Liner buckling in profiled polyethylene pipes

被引:11
|
作者
Dhar, AS [1 ]
Moore, ID
机构
[1] Univ Western Ontario, Dept Civil & Environm Engn, London, ON N6A 5B9, Canada
[2] Queens Univ, Dept Civil Engn, Kingston, ON K7L 3N6, Canada
关键词
thermoplastic pipe; HDPE; culvert; deep burial; local buckling; plate-buckling model; limit state design;
D O I
10.1680/gein.8.0197
中图分类号
P5 [地质学];
学科分类号
0709 ; 081803 ;
摘要
Thermoplastic pipes are often manufactured with profiled walls to maximize the flexural stiffness of the pipe for a given amount of polymer. Thin elements in the profile can buckle under the influence of large earth pressures associated with deep burial or other extreme loading conditions. Earth load tests have been conducted on high density polyethylene pipes with a number of different wall profiles. Two high-pressure pipe test cells have been used to conduct these tests. Observations of local buckling in the internal liners of these products have been examined and compared to stability assessments based on the conventional equation for buckling in stiffened plate structures (following modification of that equation to an equation that defines critical strain instead of critical stress). The strain levels that develop in the liner are, however, dependent on three-dimensional bending within the pipe profile. Provided the effects of three-dimensional bending in the pipe profile are considered, the modified Bryan equation appears to be a useful tool for quantifying liner stability and should be considered for inclusion in limit-state design procedures for these structures.
引用
收藏
页码:303 / 326
页数:24
相关论文
共 50 条
  • [21] NMR IMAGING OF POLYETHYLENE PIPES
    SARDASHTI, M
    BALDWIN, BA
    ODONNELL, DJ
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1995, 33 (04) : 571 - 576
  • [22] Infrared welding of polyethylene pipes
    Yeh, HJ
    PLASTICS ENGINEERING, 1997, 53 (03) : 103 - 105
  • [23] Welding polyethylene pipes with confidence
    不详
    INSIGHT, 2001, 43 (09) : 574 - 574
  • [24] Welding polyethylene pipes with confidence
    Anon
    Insight: Non-Destructive Testing and Condition Monitoring, 2001, 43 (09):
  • [26] Residual stress in polyethylene pipes
    Poduska, Jan
    Hutar, Pavel
    Kucera, Jaroslav
    Frank, Andreas
    Sadilek, Jiri
    Pinter, Gerald
    Nahlik, Lubos
    POLYMER TESTING, 2016, 54 : 288 - 295
  • [27] Energy barrier and post-buckling behavior for thermal buckling of a liner shell
    Liu, Yan
    Fan, Qinshan
    Li, Bing
    Qinghua Daxue Xuebao/Journal of Tsinghua University, 2002, 42 (11): : 1519 - 1523
  • [28] Design of profiled sandwich panels subject to local buckling effects
    Pokharel, N
    Mahendran, M
    ADVANCES IN STRUCTURES, VOLS 1 AND 2, 2003, : 397 - 402
  • [29] Buckling Research in Closed Thin-walled Profiled Elements
    Juodvalkis, D.
    Griskevicius, P.
    Skvireckas, R.
    Lendraitis, V.
    TRANSPORT MEANS 2009, 2009, : 141 - 145
  • [30] The Bubble Sign of Successful Polyethylene Liner Impaction
    Fitzgerald, Eilis
    Condon, Finbarr
    TECHNIQUES IN ORTHOPAEDICS, 2024, 39 (03) : 93 - 94