Fracture Failure Analysis of 304 Stainless Steel Elbow

被引:0
|
作者
Wang, Yian [1 ]
Xie, Guoshan [1 ]
Song, Libin [1 ]
He, Meng [2 ]
Zhuang, Fakun [1 ]
Li, Xiaopeng [1 ]
机构
[1] China Special Equipment Inspect & Res Inst, Beijing, Peoples R China
[2] Beijing Inst Technol, Beijing, Peoples R China
关键词
304SS; martensite; hydrogen induced delayed cracking; HYDROGEN ENVIRONMENT EMBRITTLEMENT; AUSTENITIC STAINLESS-STEELS; MICROSTRUCTURE; MARTENSITE;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
A cracking incident of a 304 stainless steel elbow serving in the synthesis gas purification device occurred during running. In order to get an understanding of the failure mechanism, a failure analysis was performed on the cracked elbow in this paper. The chemical composition, mechanical properties of strength, toughness and hardness, hydrogen content were identified and determined. The metallographical structure was observed and analyzed by optical microscope (OM) and X-Ray Diffraction (XRD), while the fracture morphology was observed by scanning electron microscope (SEM). The results showed that the chemical composition of the cracked elbow meet the requirements for China standard, while comparing with GB/T 14976-2012 standards, the strength and elongation of the leaked elbow are higher and lower respectively, and the hardness of the leaked elbow was higher than quality certificate documents that of H13.-.187. Large quantities of martensite and 8-ferrite were observed in elbow, which indicated that the elbow was not well solid solution heat treated required by specification(1050 C,30min). The fracture morphology presents typical brittle fracture. The hydrogen content of cracked elbow was significant higher than that of other 304 stainless steel elbow serving in the environment without hydrogen. It is acknowledged that martensite showed higher sensitivity of hydrogen embrittlement compared with austenite. Furthermore, the operating temperature of cracked elbow was in the range of high hydrogen embrittlement sensitivity. Depending on the metallographical structure, strength, service environment, hydrogen content and fracture morphology, it can be concluded that hydrogen induced delayed cracking was the dominant mechanism of the failure.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Failure analysis of an oxidative chlorination reactor clad with AISI 304L stainless steel
    Zhao, M
    Li, JC
    Jiang, Q
    PROTECTION OF METALS, 2003, 39 (06): : 595 - 596
  • [32] Failure Analysis of an Oxidative Chlorination Reactor Clad with AISI 304L Stainless Steel
    M. Zhao
    J. C. Li
    Q. Jiang
    Protection of Metals, 2003, 39 : 595 - 596
  • [33] Failure Analysis of Type 304 Stainless Steel Tubes in an Energy Production Plant Heat Exchangers
    Jahangiri, M. R.
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 2011, 133 (06):
  • [34] Failure Analysis and Finite Element Simulation on Service Conditions of SUS304 Stainless Steel
    Hongyu He
    Wenhuai Tian
    Jianchun Li
    Keke Shi
    Ming Sun
    Jinglong Li
    Journal of Materials Engineering and Performance, 2021, 30 : 5987 - 5999
  • [35] Fatigue Failure Analysis on Precracked 304 Stainless Steel Components Repaired by Laser with Addition of Nanocomposites
    Wang, Jie
    Jiang, Wei
    SOLDAGEM & INSPECAO, 2019, 24
  • [36] Failure Analysis and Finite Element Simulation on Service Conditions of SUS304 Stainless Steel
    He, Hongyu
    Tian, Wenhuai
    Li, Jianchun
    Shi, Keke
    Sun, Ming
    Li, Jinglong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (08) : 5987 - 5999
  • [37] Failure analysis of an oxidative chlorination reactor clad with AISI 304L stainless steel
    Zhao, M.
    Li, J.C.
    Jiang, Q.
    Zashchita Metallov, 2003, 39 (06): : 660 - 661
  • [38] Microstructure analysis of boride layer of 304 stainless steel
    Beijing Research Institute of Mechanical and Electrical Technology, Beijing 100083, China
    不详
    Cailiao Rechuli Xuebao, 2006, 3 (91-94):
  • [39] CORROSION FAILURE OF AISI-304 STAINLESS-STEEL TUBES
    NATARAJAN, A
    LAKSHMANAN, TS
    NAGARAJAN, KV
    SARKAR, BK
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1982, 35 (01): : 84 - &
  • [40] FAILURE BEHAVIOR OF 304L STAINLESS-STEEL IN TORSION
    SEMIATIN, SL
    HOLBROOK, JH
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (10): : 2091 - 2099