Effect of Mineral Elements Migration on Softening-melting Properties of Ti-bearing High Basicity Sinter

被引:17
|
作者
Li, Tingle [1 ,2 ]
Sun, Changyu [1 ,2 ]
Lan, Dong [1 ,2 ]
Song, Jian [3 ]
Song, Sunny [4 ]
Wang, Qi [1 ,2 ]
机构
[1] Univ Sci & Technol Liaoning, Key Lab Chem Met Engn Liaoning Prov, Anshan 114051, Liaoning, Peoples R China
[2] Univ Sci & Technol Liaoning, Sch Met & Mat, Anshan 114051, Liaoning, Peoples R China
[3] Panzhihua Steel Vanadium Ironmaking Plant, Panzhihua 617024, Peoples R China
[4] Rio Tinto Iron Ore, Tech Mkt, Perth, WA 6000, Australia
关键词
Ti-bearing sinter; softening-melting; mineral elements migration; BLAST-FURNACE; REDUCTION; BEHAVIOR; AL2O3; MGO; SLAG; ORE;
D O I
10.2355/isijinternational.ISIJINT-2018-498
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The mineral elements migration behaviours of Ti-bearing high basicity sinter during softening melting process, as well as its effect on softening melting properties, are studied using scanning electron microscope and X-ray diffractometer. We can conclude that both MgO and Al2O3 content increase while TiO2 content increases first and decreases later overall in the slag phase from the original state to melting end. At softening stage, some perovskite dissolves into the slag phase and part of TiO2 and MgO in wustite phase transfer into the slag phase. The low melting temperature of the slag phase is the main factor for the low softening temperatures of Ti-bearing sinter. At melting stage, TiO2 in the slag phase is tiny and changes little. The low liquidus temperature and viscosity of the slag phase result in the low melting start temperature of Ti-bearing sinter. The slag phase melts great earlier than metallic iron while the unfused sponge iron still bounds large amounts of perovskite crystals. And then, iron collapses and releases the restrained crystals at a higher temperature, resulting in the second rise of pressure drop.
引用
收藏
页码:245 / 252
页数:8
相关论文
共 50 条
  • [41] Smelting Vanadium-Titanium Magnetite by COREX Process: Effect of V-Ti Bearing Pellet Ratio on the Softening and Melting Behavior of Mixed Burden
    Yin, Chen
    Zhang, Shengfu
    Yang, Xuke
    Yuan, Wanneng
    Yu, Wenzhou
    Wen, Liangying
    Li, Tao
    Bai, Chenguang
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2021, 52 (06): : 4096 - 4108
  • [42] Effect of Cr2O3 on the crystallization, structure, and properties of Ti-bearing blast furnace slag-based glass ceramics
    Jiao, Mengjiao
    Wu, Hangmi
    Li, Zhuoyang
    Lai, Feifei
    Li, Jiangling
    JOURNAL OF ASIAN CERAMIC SOCIETIES, 2021, 9 (03): : 1320 - 1330
  • [43] Effect of operating parameters on high-temperature selective enrichment and precipitation of titanium component in Ti-bearing blast furnace slag and the precipitation mechanism of perovskite
    Zhang, Shiqiu
    Zheng, Kui
    Jiang, Jinxing
    Zhang, Shuyi
    Xu, Geng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 : 2686 - 2696
  • [44] Effect of operating parameters on high-temperature selective enrichment and precipitation of titanium component in Ti-bearing blast furnace slag and the precipitation mechanism of perovskite
    Zhang, Shiqiu
    Zheng, Kui
    Jiang, Jinxing
    Zhang, Shuyi
    Xu, Geng
    Journal of Materials Research and Technology, 2021, 15 : 2686 - 2696
  • [45] Effect of Basicity, Al2O3 and MgO content on the softening and melting properties of the CaO-MgO-SiO2-Al2O3 high alumina quaternary slag system
    Talapaneni, Trinath
    Yedla, Natraj
    Sarkar, Smarajit
    Pal, Snehanshu
    METALLURGICAL RESEARCH & TECHNOLOGY, 2016, 113 (05)
  • [46] EFFECT OF HOT-ROLLING IN FERRITE PHASE ON MECHANICAL-PROPERTIES OF VERY LOW-CARBON TI-BEARING COLD-ROLLED STEEL SHEET
    FURUNO, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1362 - 1362
  • [47] Melting Properties and Phase Composition Transformation of Ti-Bearing Electric Furnace Slags in CaO-SiO2-MgO-Al2O3-50%TiO2 System
    Jing, Jianfa
    Guo, Yufeng
    Wang, Shuai
    Chen, Feng
    Yang, Lingzhi
    Yang, Jianfeng
    Xu, Fuchun
    Yu, Linxuan
    METALS AND MATERIALS INTERNATIONAL, 2024, 30 (08) : 2045 - 2056
  • [48] Effect of trace alloying elements on the stress relaxation properties of high strength Cu–Ti alloys
    Huang, Lan
    Cui, Zhenshan
    Meng, Xiangpeng
    Li, Xiang
    Sheng, Xiaofei
    Lei, Qian
    Materials Science and Engineering: A, 2022, 846
  • [49] Effect of Ion Nitriding on Properties of High Carbon Chromium Bearing Steel Containing Rare Earth Elements
    Zhao, Qiancheng
    Luo, Hong
    Pan, Zhimin
    Wang, Xuefei
    Cheng, Hongxu
    Zong, Yuan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (14) : 6930 - 6941
  • [50] Effect of trace alloying elements on the stress relaxation properties of high strength Cu-Ti alloys
    Huang, Lan
    Cui, Zhenshan
    Meng, Xiangpeng
    Li, Xiang
    Sheng, Xiaofei
    Lei, Qian
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 846