Durability of an epoxy adhesive used in civil structural applications

被引:77
|
作者
Sousa, Joao M. [1 ]
Correia, Joao R. [1 ]
Cabral-Fonseca, Susana [2 ]
机构
[1] Univ Lisbon, Inst Super Tecn, CERIS, Lisbon, Portugal
[2] Natl Lab Civil Engn, Lisbon, Portugal
关键词
Structural adhesive; Epoxy; Durability; Hygrothermal ageing; Outdoor ageing; COMPOSITE SANDWICH PANELS; MECHANICAL-PROPERTIES; BRIDGE CONSTRUCTION; WATER-ABSORPTION; RESINS; MOISTURE; TEMPERATURE; ENVIRONMENT; SYSTEM; PERFORMANCE;
D O I
10.1016/j.conbuildmat.2017.11.168
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper presents an experimental study about the durability of a cold curing structural epoxy (EP) adhesive exposed to different hygrothermal and outdoor ageing environments, typical of civil engineering applications, for up to two years: water and salt water immersion at 20 degrees C and 40 degrees C, continuous condensation at 40 degrees C, and outdoor ageing in a mild Mediterranean climate. After specific exposure periods, changes in the following physical properties and mechanical behaviour of the adhesive were assessed: (i) media diffusion, through water uptake (in hygrothermal environments); (ii) viscoelastic behaviour, through dynamic mechanical analyses (DMA); and (iii) flexural and (iv) in plane shear behaviour. Regarding media diffusion, water uptake did not follow a Fickian behaviour and a final saturation stage was not reached; two alternative non-Fickian analytical models were successfully fitted to the test data and the corresponding diffusion parameters were determined. In what concerns the viscoelastic behaviour, while continuous condensation and outdoor ageing caused negligible changes, the T-g of the adhesive generally decreased due to immersion (around 20% in water and 10% in salt water after two years); in addition, at later stages of water immersion, the tan delta curve showed significant shape differences, with the usual curve peak being replaced by two different peaks; a generalised reduction of the storage modulus at the glassy plateau was also noted. In terms of mechanical performance, such plasticization effects were visible in the flexural and shear stress-strain behaviours. The flexural properties exhibited irreversible degradation, with the highest reductions (two years of ageing in water at 40 degrees C) being about 24% and 30% in strength and modulus, respectively. Regarding the shear properties, in hygrothermal environments the shear modulus showed similar decreasing trends to the flexural modulus (43% reduction after one year), but the shear strength increased (similar to 25%); the outdoor ageing affected the shear properties in the same way, but the magnitudes of the changes were lower. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:618 / 633
页数:16
相关论文
共 50 条
  • [31] Nanofilled epoxy adhesive for structural aeronautic materials
    Vietri, U.
    Guadagno, L.
    Raimondo, M.
    Vertuccio, L.
    Lafdi, K.
    COMPOSITES PART B-ENGINEERING, 2014, 61 : 73 - 83
  • [32] A Biosourced Epoxy Resin for Adhesive Thermoset Applications
    Moreira, Vitor B.
    Aleman, Carlos
    Rintjema, Jeroen
    Bravo, Fernando
    Kleij, Arjan W.
    Armelin, Elaine
    CHEMSUSCHEM, 2022, 15 (07)
  • [33] EFFECT OF SURFACE PREPARATION ON THE DURABILITY OF STRUCTURAL ADHESIVE BONDS
    GOSSELIN, CA
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1985, 190 (SEP): : 122 - PME
  • [34] Epoxy adhesive for cryogenic applications by Master Bond
    不详
    GLASS SCIENCE AND TECHNOLOGY, 2005, 78 (05): : 248 - 248
  • [35] Study of the Influence of Structural Adhesive on Durability of Vehicle Body
    Qi, Chao
    Mao, Xianhong
    Wang, Hua
    Deng, Binjiao
    PROCEEDINGS OF CHINA SAE CONGRESS 2018: SELECTED PAPERS, 2020, 574 : 699 - 707
  • [37] OPTIMIZATION OF THE DURABILITY OF STRUCTURAL TITANIUM ADHESIVE JOINTS.
    Matz, C.
    International Journal of Adhesion and Adhesives, 1988, 8 (01): : 17 - 24
  • [38] EFFECT OF SURFACE PREPARATION ON THE DURABILITY OF STRUCTURAL ADHESIVE BONDS
    GOSSELIN, CA
    ACS SYMPOSIUM SERIES, 1986, 322 : 181 - 193
  • [39] Design and durability of titanium adhesive joints for marine applications
    Golaz, B.
    Michaud, V.
    Lavanchy, S.
    Manson, J-A E.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2013, 45 : 150 - 157
  • [40] Durability of Concrete and Epoxy-Repair Mortar Used Systems
    Karaguler, Mustafa Erkan
    Yuksel, Sebnem Kuloglu
    7TH ASIAN SYMPOSIUM ON POLYMERS IN CONCRETE, 2012, : 405 - 414