Effect of Chloride and Iodide on the Corrosion Behavior of 13Cr Stainless Steel

被引:8
|
作者
Liu, Wanying [1 ,2 ]
Yang, Hong [1 ]
Li, Xiaopeng [1 ]
Zhang, Zhi [2 ]
Lin, Yuanhua [1 ,2 ]
Deng, Kuanhai [2 ]
机构
[1] Southwest Petr Univ, Sch New Energy & Mat, Chengdu 610500, Peoples R China
[2] Southwest Petr Univ, State Key Lab Oil & Gas Reservoir Geol & Exploita, Chengdu 610500, Peoples R China
基金
中国国家自然科学基金;
关键词
scanning electrochemical microscopy (SECM); stainless steel; corrosion; electroactivity; SEM; SCANNING ELECTROCHEMICAL MICROSCOPY; LOCALIZED CORROSION; CARBON-STEEL; HYDROGEN; SECM;
D O I
10.3390/met12111833
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion behavior and mechanism of 13Cr stainless steel in the solution with 1 mol/L NaCl and 5 mmol/L KI were investigated by weight loss method, scanning electrochemical microscopy (SECM), the phase analysis (XRD) of inclusions, and surface analysis technique (SEM and EDS). Results showed that the corrosion rate was a linear relationship with the time and Cl- concentration. The corrosion became serious with the increase in time and Cl- concentration. The corrosion occurred in the unstable electroactive points that contained aluminum oxide and metallic phase inclusions. The generation and disappearance of the electroactive points simultaneously occurred with the corrosion. The active dissolved level on different areas of the surface of 13Cr stainless-steel sample was different. The oxidation current peak of the sample presented the strip shape. The corrosion dissolution was mainly caused by aluminum oxide inclusions (Al2O3) and FeAl phase.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Effect of temperature on the corrosion behavior of 13Cr stainless steel under a high CO2 partial pressure environment
    Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing
    100083, China
    Gongcheng Kexue Xuebao, 11 (1463-1468):
  • [22] Clarify the effect of reversed austenite on the pitting corrosion resistance of super 13Cr martensitic stainless steel
    Zhao, Yonggang
    Zhu, Zhiyuan
    Zhao, Xuhang
    Tian, Ruichao
    Lei, Yun
    Yu, Pengfei
    Peng, Haoping
    Chen, Longjun
    CORROSION SCIENCE, 2023, 213
  • [23] Corrosion Inhibition of 13Cr Stainless Steel in HCl/HAc/HF Acid Solution
    Du, Juan
    Xiang, Kun
    Zhao, Liqiang
    Lan, Xitang
    Liu, Pingli
    Liu, Yue
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (09): : 8919 - 8930
  • [24] Corrosion Behavior of Supermartensitic Stainless Steel 13Cr and Stainless Steel 316L Under Chloride Solution and H2S/CO2 Environments
    Costa, Josiane Soares
    Altenhofen, Aldo
    CORROSION, 2024, 80 (09) : 880 - 888
  • [25] Effect of HCO3- on passivation and pitting behavior of super 13Cr martensitic stainless steel
    Lyu, Nai-Xin
    Liu, Kai-Ping
    Yin, Cheng-Xian
    Fu, An-Qing
    Zi, Yang
    Lei, Xiao-Wei
    Surface Technology, 2019, 48 (05) : 36 - 42
  • [26] Effect of extremely high CO2 pressure on the formation of the corrosion film on 13Cr stainless steel
    Zhu, Jinyang
    Li, Dapeng
    Zhang, Yunan
    Zhang, Lei
    RSC ADVANCES, 2019, 9 (66) : 38597 - 38603
  • [27] Corrosion behavior of super 13Cr stainless steel in a H2S and CO2 environment
    ZHANG Chunxia
    QI Yameng
    ZHANG Zhonghua
    Baosteel Technical Research, 2021, 15 (02) : 35 - 41
  • [28] Microstructural development and corrosion behavior of 13Cr–4Ni-1Mo martensitic stainless steel clad
    A. Farzadi
    R. Kalantarian
    Welding in the World, 2020, 64 : 1811 - 1823
  • [29] Microstructure and mechanical behavior in dissimilar 13Cr/2205 stainless steel welded pipes
    Bettahar, K.
    Bouabdallah, M.
    Badji, R.
    Gaceb, M.
    Kahloun, C.
    Bacroix, B.
    MATERIALS & DESIGN, 2015, 85 : 221 - 229
  • [30] Influence of plasma-sprayed coating on corrosion fatigue strength of 13Cr stainless steel
    Ebara, Ryuichiro
    Shigemura, Sadato
    Yamane, Takashi
    Zairyo/Journal of the Society of Materials Science, Japan, 1994, 43 (490) : 881 - 887