Copper deposition based on a newly synthesized metalorganic compound shows promise for reproducible deposition which has been a major problem. The deposition can be carried out without adverse effect on the film qualities at the bubbler temperature of 65 degrees C. Preliminary deposition results reveal that the resistivity is 2.5 mu Omega cm in the deposition temperature range between 175 and 200 degrees C. Unlike (hfac)Cu . VTMS, the resistivity increases with increasing deposition temperature due to loose packing of the grains at higher temperatures. (C) 1996 American Institute of Physics.
引用
收藏
页码:1017 / 1019
页数:3
相关论文
共 50 条
  • [41] Comparison of (hexafluoroacetylacetonate) Cu(vinyltrimethylsilane) and (hexafluoroacetylacetonate) Cu(allyltrimethylsilane) for metalorganic chemical vapor deposition of copper
    Park, MY
    Son, JH
    Kang, SW
    Rhee, SW
    JOURNAL OF MATERIALS RESEARCH, 1999, 14 (03) : 975 - 979
  • [42] Growth and nanostructure of conformai ruthenium films by liquid-source metalorganic chemical vapor deposition
    Dey, S.K.
    Goswami, J.
    Das, A.
    Cao, W.
    Floyd, M.
    Carpenter, R.
    1600, American Institute of Physics Inc. (94):
  • [43] GROWTH OF CAS THIN-FILMS BY SOLID SOURCE METALORGANIC CHEMICAL-VAPOR-DEPOSITION
    HELBING, R
    BIRECKI, H
    DICAROLIS, SA
    FEIGELSON, RS
    HISKES, R
    JOURNAL OF CRYSTAL GROWTH, 1995, 146 (1-4) : 599 - 603
  • [44] Highly (111)-oriented and conformal iridium films by liquid source metalorganic chemical vapor deposition
    Jaydeb Goswami
    Chang-Gong Wang
    Prashant Majhi
    Yong-Wook Shin
    Sandwip K. Dey
    Journal of Materials Research, 2001, 16 : 2192 - 2195
  • [45] NOVEL NITROGEN-SOURCE MATERIALS IN ZINC SELENIDE METALORGANIC CHEMICAL-VAPOR-DEPOSITION
    KAMATA, A
    JOURNAL OF CRYSTAL GROWTH, 1994, 145 (1-4) : 557 - 561
  • [46] Preparation of GaN films on sapphire by metalorganic chemical vapor deposition using dimethylhydrazine as nitrogen source
    Sato, H
    Takahashi, H
    Watanabe, A
    Ota, H
    APPLIED PHYSICS LETTERS, 1996, 68 (25) : 3617 - 3619
  • [47] Low temperature metalorganic chemical vapor deposition of gallium nitride using dimethylhydrazine as nitrogen source
    Hsu, YJ
    Hong, LS
    Huang, KF
    Tsay, JE
    THIN SOLID FILMS, 2002, 419 (1-2) : 33 - 39
  • [48] Growth and nanostructure of conformal ruthenium films by liquid-source metalorganic chemical vapor deposition
    Dey, SK
    Goswami, J
    Das, A
    Cao, W
    Floyd, M
    Carpenter, R
    JOURNAL OF APPLIED PHYSICS, 2003, 94 (01) : 774 - 777
  • [49] Highly (111)-oriented and conformal iridium films by liquid source metalorganic chemical vapor deposition
    Goswami, J
    Wang, CG
    Majhi, P
    Shin, YW
    Dey, SK
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (08) : 2192 - 2195
  • [50] Chemical vapour deposition of thin copper films using a new metalorganic precursor
    Goswami, J
    Raghunathan, L
    Devi, A
    Shivashankar, SA
    Chandrasekaran, S
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1996, 15 (07) : 573 - 575