Effects of debinding parameters on powder injection molded Ti-6Al-4V/HA composite parts

被引:46
|
作者
Thian, ES [1 ]
Loh, NH [1 ]
Khor, KA [1 ]
Tor, SB [1 ]
机构
[1] Nanyang Technol Univ, Sch Mech & Prod Engn, Singapore 639798, Singapore
关键词
titanium alloy-hydroxyapatite; powder injection molding; thermal debinding; composites; ceramic slurry;
D O I
10.1163/156855201750537901
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Titanium alloy-hydroxyapatite (Ti-6Al-4V/HA) composite powders produced by a ceramic slurry were mixed with a multi-component binder system in the powder injection molding process. The binder system comprises mainly of natural wax, fatty acid wax, stearic acid, poly-oxi-alkyen-ether and olefin-hydrocarbons. After molding, the binder system was removed by conventional thermal debinding. The effects of heating rate and gas flow rate on the quality of the debound part in terms of defects, mass of binder removed and residual carbon level were discussed. A slow heating rate (20 degreesC/h) at the beginning stage of the debinding step and a higher gas flow rate (250 cm(3)/min) were required for the production of defect-free parts with minimal carbon level.
引用
收藏
页码:361 / 370
页数:10
相关论文
共 50 条
  • [41] Finite element analysis of the rapid manufacturing of Ti-6Al-4V parts by laser powder deposition
    Crespo, Antonio
    Vilar, Rui
    SCRIPTA MATERIALIA, 2010, 63 (01) : 140 - 143
  • [42] Laser powder bed fusion of Ti-6Al-4V parts: Thermal modeling and mechanical implications
    Masoomi, Mohammad
    Thompson, Scott M.
    Shamsaei, Nima
    INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2017, 118 : 73 - 90
  • [43] Laser surface polishing of Ti-6Al-4V parts manufactured by laser powder bed fusion
    Obeidi, Muhannad Ahmed
    Mussatto, Andre
    Dogu, Merve Nur
    Sreenilayam, Sithara P.
    McCarthy, Eanna
    Ul Ahad, Inam
    Keaveney, Shane
    Brabazon, Dermot
    SURFACE & COATINGS TECHNOLOGY, 2022, 434
  • [44] Microstructure and mechanical properties of plasma sprayed HA/YSZ/Ti-6Al-4V composite coatings
    Khor, KA
    Gu, YW
    Pan, D
    Cheang, P
    BIOMATERIALS, 2004, 25 (18) : 4009 - 4017
  • [45] Effect of oxygen content and relative density on the tensile properties of injection molded Ti-6Al-4V alloy
    Itoh, Yoshinori
    Uematsu, Toshiaki
    Sato, Kenji
    Miura, Hideshi
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2009, 56 (05): : 259 - 263
  • [46] Study on SCS-6/Ti-6Al-4V composite
    Zeng, LY
    Zhao, YQ
    Zhou, L
    Vassel, A
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 and 2, PROCEEDINGS, 2004, : 110 - 112
  • [47] DIFFUSION BONDING OF SIC/TI-6AL-4V COMPOSITE TO TI-6AL-4V ALLOY AND FRACTURE-BEHAVIOR OF JOINT
    FUKUMOTO, S
    HIROSE, A
    KOBAYASHI, KF
    MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (06) : 520 - 527
  • [48] The Effects of Feature Sizes in Selectively Laser Melted Ti-6Al-4V Parts on the Validity of Optimised Process Parameters
    Phutela, Chinmay
    Aboulkhair, Nesma T.
    Tuck, Christopher J.
    Ashcroft, Ian
    MATERIALS, 2020, 13 (01) : 117
  • [49] Microstructure and mechanical properties of severely deformed TI-6AL-4V and TI-6AL-4V/TiC metal matrix composite
    Yapici, GG
    Karaman, I
    Luo, ZP
    ULTRAFINE GRAINED MATERIALS III, 2004, : 433 - 438
  • [50] Effect of mixing parameters on the mixing time and density of composite HA/Ti6AI4V feedstock for powder injection molding
    Arifin, Amir
    Sulong, Abu Bakar
    SRIWIJAYA INTERNATIONAL CONFERENCE ON ENGINEERING, SCIENCE AND TECHNOLOGY (SICEST 2016), 2017, 101