摘要
The high-temperature fatigue and creep behaviour of near-a titanium alloy IMI 834 was studied for temperatures up to 650 degrees C. In order to identify the relevant damage mechanisms, the test program involved continuous cycling, dwell tests with hold periods in tension and compression, and asymmetrical strain-time cycles. The dominant damage mechanism was found to change at a temperature of about 600 degrees C. At low test temperatures fatigue life is largely dependent on the maximum stress of the fatigue cycle. At high temperatures a brittle oxygen-enriched subsurface layer forms, and thus, environmental degradation governs fatigue life in high-temperature low frequency tests. Lamella boundaries present in the bimodal microstructure were seen to deflect small fatigue cracks, and thus, this microstructure has superior fatigue properties as compared to an equiaxed one. During long-term high-temperature exposure, however, significant degradation of the lamella boundaries was observed, and then both microstructures display similar fatigue properties. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:779 / 789
页数:11
相关论文
共 50 条
  • [31] Effect of Microstructure on the Properties of a Near-α High-Temperature Titanium Alloy
    Guo Ping
    Zhao Yongqing
    Hong Quan
    Xin Shewei
    Liu Wei
    Zeng Weidong
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL II, 2012, : 1269 - 1271
  • [32] Life prediction for the titanium alloy IMI 834 under high temperature creep-fatigue loadings
    Kordisch, T.
    Nowack, H.
    Fatigue and Fracture of Engineering Materials and Structures, 1998, 21 (01): : 47 - 63
  • [33] Life prediction for the titanium alloy IMI 834 under high temperature creep-fatigue loadings
    Kordisch, T
    Nowack, H
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1998, 21 (01) : 47 - 63
  • [34] The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt
    Pustode, Mangesh D.
    Raja, V.S.
    Paulose, Neeta
    Corrosion Science, 2014, 82 : 191 - 196
  • [35] The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt
    Pustode, Mangesh D.
    Raja, V. S.
    Paulose, Neeta
    CORROSION SCIENCE, 2014, 82 : 191 - 196
  • [36] Effect of Thermomechanical Processing on the Dwell Fatigue Behaviour of Near Alpha Titanium Alloy IMI 834
    K. U. Yazar
    Amit Bhattacharjee
    Satyam Suwas
    JOM, 2023, 75 : 218 - 231
  • [37] Effect of Thermomechanical Processing on the Dwell Fatigue Behaviour of Near Alpha Titanium Alloy IMI 834
    Yazar, K. U.
    Bhattacharjee, Amit
    Suwas, Satyam
    JOM, 2023, 75 (01) : 218 - 231
  • [38] The influence of high-temperature oxidation resistant titanium aluminide coating on low-cycle fatigue behaviour of titanium alloy IMI 834 at 600°C
    Sahu, J. K.
    Sahu, K. K.
    Ray, A. K.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2012, 226 (L1) : 34 - 41
  • [39] Influence of thermomechanical processing on microstructural evolution in near-α alloy IMI834
    Wanjara, P
    Jahazi, M
    Monajati, H
    Yue, S
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 416 (1-2): : 300 - 311
  • [40] SUPERPLASTIC DEFORMATION AND POSTFORMED MECHANICAL-PROPERTIES OF HIGH-TEMPERATURE TITANIUM-ALLOY IMI-834
    WISBEY, A
    KEARNS, MW
    PARTRIDGE, PG
    BOWEN, AW
    MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (11) : 987 - 993