Corrosion of Fe-2.25%Cr-1%Mo steels at 600-800°C in N2/H2O/H2S atmospheres

被引:9
|
作者
Kim, Min Jung [1 ]
Park, Sang Hwan [2 ]
Lee, Dong Bok [1 ]
机构
[1] Sungkyunkwan Univ, Sch Adv Mat Sci & Engn, Suwon 440746, South Korea
[2] Funct Mat Ctr, Seoul 130650, South Korea
来源
2011 2ND INTERNATIONAL CONFERENCE ON ADVANCES IN ENERGY ENGINEERING (ICAEE) | 2012年 / 14卷
关键词
Fe-Cr alloys; corrosion; sulfidation; H2S; SULFIDATION; KINETICS;
D O I
10.1016/j.egypro.2011.12.1176
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Fe-2.25%Cr-1%Mo alloys were corroded at 600, 700 and 800 degrees C for up to 70 h in 1 atm of N-2/H2O/H2S-mixed gases. The base metal sulfidized to FeS. This at the outer scale formed by the outwardly diffusing Fe ions, whereas that at the inner scale formed by the inwardly diffusing sulfur ions. Some of FeS at the inner scale further reacted with Cr2S3 to the FeCr2S4 spinel. The alloying elements of Cr and Mo sulfidized by the inwardly diffusing sulfur ions at the inner scale. Although FeCr2S4 can suppress sulfidation to a certain extent, the alloys corroded fast, owing to the formation of the nonstoichiometric FeS. (C) 2011 Published by Elsevier Ltd. Selection and/or peer-review under responsibility of the organizing committee of 2nd International Conference on Advances in Energy Engineering (ICAEE).
引用
收藏
页码:1837 / 1842
页数:6
相关论文
共 50 条
  • [31] EARLY STAGES OF OXIDATION OF FE-25CR AND FE-25CR-6AL ALLOYS IN H2/H2O/H2S ATMOSPHERES AT 700-DEGREES-C
    VEDULA, K
    BOULOGNE, B
    HUGHES, P
    CHANG, S
    MICHAL, GM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1989, 120 : 259 - 266
  • [32] The corrosion behavior of sulfidation-resistant Fe-Mo-Al alloys in H2/H2S atmospheres at 900°C
    Chen, RY
    Young, DJ
    Blairs, S
    OXIDATION OF METALS, 2000, 54 (1-2): : 103 - 120
  • [33] Corrosion behavior of sulfidation-resistant Fe-Mo-Al alloys in H2/H2S atmospheres at 900°C
    Chen, R.Y.
    Young, D.J.
    Blairs, S.
    Oxidation of Metals, 2000, 54 (01): : 103 - 120
  • [34] Corrosion behavior of Y-Al alloys in a H2/H2S/H2O gas mixture at 800-950°C
    Kai, W
    Chang, MT
    Liu, CD
    Lee, TW
    OXIDATION OF METALS, 2002, 57 (5-6): : 523 - 547
  • [35] The corrosion of Fe-15wt% Y and of pure Y and Fe in H2-H2S mixtures under 10-8 atm S2 at 600-800°C
    Niu, Y
    Gesmundo, F
    Zeng, C
    Wu, W
    Viani, F
    Rizzo, F
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 : 97 - 104
  • [36] Corrosion of Hot-dip Aluminized 9Cr-1Mo Steel in N2/0.1%H2S Gas
    Abro, Muhammad Ali
    Hahn, Junhee
    Lee, Dong Bok
    KOREAN JOURNAL OF METALS AND MATERIALS, 2019, 57 (04): : 236 - 244
  • [37] THE CORROSION BEHAVIOR OF NI-MO ALLOYS IN A H2/H2O/H2S GAS-MIXTURE
    HE, YR
    DOUGLASS, DL
    GESMUNDO, F
    OXIDATION OF METALS, 1992, 37 (5-6): : 413 - 439
  • [38] Corrosion of Fe-15wt% Y and of pure Y and Fe in H2-H2S mixtures under 10-8 atm S2 at 600-800 °C
    Academia Sinica, Shenyang, China
    Mater Sci Forum, part 1 (97-104):
  • [39] Corrosion performance of unbalanced magnetron-sputter coatings in atmospheres containing 1%H2S or H2S+1%HCI at 600°C
    Levi, TP
    Norton, JF
    Liu, Z
    Gao, W
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 391 - 400
  • [40] The effect of (H2O)n (n=1-2) or H2S on the hydrogen abstraction reaction of H2S by OH radicals in the atmosphere
    Du, Benni
    Zhang, Weichao
    COMPUTATIONAL AND THEORETICAL CHEMISTRY, 2015, 1069 : 77 - 85