Oxidation-enhanced annealing of implantation-induced Z1/2 centers in 4H-SiC: Reaction kinetics and modeling

被引:22
|
作者
Lovlie, L. S. [1 ]
Svensson, B. G. [1 ]
机构
[1] Univ Oslo, Dept Phys, Ctr Mat Sci & Nanotechnol, N-0316 Oslo, Norway
来源
PHYSICAL REVIEW B | 2012年 / 86卷 / 07期
关键词
4H SILICON-CARBIDE; CHEMICAL-VAPOR-DEPOSITION; DEEP-LEVEL DEFECTS; 4H-SILICON CARBIDE; EPITAXIAL LAYERS; DIFFUSION;
D O I
10.1103/PhysRevB.86.075205
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High-purity epitaxial layers of n-type 4H-SiC have been implanted with 4.3-MeV Si ions to a dose of 3 x 10(8) cm(-2) and then subjected to dry isothermal oxidation at temperatures between 1050 and 1175 degrees C. Analysis of the samples by depth-resolved deep level transient spectroscopy unveils a strong oxidation-enhanced annealing of the prominent Z(1/2) center, commonly ascribed to the carbon vacancy. The integrated (total) loss of Z(1/2) centers is proportional to the thickness of the silicon dioxide (SiO2) layer grown but the proportionality constant, or annihilation efficiency, decreases with decreasing oxidation temperature. At a given depth x, the annealing of Z(1/2) obeys first-order kinetics with a rate constant c having an activation energy of similar to 5.3 eV. The pre-exponential factor c decreases with increasing x and a normalized concentration-versus-depth distribution of the species injected from the surface and annihilating the Z(1/2) centers has been deducted. This species is believed to be the carbon interstitial and is labeled C-I: numerical simulations of the reaction kinetics employing a model where (i) the generation rate of C-I at the SiO2/SiC interface is related to the oxidation rate, (ii) the diffusion of C-I into the SiC layer is fast, and (iii) a steady-state concentration profile of C-I is rapidly established, yield good agreement with the experimental data for the evolution of both Z(1/2) (absolute values) and C-I (relative values) with temperature, depth, and time. The activation energy obtained for the diffusivity of C-I is similar to 3.0 eV, presumably reflecting the migration barrier for C-I and possibly some contribution from an extra barrier to be surmounted at the SiO2/SiC interface.
引用
收藏
页数:8
相关论文
共 50 条
  • [31] Oxidation induced ON1, ON2a/b defects in 4H-SiC characterized by DLTS
    Booker, I. D.
    Abdalla, H.
    Lilja, L.
    Hassan, J.
    Bergman, J. P.
    Sveinbjornsson, E. O.
    Janzen, E.
    SILICON CARBIDE AND RELATED MATERIALS 2013, PTS 1 AND 2, 2014, 778-780 : 281 - +
  • [32] Formation of the Z1,2 deep-level defects in 4H-SiC epitaxial layers:: Evidence for nitrogen participation
    Pintilie, I
    Pintilie, L
    Irmscher, K
    Thomas, B
    APPLIED PHYSICS LETTERS, 2002, 81 (25) : 4841 - 4843
  • [33] Effect of post-oxidation-annealing in hydrogen on SiO2/4H-SiC interface
    Suzuki, S
    Fukuda, K
    Okushi, H
    Nagai, K
    Sekigawa, T
    Yoshida, S
    Tanaka, T
    Arai, K
    SILICON CARBIDE AND RELATED MATERIALS - 1999 PTS, 1 & 2, 2000, 338-3 : 1073 - 1076
  • [34] Significant structural distortion in the surface region of 4H-SiC induced by thermal oxidation and recovered by Ar annealing
    Kita, K.
    Hatmanto, Adhi Dwi
    GALLIUM NITRIDE AND SILICON CARBIDE POWER TECHNOLOGIES 8, 2018, 86 (12): : 63 - 67
  • [35] Influences of coexisting O2 in H2O-annealing ambient on thermal oxidation kinetics and MOS interface properties on 4H-SiC (1-100)
    Chu, Qiao
    Noborio, Masato
    Shimizu, Sumera
    Kita, Koji
    MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2020, 116 (116)
  • [36] Reaction of NO molecule at 4H-SiC/SiO2 interface: an ab initio study for the effect of NO annealing after dry oxidation
    Shimizu, Tsunashi
    Akiyama, Toru
    Nakamura, Kohji
    Ito, Tomonori
    Kageshima, Hiroyuki
    Uematsu, Masashi
    Shiraishi, Kenji
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2021, 60 (SB)
  • [37] Electrically active defects induced by thermal oxidation and post-oxidation annealing of n-type 4H-SiC
    Kumar, P.
    Bathen, M. E.
    Martins, M. I. M.
    Prokscha, T.
    Grossner, U.
    JOURNAL OF APPLIED PHYSICS, 2024, 135 (18)
  • [38] Properties of Z1 and Z2 Deep-Level Defects in n-Type Epitaxial and High-Purity Semi-Insulating 4H-SiC
    Kaminski, Pawel
    Kozlowski, Roman
    Zelazko, Jaroslaw
    Kosciewicz, Kinga
    Ciuk, Tymoteusz
    CRYSTALS, 2024, 14 (06)
  • [39] An IR-reflectivity and X-ray diffraction study of high energy He-ion implantation-induced damage in 4H-SiC
    Declémy, A
    Oliviero, E
    Beaufort, MF
    Barbot, JF
    David, ML
    Blanchard, C
    Tessier, Y
    Ntsoenzok, E
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2002, 186 : 318 - 323
  • [40] Effect of Ar annealing temperature on the densification of SiO2 film grown by thermal oxidation on 4H-SiC
    Zhong, Z.-Q., 1600, Univ. of Electronic Science and Technology of China (43):