Effect of Mn Addition on the Mechanical Properties of Al-12.6Si Alloy: Role of Al15(MnFe)3Si2 Intermetallic and Microstructure Modification

被引:27
|
作者
Biswas, Prosanta [1 ]
Patra, Surajit [1 ]
Roy, Himadri [2 ,3 ]
Tiwary, Chandra Sekhar [4 ]
Paliwal, Manas [5 ]
Mondal, Manas Kumar [1 ]
机构
[1] Natl Inst Technol Durgapur, Dept Met & Mat Engn, Durgapur 713209, W Bengal, India
[2] CSIR Cent Mech Engn Res Inst, Dept NDT, Durgapur 713209, W Bengal, India
[3] CSIR Cent Mech Engn Res Inst, Met Grp, Durgapur 713209, W Bengal, India
[4] Indian Inst Technol Kharagpur, Dept Met & Mat Engn, Kharagpur 721302, W Bengal, India
[5] Indian Inst Technol, Dept Mat Sci & Engn, Gandhinagar 382355, Gujrat, India
关键词
Al-Si-Mn alloy; Gravity casting; Microstructure; Hardness; Mechanical properties; Fracture behavior; AL-SI ALLOYS; TENSILE PROPERTIES; DEFORMATION-BEHAVIOR; GRAIN REFINER; SOLIDIFICATION; FE;
D O I
10.1007/s12540-019-00535-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Effect of manganese (Mn) addition (0.0, 1.0, 2.0 and 3 wt%) on the microstructural morphology, hardness, tensile properties and fracture behaviour of the gravity cast eutectic Al-12.6Si alloy has been studied through XRD analysis, chemical analysis, optical metallography, FESEM analysis, energy dispersive spectroscopy analysis, hardness test, tensile test and quantitative phase analysis. As-cast Al-12.6Si-0.0Mn alloy has a non-uniformly distributed coarser and irregular shape primary and eutectic silicon particles inside the alpha-Al phase, and both the Si phase have very sharp corners. Whereas, the 1 wt% Mn added alloy has uniformly distributed fine eutectic and primary Si particles with blunt corners. Further, the addition of 1.0 wt% Mn forms very few (0.26 vol %) irregular shape Al-15(MnFe)(3)Si(2)intermetallic phase within the alpha-Al phase and eutectic Si phase. But, 2.0 wt% and 3 wt% Mn added alloy has an irregular shape coarse plate-like Al-15(MnFe)(3)Si-2 intermetallic phase besides the primary and eutectic Si phase. The bulk hardness of the Al-12.6Si alloy is increased with an increase in Mn concentration as the harder Al-15(MnFe)(3)Si-2 intermetallic phase forms and both the Si phase morphology modify. The microhardness of the constituent phases also varies with the change in Mn concentration in the alloy. The Mn addition improved the ultimate tensile strength, yield strength, and elongation (%) of the alloy. However, fractographs reveal that the brittle mode of fracture has been increased due to the presence of a higher volume of brittle Al-15(MnFe)(3)Si-2 intermetallic in 2.0 and 3.0% Mn alloy. On the other hand, the amount of brittle and cleavage fracture of Si particles decreased, and ductile fracture with dimples formation increased in 1.0 wt%Mn added alloy. Graphic
引用
收藏
页码:1713 / 1727
页数:15
相关论文
共 50 条
  • [31] Effect of Cu Addition on the Microstructure, Mechanical and Thermal Properties of a Piston Al-Si Alloy
    Chankitmunkong, Suwaree
    Eskin, Dmitry G.
    Limmaneevichitr, Chaowalit
    LIGHT METALS 2019, 2019, : 463 - 469
  • [32] The Effect of Chilling and Ce Addition on the Microstructure and Mechanical Properties of Al-23Si Alloy
    V. Vijeesh
    K. Narayan Prabhu
    Journal of Materials Engineering and Performance, 2017, 26 : 343 - 349
  • [33] Effect of Bi addition on microstructure and mechanical properties of hypereutectic Al-17.6Si alloy
    Biswas, Prosanta
    Prasadu, Kona Durga
    Mondal, Manas Kumar
    MATERIALS RESEARCH EXPRESS, 2019, 6 (11)
  • [34] Effect of Vanadium addition to Al-Si alloy on its mechanical, tribological and microstructure properties
    Kumar, Aakash
    Sasikumar, C.
    MATERIALS TODAY-PROCEEDINGS, 2017, 4 (02) : 307 - 313
  • [35] The Effect of Chilling and Ce Addition on the Microstructure and Mechanical Properties of Al-23Si Alloy
    Vijeesh, V.
    Prabhu, K. Narayan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (01) : 343 - 349
  • [36] Effect of Complex Modification on Microstructure and Mechanical Properties of Hypoeutectic Al–Si
    Jianhua Wang
    Yaling Liu
    Jiaqing Zhu
    Ya Liu
    Xuping Su
    Metallography, Microstructure, and Analysis, 2019, 8 : 833 - 839
  • [37] Two-phase intermetallic alloy Ni3(Al, Si):: microstructure and mechanical properties
    Merabtine, R
    Devaud-Rzepski, J
    Trichet, MF
    Cornet, M
    INTERMETALLICS, 2001, 9 (12) : 1015 - 1020
  • [38] Modification of eutectic Si and the microstructure in an Al-7Si alloy with barium addition
    Rao, Jinsong
    Zhang, Jin
    Liu, Ruxue
    Zheng, Jiang
    Yin, Dongdi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 728 : 72 - 79
  • [39] Effects of Cu addition on the microstructure and properties of the Al-Mn-Fe-Si alloy
    Cao, Cheng
    Chen, Dengbin
    Fang, Xiaoyang
    Ren, Jieke
    Shen, Jianguo
    Meng, Liang
    Liu, Jiabin
    Qiu, Lin
    Fang, Youtong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 834
  • [40] Effect of Mn and B Addition on the Microstructure and Properties of Al-Si-Cu-Mg Cast Alloy
    Zheng, Jiale
    Pang, Yafei
    Shi, Haojie
    Hu, Wenru
    Liu, Hao
    Du, Xiaodong
    INTERNATIONAL JOURNAL OF METALCASTING, 2024, 18 (04) : 2972 - 2984