu, Akira
    Shigematsu, Ichinori
    Saito, Naobumi
    JOURNAL OF MATERIALS RESEARCH, 2008, 23 (11) : 3029 - 3039
  • [32] Tailoring the Mechanical and Degradation Performance of Mg-2.0Zn-0.5Ca-0.4Mn Alloy Through Microstructure Design
    Ehsan Mostaed
    Malgorzata Sikora-Jasinska
    Lifei Wang
    Ali Mostaed
    Ian M. Reaney
    Jaroslaw W. Drelich
    JOM, 2020, 72 : 1880 - 1891
  • [33] Tailoring the Mechanical and Degradation Performance of Mg-2.0Zn-0.5Ca-0.4Mn Alloy Through Microstructure Design
    Mostaed, Ehsan
    Sikora-Jasinska, Malgorzata
    Wang, Lifei
    Mostaed, Ali
    Reaney, Ian M.
    Drelich, Jaroslaw W.
    JOM, 2020, 72 (05) : 1880 - 1891
  • [34] Microstructural refinement and mechanical properties improvement of Mg-Al-Mn-Zn-Ca alloy processed by rotary swaging at room temperature
    Wang, Yongxin
    Yang, Yanmei
    Lin, Yini
    Chen, Hao
    Li, Guo
    Huang, Yuanding
    Xie, Weidong
    Wei, Guobing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 913
  • [35] Mg6Zn0.4Ca0.5Cu alloy: Physically blended microalloyed lightweight alloy with significantly high strength and ductility
    Hassan, S. Fida
    Islam, M. T.
    Nouari, S.
    Al-Aqeeli, N.
    Baig, M. M. A.
    Patel, F.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 787 : 1015 - 1022
  • [36] Influence of finish rolling temperature on the microstructure and mechanical properties of Mg-8.5Al-0.5Zn-0.2Mn-0.15Ag alloy sheets
    Cao, Li
    Liu, Chuming
    Gao, Yonghao
    Jiang, Shunong
    Liu, Yunfeng
    MATERIALS CHARACTERIZATION, 2018, 139 : 38 - 48
  • [37] Effects of Sc and Zr on the Texture and Mechanical Anisotropy of High Strength Al–Zn–Mg Alloy Sheets
    Y. Deng
    Z. M. Yin
    G. F. Xu
    Y. J. Wang
    L. Y. Lu
    J. Q. Duan
    Strength of Materials, 2016, 48 : 39 - 48
  • [38] Influence of different minor additions on structure and properties of high-strength Al-Zn-Mg-Cu alloy sheets
    Senatorova, OG
    Uksusnikov, AN
    Legoshina, SF
    Fridlyander, IN
    Zhegina, IP
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 2000, 331-3 : 1249 - 1253
  • [39] Ceramic coating for delayed degradation of Mg-1.2Zn-0.5Ca-0.5Mn bone fixation and instrumentation
    Ibrahim, Hamdy
    Dehghanghadikolaei, Amir
    Advincula, Rigoberto
    Dean, David
    Luo, Alan
    Elahinia, Mohammad
    THIN SOLID FILMS, 2019, 687
  • [40] Great room temperature stretch formability of fine-grained Mg-Mn alloy
    Somekawa, Hidetoshi
    Kinoshita, Akihito
    Kato, Akira
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 697 : 217 - 223