摘要
Gel-type and macroporous 4-vinylpyridine-derived polymer resins have been prepared by suspension polymerisation employing ethylene glycol diacrylate, ethylene glycol dimethacrylate or divinylbenzene as the crosslinker. Each resin has also been converted into its pyridinium ion form via methylation using methyl iodide, in effect producing the corresponding anion exchange resins. The hydrolytic stability under both acidic and alkaline conditions of both the neutral and the cationic forms of all the resins has been assessed. Crosslinks derived from the diacrylate monomer are the most hydrolytically labile whereas the dimethacrylate derived crosslinks cleave only under basic conditions and when the resin is in its quaternised form. Remarkably a gel-type resin lightly crosslinked using divinylbenzene also degrades under similar conditions, and since the crosslink itself is likely to be stable it seems that mainchain scission is involved in this instance. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:9585 / 9594
页数:10
相关论文
共 50 条
  • [31] Hydrolysis of urea-formaldehyde resins: Disintegration of wood-based panels due to hydrolytic degradation of the glue-joint
    Fleischer, O
    Marutzky, R
    HOLZ ALS ROH-UND WERKSTOFF, 2000, 58 (05) : 295 - 300
  • [32] COMPLEX-FORMATION OF CROSSLINKED POLY(4-VINYLPYRIDINE) RESINS WITH COPPER(II)
    NISHIDE, H
    DEGUCHI, J
    TSUCHIDA, E
    BULLETIN OF THE CHEMICAL SOCIETY OF JAPAN, 1976, 49 (12) : 3498 - 3501
  • [33] Complex chemical interactions on thermo hydrolytic degradation of urea formaldehyde resins (UF-resins) in recycling UF-bonded boards
    Roffael, E.
    Huester, H-G
    EUROPEAN JOURNAL OF WOOD AND WOOD PRODUCTS, 2012, 70 (04) : 401 - 405
  • [34] Hydrolytic degradation of D-mannitol-based polyurethanes
    Romero-Azogil, Lucia
    Benito, Elena
    Martinez de Ilarduya, Antxon
    Gracia Garcia-Martin, M.
    Galbis, Juan A.
    POLYMER DEGRADATION AND STABILITY, 2018, 153 : 262 - 271
  • [35] The Thermal Degradation of Poly(dimethyl Itaconate-co-4-vinylpyridine)
    J. Filipović
    D. Petrović-Đakov
    L. Katsikas
    B. Božić
    Journal of Thermal Analysis and Calorimetry, 2000, 62 : 251 - 256
  • [36] Synthesis and hydrolytic degradation of aliphatic polycarbonate based on dihydroxyacetone
    Wang, Lian-Sheng
    Cheng, Si-Xue
    Zhuo, Ren-Xi
    POLYMER SCIENCE SERIES B, 2013, 55 (11-12) : 604 - 610
  • [37] Synthesis and hydrolytic degradation of aliphatic polycarbonate based on dihydroxyacetone
    Lian-Sheng Wang
    Si-Xue Cheng
    Ren-Xi Zhuo
    Polymer Science Series B, 2013, 55 : 604 - 610
  • [38] The thermal degradation of poly(dimethyl itaconate-co-4-vinylpyridine)
    Filipovic, J
    Petrovic-Dakov, D
    Katsikas, L
    Bozic, B
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2000, 62 (01) : 251 - 256
  • [39] Probing the hydrolytic degradation of UF4 in humid air
    Foley, Bryan J.
    Christian, Jonathan H.
    Klug, Christopher A.
    Villa-Aleman, Eliel
    Wellons, Matthew S.
    DeVore, Michael, II
    Groden, Nicholas
    Darvin, Jason
    DALTON TRANSACTIONS, 2022, 51 (15) : 6061 - 6067
  • [40] PYROLYSIS OF POLY-4-VINYLPYRIDINE - DEGRADATION MECHANISM AND STRUCTURAL-ANALYSIS
    AUDISIO, G
    SEVERINI, F
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1987, 12 (02) : 135 - 147