Oxidative protection of carbon fibers with poly(carborane-siloxane-acetylene)

被引:36
|
作者
Keller, TM [1 ]
机构
[1] USN, Res Lab, Adv Mat Sect, Div Chem, Washington, DC 20375 USA
关键词
carbon fibers; carbon composites; oxidation; pyrolysis; thermal analysis;
D O I
10.1016/S0008-6223(01)00092-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Linear carborane-siloxane-acetylenic polymers have been synthesized as precursor materials for thermosets and ceramics for composite applications up to 500 and 1500degreesC, respectively, in an oxidizing environment. The novel linear polymers have the advantage of being extremely easy to process and convert into thermosets or ceramics since they are either liquids at room temperature or low melting solids and are soluble in most organic solvents. Carbon fibers coated with poly(carborane-siloxane-acetylene) forms a protective barrier against oxidation at elevated temperatures. The novel polymer when used as a matrix material (ceramic) was found to protect the carbon fibers from oxidative breakdown. Boron appears to be the key to the unique oxidative stability of the composite compositions. Oxidative studies were performed by thermogravimetric analyses. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:225 / 229
页数:5
相关论文
共 50 条
  • [21] X-RAY PHOTOELECTRON SPECTROSCOPIC DEPTH PROFILING OF AN ATOMIC OXYGEN RESISTANT POLY(CARBORANE SILOXANE) COATING
    SCHWAMM, D
    KULIG, J
    LITT, MH
    CHEMISTRY OF MATERIALS, 1991, 3 (04) : 616 - 620
  • [22] Piezoresistance characterization of poly(dimethyl-siloxane) and poly(ethylene) carbon nanotube composites
    Rizvi, Reza
    Cochrane, Brendan
    Biddiss, Elaine
    Naguib, Hani
    SMART MATERIALS AND STRUCTURES, 2011, 20 (09)
  • [23] Synthesis of poly(arylate-siloxane)s in supercritical carbon dioxide
    Stakhanov, A. I.
    Said-Galiev, E. E.
    Izmailov, B. A.
    Vasnev, V. A.
    Khokhlov, A. R.
    POLYMER SCIENCE SERIES B, 2008, 50 (1-2) : 11 - 15
  • [24] Environmental durability of carbon fiber reinforced poly(imide siloxane) composites
    Lincoln, Jason E.
    Hout, Sara
    Morgan, Roger J.
    Curliss, David B.
    JOURNAL OF ADVANCED MATERIALS, 2008, 40 (01): : 12 - 19
  • [25] Synthesis of poly(arylate-siloxane)s in supercritical carbon dioxide
    A. I. Stakhanov
    E. E. Said-Galiev
    B. A. Izmailov
    V. A. Vasnev
    A. R. Khokhlov
    Polymer Science Series B, 2008, 50 : 11 - 15
  • [26] Oxidative dehydrogenation of ethylbenzene on activated carbon fibers
    Pereira, MFR
    Orfao, JJM
    Figueiredo, JL
    CARBON, 2002, 40 (13) : 2393 - 2401
  • [27] OXIDATION PROTECTION OF CARBON-FIBERS BY COATINGS
    WANG, YQ
    ZHOU, BL
    WANG, ZM
    CARBON, 1995, 33 (04) : 427 - 433
  • [28] PREPARATION AND PROPERTIES OF COILED CARBON-FIBERS BY THE CATALYTIC PYROLYSIS OF ACETYLENE
    MOTOJIMA, S
    HASEGAWA, I
    KAGIYA, S
    ASAKURA, S
    KAWAGUCHI, M
    IWANAGA, H
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C3): : 599 - 606
  • [29] Thermal and thermo-oxidative stabilities of some poly(siloxane-azomethine)s
    Budrugeac, P.
    Racles, Carmen
    Cozan, V.
    Cazacu, Maria
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2008, 92 (01) : 263 - 269
  • [30] POLY(CYANOGEN) AND DERIVED CARBON-FIBERS
    CHEN, JH
    CHANG, PH
    LABES, MM
    SYNTHETIC METALS, 1987, 19 (1-3) : 988 - 988