Microstructure evolutions of SiCp/AZ91 Mg matrix composites during hot compression

被引:27
|
作者
Wang, X. J. [1 ]
Hu, X. S. [1 ]
Wang, Y. Q. [2 ]
Nie, K. B. [1 ]
Wu, K. [1 ]
Zheng, M. Y. [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin, Peoples R China
[2] Harbin Engn Univ, Harbin, Peoples R China
基金
中国国家自然科学基金;
关键词
Mg matrix composites; Compression; Strain rates; Temperatures; DRX; MECHANICAL-PROPERTIES; DYNAMIC RECRYSTALLIZATION; BEHAVIOR; DEFORMATION; TEMPERATURE; EXTRUSION; SIZE;
D O I
10.1016/j.msea.2012.08.054
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
10 vol% 10 mu m SiCp/AZ91 composite fabricated by stir casting was compressed with four temperatures and four strain rates. Compression improved the SIC particle distribution of the composite. Particles segregation was easy to be reduced at higher compressive temperatures. Dynamic recrystallization (DRX) took place in the matrix during hot compression. DRX areas were mainly located near particle aggregations at grain boundaries. Temperatures and strain rates significantly affected the DRX behavior of the matrix, which causes the different microstructures of the composites compressed at different parameters. In addition, temperatures and strain rates also significantly affected the dislocations and twins of the matrix. The secondary twins were observed at higher strain rates. The twins recovered at the higher temperatures and lower strain rates. As temperatures increased, the density and morphology of the dislocations evidently changed. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:139 / 146
页数:8
相关论文
共 50 条
  • [21] Mechanical Properties and Wear Resistance of (Grp+SiCp)/AZ91 Magnesium Matrix Composites after Hot Extrusion
    Bai Yan
    Deng Kunkun
    Kang Jinwen
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (07) : 2251 - 2257
  • [22] Hot deformation behavior of Sicw/AZ91 magnesium matrix composite in compression
    Li, SB
    Zheng, MY
    Gan, WM
    Wu, K
    PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 893 - 896
  • [23] Effect of particle size on microstructure and mechanical properties of SiCp/AZ91 magnesium matrix composite
    Deng, K. K.
    Wang, X. J.
    Wu, Y. W.
    Hu, X. S.
    Wu, K.
    Gan, W. M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 543 : 158 - 163
  • [24] Hot deformation behavior of SiCp/AZ91 magnesium matrix composite fabricated by stir casting
    Wang, X. J.
    Hu, X. S.
    Wu, K.
    Deng, K. K.
    Gan, W. M.
    Wang, C. Y.
    Zheng, M. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 492 (1-2): : 481 - 485
  • [25] Microstructure, and Mechanical and Wear Properties of Grp/AZ91 Magnesium Matrix Composites
    Wang, Chang-rui
    Deng, Kun-kun
    Bai, Yan
    MATERIALS, 2019, 12 (07)
  • [26] Microstructure and mechanical properties of hybrid hexagonal BN nanotube and nanoplatelet reinforced AZ91 Mg matrix composites
    Jin, Ge
    Xiao, Min
    Liu, Fei
    Liu, Weiwei
    Chen, Yao
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 1509 - 1520
  • [27] Microstructure and mechanical properties of AZ91-(SiCP/AZ91) clad plate fabricated by extrusion
    Hai, Chang
    Zhao, Congming
    Wang, Cuiju
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2023, 51 (01): : 16 - 25
  • [28] Creep and hot working of Mg alloy AZ91
    McQueen, HJ
    Konopleva, EV
    MAGNESIUM TECHNOLOGY 2001, 2001, : 227 - 234
  • [29] Corrosion of Mg alloy AZ91 - the role of microstructure
    Raman, RKS
    Birbilis, N
    Efthimiadis, J
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2004, 39 (04) : 346 - 350
  • [30] Low cost SiCp/AZ91 magnesium composites prepared by RCM
    Kim, SK
    Jo, HH
    Kim, YJ
    MAGNESIUM TECHNOLOGY 2003, 2003, : 289 - 293